1-14 of 14 Search Results for

wet scrubbers

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030209
EISBN: 978-1-62708-282-2
... … Fluid catalytic cracking, coker Fractionator overhead X … Compressed wet gas X … Absorber lean oil X … Debutanizer overhead X … Depropanizer overhead X … Hydroprocessing Stabilizer overheads X X Effluent X … Alkylation (H 2 SO 4 ) Deisobutanizer tower overhead X X...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910427
EISBN: 978-1-62708-250-1
...: Wetting of the surface by condensing media in humid atmospheres (simulated atmosphere tests) Spraying of aggressive media (salt spray tests) Immersion into corrosive liquid (immersion tests) Table 1 compares the characteristics of these laboratory corrosion tests. Laboratory corrosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910193
EISBN: 978-1-62708-250-1
... lesser tendency to oxidize materials. Figure 2 illustrates the oxidizing/reducing power of several common environments. Concentrated nitric acid and wet chlorine environments are strongly oxidizing and promote the oxidation of all but the most noble metals. The oxidizing power of sulfuric acid...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
... equipment Inspection of coating applications Determination of wet-film thickness Determination of dry-film thickness Evaluation of cleanliness between coats Pinhole and holiday testing Evaluation of adhesion and cure A brief review of each of the above inspection sequences can...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910237
EISBN: 978-1-62708-250-1
...–0.50 0.40–0.70 0.40 0.30–0.50 … 0.10 Mo, 0.005–0.05 Nb (a) If a single value is shown, it is a maximum unless otherwise stated. Characteristics of the Protective Oxide Film On alternate wetting and drying, the weathering steels develop a thick, protective oxide film...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480353
EISBN: 978-1-62708-318-8
... and temperature. Titanium alloys with improved crevice-corrosion resistance, such as ASTM grades 7, 11, and 12, should be considered in these situations. Titanium is widely used to handle moist and wet chlorine gas, it and has earned a reputation in the chloralkali industry for outstanding performance...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870573
EISBN: 978-1-62708-314-0
... the substrates, a pressure control system, and scrubbers or traps to remove hazardous materials from the effluent gases. The details of a reactor are shown in Fig. 21.16 , and a schematic of the equipment layout is given in Fig. 21.17 . Reactants may be gases, liquids, or solids at room temperature. Direct...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910099
EISBN: 978-1-62708-250-1
... in which the bulk environment is particularly aggressive, general corrosion may preclude localized corrosion at a crevice site. Figure 10 compares the behavior of type 304 and type 316 stainless steels exposed in different zones of a model sulfur dioxide (SO 2 ) scrubber. In the aggressive acid...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030215
EISBN: 978-1-62708-282-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030292
EISBN: 978-1-62708-282-2
... in refineries and petrochemical plants. Over the past two decades, a substantial amount of new information has been obtained from laboratory simulation of process environments involving exposure to naphthenic acids and sulfur compounds at elevated temperature, and to lower-temperature wet hydrogen sulfide (H 2...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060315
EISBN: 978-1-62708-261-7
... Pollution control equipment : scrubbers Metals processing mills : ovens, afterburners, exhaust fans Coal gasification and liquefaction systems : heat exchangers, reheaters, piping Superalloys are intended to prevent or minimize creep deformation at high temperature ( Fig. 13.5 ). They all have...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480331
EISBN: 978-1-62708-318-8
... chlorides under certain conditions. Crevices should be avoided in equipment for the acidic, light-metal chlorides. At high temperatures and concentrations, it is best to use an alloy such as Ti-0.2%Pd, which offers improved corrosion resistance. The Ti-1%Ni alloy shows promise for scrubbers in boiling 42...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350125
EISBN: 978-1-62708-315-7
... Iridescent 24–72 Olive drab 72–100 Moderate (mostly dry, indoor atmosphere; occasional condensation, wear, and abrasion) 8 0.3 None … Tools, zipper pulls, shelves, machine parts Clear 12–24 Iridescent 24–72 Olive drab 72–100 Severe (exposure to condensation; infrequent wetting...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.9781627082532
EISBN: 978-1-62708-253-2