1-20 of 64 Search Results for

zirconia ceramics

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300271
EISBN: 978-1-62708-323-2
... Abstract This chapter concerns itself with the tribology of ceramics, cermets, and cemented carbides. It begins by describing the composition and friction and wear behaviors of aluminum oxide, silicon carbide, silicon nitride, and zirconia. It then compares and contrasts the microstructure...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550511
EISBN: 978-1-62708-307-2
.... This chapter describes the applications, properties, and behaviors of some of the more widely used structural ceramics, including alumina, aluminum titanate, silicon carbide, silicon nitride, zirconia, zirconia-toughened alumina (ZTA), magnesia-partially stabilized zirconia (Mg-PSZ), and yttria-tetragonal...
Image
Published: 01 October 2012
Fig. 10.9 Increase in fracture toughness ( K Ic ) observed upon inclusion of zirconia particles in the ceramic matrix. The volume of zirconia added is shown in the shaded histogram. The toughness of the matrix material is shown in the adjacent white histogram bars. S, sintered. HP, hot More
Image
Published: 01 October 2012
Fig. 1.24 Structural ceramic parts. (a) Zirconium oxide. (b) Silicon carbide. (c) Alumina. (d) Magnesia partially stabilized zirconia More
Image
Published: 01 October 2012
Fig. 11.18 Exhaust nozzle of an F414 engine on an F-18 E/F aircraft, showing the twelve sets of ceramic-matrix composite (CMC) flaps and seals. The white areas on the seals are a zirconia overcoat for mechanical fasteners. Over an order of magnitude increase in life has been obtained More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2022
DOI: 10.31399/asm.tb.tstap.t56040010
EISBN: 978-1-62708-428-4
... of the component group at rebuilding time. They are typically applied by air plasma spray (APS) or high-velocity oxy fuel (HVOF) processes. Thermal barrier coatings consist of a low thermal-conductivity ceramic layer deposited over an MCrAlY bond coat. The ceramic coating is usually zirconia (ZrO 2 ), but pure...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220241
EISBN: 978-1-62708-341-6
..., powder metallurgy (PM) materials and ceramics are generally used because the particle size of the permeable material must be very small–i.e., on the order of 40 τ m (1.57 mils) each. Since these must be isolated from each other, they are usually sintered compacts of magnetic powders which may consist...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610327
EISBN: 978-1-62708-303-4
... are transformation toughening and ceramic-matrix composites. Transformation-Toughened Ceramics One remarkable method of microstructural control to yield improved properties is transformation (martensitic) toughening, first observed in zirconia (ZrO 2 ) ceramics. Zirconia exhibits phase transformations from...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.tm.t52320001
EISBN: 978-1-62708-357-7
... Transparent alumina Optical fiber High-strength zirconia Superconducting oxides Glass fiber reinforced plastics Carbon fiber reinforced plastics Multiphase polymers Fig. 1.8 History of development in new materials. OP, oxide powder 1.4.2 Progress in Synthetic Polymers and Ceramics Steel is a foundation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550569
EISBN: 978-1-62708-307-2
...-reinforced Al 2 O 3 . Fig. 11.8 Tool life of ceramic, ceramic-matrix composite, and cemented carbide materials when machining Inconel 718 (feed of 0.2 mm/rev; depth of cut of 2 mm). Source: Ref 11.4 Wear-Resistant Materials/Applications Particulate-toughened ceramics, such as the zirconia...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.9781627083232
EISBN: 978-1-62708-323-2
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290261
EISBN: 978-1-62708-319-5
... a high melting temperature, usually over 1700 C (3090 F). Examples of refractory metals 270 / Binder and Polymer Assisted Powder Processing include tungsten, molybdenum, rhenium, and zirconium, while examples of refractory ceramics are alumina, zirconia, yttria, and chromia. rheology. The study...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.9781627083195
EISBN: 978-1-62708-319-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540297
EISBN: 978-1-62708-309-6
... they compare with metals. It begins by describing the fracture characteristics of ceramics and glasses along with typical properties and subcritical crack growth mechanisms. It then discusses the properties of engineering plastics and the factors affecting crack formation and growth, fracture toughness...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.tt2.t51060163
EISBN: 978-1-62708-355-3
... Fig. 1 Specimen configurations for direct tensile testing of advanced ceramics. (a) Flat plate or “dog-bone” direct tensile specimen with large ends for gripping and reduced gage section. (b) Cylindrical tensile specimen with straight ends for collet grips and reduced gage section. Tapers...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.tm.9781627083577
EISBN: 978-1-62708-357-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2022
DOI: 10.31399/asm.tb.tstap.t56040055
EISBN: 978-1-62708-428-4
... and misinterpretation of the TSC microstructure. This article aims to aid in identifying metallographic TSC artifacts, specifically in the air plasma spray zirconia-based TBC, including both of its common constituents, the bond coating and the top coating. Artifacts that result from specific sectioning and mounting...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350043
EISBN: 978-1-62708-315-7
... for ceramics sliding on various materials and corresponding references and test conditions Specimens tested in air at room temperature Material Test geometry (a) Friction coefficient Source Fixed specimen Moving specimen Static Kinetic Ag Alumina RPOF … 0.37 1 Zirconia RPOF...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870573
EISBN: 978-1-62708-314-0
... Abstract This chapter discusses the types of fibers and matrix materials used in ceramic matrix composites and the role of interfacial coatings. It describes the methods used to produce ceramic composites, including powder processing, slurry infiltration and consolidation, polymer infiltration...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290009
EISBN: 978-1-62708-319-5
... optimization. With the increasing importance of additive manufacturing (AM) of metals and ceramics, the evaluation of several other powder characteristics, such as powder flow and rheology, has become important. Several powder flow and rheology characterization techniques have recently been developed...