1-20 of 263 Search Results for

wear failure analysis

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250257
EISBN: 978-1-62708-345-4
... the characteristics of various fatigue failures. Then, it provides information on the modes of impact fractures, wear, scuffing, and stress rupture. Next, the chapter describes the causes of gear failures and discusses the processes involved in conducting the failure analysis. Finally, the chapter presents examples...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130111
EISBN: 978-1-62708-284-6
... . (b) K min > K cl Abstract Abstract This chapter briefly outlines some of the basic aspects of failure analysis, describing some of the basic steps and major concerns in conducting a failure analysis. A brief review of failure types from fracture, distortion, wear-assisted failure...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250293
EISBN: 978-1-62708-345-4
... contact (pitting or spalling), rolling contact, thermal fatigue Impact Tooth bending, tooth shear, tooth chipping, case crushing, torsional shear Wear Abrasive, adhesive Stress rupture Internal, external In an analysis of more than 1500 studies, the three most common failure modes, which...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270074
EISBN: 978-1-62708-301-0
... of the springs along with photographs of the damaged slipper pads and cam plate. It also includes an image of a copper flake found in one of the pistons and discusses the results of qualitative x-ray chemical analysis. adhesive wear scanning electron microscopy slipper pads visual examination Summary...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040295
EISBN: 978-1-62708-300-3
...Abstract Abstract This chapter addresses the issue of die failures in hot and cold forging operations. It describes failure classifications, fatigue fracture and wear mechanisms, analytical wear models, and the various factors that limit die life. It also includes several case studies in which...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110563
EISBN: 978-1-62708-247-1
... indicates the location rubbing along the surface. Figure 32 a) SEM image of a failed comb drive. Failure analysis revealed b) a MEMS element spot welded to the ground plane, and c) a MEMS element that contacted the ground plane and popped back. Figure 28 SEM images of the control, the 39...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250019
EISBN: 978-1-62708-345-4
... , 1985 6. Alban L.E. , Failures of Gears , Failure Analysis and Prevention , Vol 11 , 9th ed. , Metals Handbook , ASM International , 1986 , p 586 – 601 7. Godfrey D. , Recognition and Solution of Some Common Wear Problems Related to Lubrication and Hydraulic Fluids...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630001
EISBN: 978-1-62708-270-9
...Abstract Abstract Failure analysis is a systematic investigative procedure using the scientific method to identify the causes of a failure. This chapter begins by exploring what failure analysis is followed by a section describing the sequence of stages in the investigation and analysis...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780109
EISBN: 978-1-62708-268-6
... to deform the parts. The fault tree may identify conditions in which mechanical interference can prevent proper system operation, induce inadvertent operation, or accelerate wear. To address this concern, the failure analysis team should dimensionally inspect suspect parts to confirm engineering drawing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130395
EISBN: 978-1-62708-284-6
... Fe-O-H 2 O diagram indicating the zones in which various oxides of iron are stable. Courtesy of P. Beiss, University of Aachen, Germany Fig. 4 Steps in a failure analysis Fig. 5 (Part 1) Cause-and-effect matrix derived from powder metallurgy process map Fig. 5 (Part 2...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060385
EISBN: 978-1-62708-261-7
... , Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM International , 2002 10.31399/asm.hb.v11.a0003543 Fatigue Crack Growth Stage III (Overload Fracture after Fatigue) Abrasive Wear Erosive Wear Adhesive Wear Fretting Wear Contact Fatigue Cavitation 16.1 The Many...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780267
EISBN: 978-1-62708-281-5
.../S0043-1648(96)07270-5 51. Bahadur S. , Gong D. , and Anderegg J.W. , The Role of Copper Compounds as Fillers in Transfer Film Formation and Wear of Nylon , Wear , Vol 154 , 1992 , p 207 – 223 10.1016/0043-1648(92)90155-2 52. Moet A. , Failure Analysis...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.horfi.9781627082563
EISBN: 978-1-62708-256-3
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780141
EISBN: 978-1-62708-268-6
.... contaminant sources contaminants failure analysis Litton lasers titanium CONTAMINATION has been mentioned in this book. Contaminants can be a cause of numerous types of system failures: Contaminants can act as an abrasive, accelerating wear on mating parts. Contaminants can act as a source...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.9781627082709
EISBN: 978-1-62708-270-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130311
EISBN: 978-1-62708-284-6
... proper hardening and tempering procedures. (a) Surface and (b) core microstructure of a nitrided forging tool, showing (in a) the problems of a coarse white layer and nitrides on grain boundaries. (c) and (d) Extracted from a die-casting die failure analysis, also for surface and core respectively. Note...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130133
EISBN: 978-1-62708-284-6
... of production and resulting lower strength at trim. Measured clearance between punch and die is reduced. steel forgings crankshaft underfill tube bending spade bit trim tear upset forging failure analysis wear friction cold forging hot forging ...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030117
EISBN: 978-1-62708-282-2
... , ASM International , 1992 , p 214 – 220 • Herro H.M. and Port R.D. , Cavitation Damage , The Nalco Guide to Cooling Water System Failure Analysis , McGraw-Hill , 1993 , p 270 – 271 • Madsen B.W. , Corrosive Wear , Friction, Lubrication, and Wear Technology , Vol...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250311
EISBN: 978-1-62708-345-4
... , Friction, Lubrication, and Wear Technology , Vol 18 , ASM Handbook , ASM International , 1992 , p 535 – 545 6. Alban L. , Systematic Analysis of Gear Failures , American Society for Metals , 1985 7. Boresi A.P. and Sidebottom O.M. , Advanced Mechanics of Materials...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630169
EISBN: 978-1-62708-270-9
... of the general characteristics and effects of and the methods for preventing or reducing different categories of wear failures, namely abrasive (erosive, grinding, and gouging), adhesive, and fretting wear. References References 1. Failure Analysis and Prevention , Vol 11 , ASM Handbook , ASM...