1-20 of 50 Search Results for

viscous pressure bulge test

Sort by
Image
Published: 01 August 2012
Fig. A.8 Flow stress obtained by viscous pressure bulge test and uniaxial tensile test for both DP 500 and BH 210 Experimental strain range, DP 500 tensile: 0 to 0.14; DP 500 bulge: 0 to 0.55; BH 210 tensile: 0 to 0.17; BH 210 bulge: 0 to 0.6. More
Image
Published: 01 August 2012
Fig. A.9 Flow stress of DP 600 obtained by viscous pressure bulge test. Experimental strain range, bulge test: 0 to 0.33 More
Image
Published: 01 August 2012
Fig. A.16 Flow stress curves of DQS (0.75 mm) obtained by viscous pressure bulge test. Experimental strain range, bulge test, DQS-270D: 0.05 to 0.44; DQS-270F: 0.05 to 0.37 More
Image
Published: 01 August 2012
Fig. A.18 Flow stress of SS 304 (1 mm) obtained by viscous pressure bulge test and tensile test. Experimental strain range, tensile test: 0 to 0.44; bulge test: 0.03 to 0.56 More
Image
Published: 01 August 2012
Fig. A.22 Flow stress of aluminum X626 obtained by viscous pressure bulge test. Experimental strain range, bulge test: 0.1 to 0.31 More
Image
Published: 01 August 2012
Fig. A.25 Flow stress data of various materials by viscous pressure bulge test. Experimental strain range, for AMS 5504: 0 to 0.6; SS 409: 0 to 0.68; HSS: 0 to 0.54; AKDQ: 0 to 0.72; AZ31B: 0 to 0.14 More
Image
Published: 01 August 2012
Fig. A.26 Comparison of flow stress curves obtained by viscous pressure bulge test and tensile test (a) for AKDQ steel (0.83 mm) and AA 5754-O (1.3 mm) and (b) for DP 600 (0.6 mm) and DDS (0.77 mm). Experimental strain range, for AKDQ, tensile: 0 to 0.24; AKDQ, bulge: 0 to 0.64; AA 5754-O More
Image
Published: 01 August 2012
Fig. 2.15 Flow curve of DP780 material, obtained from a viscous pressure bulge test (VBT). Source: Ref 2.12 More
Image
Published: 01 August 2012
Fig. A.5 Flow stress of 1050 sheet obtained by viscous pressure bulge (VPB) test and tensile test. Experimental strain range, tensile test: 0 to 0.058; bulge test: 0 to 0.32 More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400221
EISBN: 978-1-62708-316-4
... Abstract This appendix contains flow stress data (in the form of flow curves) obtained by viscous pressure bulge tests conducted on various grades of sheet steel as well as aluminum and magnesium alloys. automotive sheet steels flow stress curves viscous pressure bulge test VISCOUS...
Image
Published: 01 August 2012
Fig. A.10 Flow stress of DP 600 (1 mm) determined by tensile test and viscous pressure bulge test. Experimental strain range, tensile test: 0 to 0.15; bulge test without anisotropy correction: 0.04 to 0.49; bulge test with anisotropy correction: 0.05 to 0.55 More
Image
Published: 01 August 2012
Fig. A.19 Flow stress of AA 6111 (1.04 mm) obtained by tensile test and viscous pressure bulge test. Experimental strain range, tensile test: 0 to 0.19; bulge test: 0.03 to 0.46 More
Image
Published: 01 August 2012
Fig. A.4 Flow stress of AKDQ steel sheet (0.83 mm) obtained by viscous pressure bulge test and uniaxial tensile test. Experimental strain range, tensile test: 0 to 0.32; bulge test: 0.25 to 0.8 More
Image
Published: 01 August 2012
Fig. A.3 Flow stress of AISI 1018 sheet (2.13 mm) obtained by viscous pressure bulge test. Experimental strain range, bulge test: 0 to 1 More
Image
Published: 01 August 2012
Fig. 6.3 Flow stress at room temperature for type 304 stainless steel (1 mm) obtained by viscous pressure bulge test and tensile test. Experimental strain range: tensile test, 0 to 0.44; bulge test, 0.03 to 0.56. More
Image
Published: 01 August 2012
Fig. A.7 Flow stress of DR 120 (1 mm) obtained by circular and elliptical viscous pressure bulge tests. Experimental strain range, circular bulge test: 0 to 0.62 More
Image
Published: 01 August 2012
Fig. A.17 Flow stress of (a) SS 301 and (b) SS 201 (0.25 mm) obtained by viscous pressure bulge test. Experimental strain range, bulge test, SS 301: 0.05 to 0.2; SS 201: 0.05 to 0.19 More
Image
Published: 01 August 2012
Fig. A.2 Flow stress of St1403 sheet material (1 mm) estimated by viscous pressure bulge test. Uniaxial tensile tests were conducted to obtain the anisotropy coefficients ( r 0 , r 45 , r 90 ). Experimental strain range, bulge test: 0 to 0.72 More
Image
Published: 01 August 2012
Fig. A.15 Flow stress of five advanced high strength steel (AHSS) sheet materials obtained by viscous pressure bulge test. Experimental strain range, bulge test, DP 980: 0.05 to 0.3; bare DP 780: 0.05 to 0.33; DP 780 T-Al type: 0.05 to 0.31; DP 780 Y-type U: 0.05 to 0.35; DP 780 Y-type V: 0.05 More
Image
Published: 01 August 2012
Fig. A.6 Flow stress of different sheet materials obtained by viscous pressure bulge test. The sheet material thicknesses were, for AKDQ, 0.72 mm; DP 600, 1 mm; DP 590, 1.24 mm; DP 980, 1 mm; DP 780, 1 mm; and TRIP 780, 1 mm. Experimental strain range, bulge test, DP 980: 0 to 0.12; DP 780: 0 More