... the stress state at any point in a material can be expressed in different ways for different purposes. It then compares and contrasts some of the more widely used yield criteria and demonstrates the use of flow rules. It also explains how to calculate power, energy, and effective strain and strain rate...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090043
EISBN: 978-1-62708-266-2
... ). References 2.1 Carter C.S. and Hyatt M.V. , Review of Stress Corrosion Cracking in Low Alloy Steels with Yield Strengths Below 150 ksi , Stress Corrosion Cracking and Hydrogen Embrittlement in Iron Base Alloys , Vol 6 , National Association of Corrosion Engineers , 1977 , p 524 – 600...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090067
EISBN: 978-1-62708-266-2
... steels and discusses the influence of composition, steelmaking practice, and application environment. chemical composition heat treatment high-strength steel stress-corrosion cracking STEELS with yield strengths greater than 1240 MPa (180 ksi), corresponding to hardnesses greater than 40...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780199
EISBN: 978-1-62708-281-5
... Abstract This article describes the general aspects of and practical problems of failure analysis of creep, stress relaxation, and yielding for homogeneous polymers. The effect of temperature and strain rate on the relationship between yield point and elastic modulus and the aging effect...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090349
EISBN: 978-1-62708-266-2
..., environmental factors, and cracking characteristics. It includes a model that accounts for the primary factors involved in intergranular SCC, namely, tensile stresses above the yield stress of the base material, a sensitized microstructure, and reactor cooling water. The chapter also provides proven remedies...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540121
EISBN: 978-1-62708-309-6
... Abstract This chapter examines the stress-strain characteristics of metals and alloys subjected to cyclic loading and the cumulative effects of fatigue. It begins by explaining how a single load reversal can lower the yield stress of a material and how repeated reversals can cause strain...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240201
EISBN: 978-1-62708-251-8
.... Important tensile properties that can be determined by the tensile test include yield strength, ultimate tensile strength, ductility, resilience, and toughness. The chapter describes the effects of stress concentrations on ductile metals under cyclic loads. Other topics covered include combined stresses...
Series: ASM Technical Books
Publisher: ASM International
Published: 15 June 2021
DOI: 10.31399/asm.tb.mpktmse.t56010001
EISBN: 978-1-62708-384-3
... as engineering and true stress-strain curves, calling attention to certain points and features and what they reveal about the test sample and, in some cases, the cause of the behavior observed. It explains, for example, why some materials exhibit discontinuous yielding while others do not, and in such cases, how...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040051
EISBN: 978-1-62708-300-3
.... It then explains how to determine the onset of yielding, which corresponds to the start of plastic deformation and the flow of metal within the workpiece. The chapter then goes on to present two important yield criteria, one based on shear stress (Tresca criterion), the other on distortion energy (von Mises...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540047
EISBN: 978-1-62708-309-6
... they reveal about the load-carrying characteristics of engineering materials. It then discusses the use of failure criteria and the determination of yielding and fracture limits. It goes on to describe the mechanisms and appearances of brittle and ductile fractures and stress rupture, providing detailed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540281
EISBN: 978-1-62708-309-6
... Abstract Large-scale yielding at the crack tip and time-dependent crack growth mechanisms, such as stress relaxation due to creep, are nonlinear behaviors requiring nonlinear analysis methods. This chapter presents two such methods, one based on elastic-plastic fracture mechanics, the other...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610025
EISBN: 978-1-62708-303-4
.... The chapter also covers compression, shear, and torsion testing, the prediction of yielding, residual stress, and hardness. compression hardness notched tensile test shear stress-strain curve tension MANY MATERIALS, both during initial fabrication and later when placed in service...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410213
EISBN: 978-1-62708-265-5
.... Iron Steel Inst. , Vol 174 , 1953 , p 25 11.26 Armstrong R.W. , The Yield and Flow Stress Dependence on Polycrystalline Grain Size , Yield, Flow and Fracture of Polycrystals , Baker T.N. , Ed, Applied Science Publishers , London , 1983 , p 1 – 31 11.27 Matlock D.K...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220403
EISBN: 978-1-62708-259-4
... and plastic deformations. When this happens, the proportionality between stress and strains ceases to exist. The point at which plastic deformation starts is called yield point or yield stress or yield strength (the latter is the accepted term according to ASTM E6). The start of plastic deformation may or may...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1999
DOI: 10.31399/asm.tb.cmp.t66770135
EISBN: 978-1-62708-337-9
... on core properties including hardenability, microstructure, tensile and yield strength, ductility, toughness, and fatigue resistance. It likewise explains how carbon affects case hardenability, surface hardness, and case toughness and how case depth influences residual stresses and bending and contact...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630081
EISBN: 978-1-62708-270-9
... Abstract A brittle fracture occurs at stresses below the material's yield strength (i.e., in the elastic range of the stress-strain diagram). This chapter focuses on brittle fracture in metals and, more specifically, ferrous alloys. It lists the factors that must all be present simultaneously...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000109
EISBN: 978-1-62708-312-6
..., and heating and cooling profiles, affect strength, ductility, and corrosion resistance. It also provides an extensive amount of property data – including tensile and yield strength, elongation, hardness, and creep and stress rupture measurements as well as fatigue curves – for various grades of powder metal...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780216
EISBN: 978-1-62708-281-5
.... If the material is a plastic that yields, the stress at which it occurs is often a function of the rate of the loading event. Even more important is the fact that the mode of failure for a particular plastic may be very dependent on the rate of loading. A plastic that exhibits extreme ductility when loaded...
Series: ASM Technical Books
Publisher: ASM International
Published: 15 June 2021
DOI: 10.31399/asm.tb.mpktmse.9781627083843
EISBN: 978-1-62708-384-3
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780204
EISBN: 978-1-62708-281-5
... plastic. As the strain is increased, the stress rises (nonlinearly) to a point at which there appears to be a change in behavior. Beyond a critical strain, the stress appears to decrease with increasing strain. This critical strain is referred to as the yield strain, ω y , and the corresponding stress...