1-20 of 228 Search Results for

zinc plating

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270196
EISBN: 978-1-62708-301-0
... brittle intergranular failure. The most probable cause of the failure was hydrogen embrittlement. Max screws failed during assembly in fuel-injection pumps. Their specified heat treatment was hardening and tempering to 33 to 39 HRC, to be followed by zinc plating, passivation, and tempering again...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350183
EISBN: 978-1-62708-315-7
... Electroless nickel-SiC <20 Nickel electroplate <1000 Nickel-ceramic electroplate 500 Cadmium plate <2000 Zinc plate 1000 Zinc-9Ni plate 2000 Hot dip galvanized 1000 Hot dip aluminized 500 PVD TiN 2 Plasma sprayed ceramic 10 High-velocity oxyfuel cermet 1000...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
... Abstract This chapter covers a wide range of finishing and coating operations, including cleaning, honing, polishing and buffing, and lapping. It discusses the use of rust-preventative compounds, conversion coatings, and plating metals as well as weld overlay, thermal spray, and ceramic...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290207
EISBN: 978-1-62708-306-5
... content of 0.50 to 0.80%. Fasteners are generally formed in the annealed stage and then hardened and tempered to a hardness of 45 to 50 Rc. Zinc or cadmium electroplating is specified for certain applications. Other applications may use a zinc mechanical plating to eliminate hydrogen embrittlement...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
..., magnetic properties, solderability, reflectance, and reduction of friction. Electrodeposited coatings are sometimes applied for two or more reasons. For example, decorative and protective plating are combined in such applications as chromium-plated steel automobile bumpers, trim items made of zinc die...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610501
EISBN: 978-1-62708-303-4
... corrosion in salt water. However, if a pit develops on the surface and destroys the oxide layer, it forms a local anodic area and corrosion is accelerated. Table 1 Galvanic series in seawater at 25 °C (77 °F) Anodic end (most easily corroded) Magnesium Magnesium alloys Zinc...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910237
EISBN: 978-1-62708-250-1
.... Table 13 Typical zinc coating processes and thicknesses Method Process Coating thickness, μm (mils) Applications Electrogalvanizing Electrolysis 0.5–4 (0.02–1.65) Interior; appliance panels, studs, acoustical ceiling members Zinc plating Electrolysis 39 (1.53) Interior...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910331
EISBN: 978-1-62708-250-1
... alloys other than 2000 series aluminum, cast alloys of the silicon type −0.75 0.90 15 Aluminum, cast alloys other than silicon type; cadmium, plated and chromated −0.80 0.95 16 Hot-dip-zinc plate; galvanized steel −1.05 1.20 17 Zinc, wrought; zinc-base die-casting alloys; zinc plated...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240323
EISBN: 978-1-62708-251-8
... Cadmium Alclad 6053 aluminum 1100 aluminum 3003 aluminum 5052 aluminum Zinc Magnesium alloys Magnesium Anodic (corrodes) One of the most important factors influencing corrosion is the difference in electrical potential of two different metals when they are coupled...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550141
EISBN: 978-1-62708-307-2
... that contain 2 to 10% Al combined with minor additions of zinc and manganese. These alloys are widely available at moderate cost, and their mechanical properties are good to 95 to 120 °C (200 to 250 °F). Beyond this, the properties deteriorate rapidly with increasing temperature. The second group consists...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910099
EISBN: 978-1-62708-250-1
... occur in a liquid environment when ions of more cathodic metal (e.g., copper) are plated out of solution onto a more anodic metal surface (e.g., aluminum). Despite its shortcomings, the classification of corrosion forms based on physical appearance or attack mechanism allows a large and complex...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350125
EISBN: 978-1-62708-315-7
... Abstract This chapter discusses the use of coating methods and materials and their impact on corrosion and wear behaviors. It provides detailed engineering information on a wide range of processes, including organic, ceramic, and hot dip coating, metal plating and cladding, and the use of weld...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780383
EISBN: 978-1-62708-281-5
... in the detector, which consists of two parallel conductive plates, one placed above the sample and one that acts as the sample holder. By proper selection of where the current is measured, a secondary or backscattered image can be obtained. In many cases, a combination of analytical techniques ( Table 1...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630211
EISBN: 978-1-62708-270-9
...) Ni-Resist (high-nickel cast iron) Cast iron Wrought iron Low-carbon steel 2117, 2017, 2024, in this order Aluminum alloys Cadmium 5052, 3004, 3003, 1100, 6053, in this order Aluminum alloys Galvanized steel or galvanized wrought iron Zinc Magnesium alloys Magnesium...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300227
EISBN: 978-1-62708-323-2
...) are often silver-plated to ensure removal. There are many tribosystems in which it is not possible to lubricate, and the sliding members will seize if there is no intermediary; silver plating can come to the rescue. Zinc is a stealth metal. It is seldom discussed, and it is usually ignored in technical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030215
EISBN: 978-1-62708-282-2
... stainless steel (UNS S31603) for hot acetic acid service might be to test every plate, flange, nozzle, weld, and so on for the presence of molybdenum by using a chemical spot test method ( Ref 18 ). The absence of molybdenum, which might indicate the mistaken use of a different stainless steel, such as type...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.t53730149
EISBN: 978-1-62708-283-9
... is produced in electric arc furnaces. In the process, flue dust with high zinc contents is treated to recover zinc. Lead battery plates are melted, refined, and recycled. The plastic case is shredded and recycled. The U.S. Environmental Protection Agency (EPA) estimates that approximately 80% of all lead...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350195
EISBN: 978-1-62708-315-7
... Thermally sprayed zinc or aluminum for moderate protection Electrolytic zinc or zinc-nickel alloy (10–14% Ni) coating followed by chromate passivation and an organic topcoat Painting, with appropriate preparation and priming, perhaps zinc or aluminum loaded Cadmium plate, preferably chromate...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130043
EISBN: 978-1-62708-284-6
.... , Some of the Effects of Cadmium, Zinc, and Tin Plating on Springs , Proc. ASTM , Vol 47 , 1947 , p 782 55. Valentine K.B. , Stress Cracking of Electroplated Lockwashers , Trans. ASM , Vol 38 , 1947 , p 488 – 504 56. Zapffe C.A. and Haslem M.E. , Measurement...