Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140021
EISBN: 978-1-62708-264-8
... various phases. The chapter concludes with a brief review of spheroidized microstructures. electron microscopes grain structure heat treatment microstructure optical microscopes steel THE OPTICAL MICROSCOPE is the principal tool used to characterize the internal grain structure of steels...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780359
EISBN: 978-1-62708-281-5
... Abstract This article reviews various analytical techniques most commonly used in plastic component failure analysis. The description of the techniques is intended to make the reader familiar with the general principles and benefits of the methodologies. The descriptions of the analytical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280287
EISBN: 978-1-62708-267-9
... Abstract Superalloys tend to operate in environments where they are subjected to high-temperature corrosion, oxidation, and the erosive effects of hot gases. This chapter discusses the nature of these attacks and the effectiveness of various protection methods. It describes the primary forms of...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310163
EISBN: 978-1-62708-326-3
... the soft austenite into martensite or lower bainite in the hardening operation. The chapter provides information on various quenching systems and a description of quenching techniques, namely austempering, martempering, and patenting. Difficulties associated with hardening of steel are discussed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110010
EISBN: 978-1-62708-247-1
... Abstract As semiconductor feature sizes have shrunk, the technology needed to encapsulate modern integrated circuits has expanded. Due to the various industry changes, package failure analyses are becoming much more challenging; a systematic approach is therefore critical. This article proposes...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110032
EISBN: 978-1-62708-247-1
... Abstract The management of a failure analysis (FA) laboratory requires a broad range of activities to optimize the efficiency of the operation. The purpose of this article is to stimulate readers to consider the various aspects of FA laboratory operations and their respective business...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780204
EISBN: 978-1-62708-281-5
... Abstract This article discusses various factors influencing general polymeric behavior, ductile-brittle transitions, crazing, and the brittle fracture of polymeric materials. The discussion covers the effects of environment on glassy thermoplastic, several parametric descriptions of craze...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310173
EISBN: 978-1-62708-286-0
... Abstract The various types of stainless steel have very different deformation characteristics in terms of strain hardening and anisotropy. It is important to understand and exploit these characteristics to optimize forming of stainless steels. This chapter discusses the various deformation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440027
EISBN: 978-1-62708-262-4
... commonly used hardness testing systems: the Brinell, Rockwell, Vickers, Scleroscope, and various microhardness testers that employ Vickers or Knoop indenters. The effect of carbon content on annealed steels and hardened steels is then discussed. A brief discussion on the concept of the ideal critical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090419
EISBN: 978-1-62708-266-2
... Abstract This chapter describes nondestructive evaluation (NDE) test methods and their relative effectiveness for diagnosing the cause of stress-corrosion cracking (SCC) service failures. It discusses procedures for analyzing various types of damage in carbon and low-alloy steels, high-strength...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410039
EISBN: 978-1-62708-265-5
... that promote such transformations and, in turn, how they affect the structure of various phases and the rate at which they form. The chapter also discusses the concepts of transformation kinetics, minimum free energy, and nucleation and growth, and provides information on alloying, interphase...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040151
EISBN: 978-1-62708-300-3
... Abstract Separation of billets by shearing avoids material loss and is considerably faster than sawing or cutting. This chapter discusses the billet shearing process, the characteristics of sheared surfaces, and the effect of various operating parameters on surface quality. It also includes...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030019
EISBN: 978-1-62708-282-2
... relationships, followed by a brief section on polarization of metals or alloys. The effects of area, distance, and geometric shapes on galvanic-corrosion behavior are then discussed. Various alloys susceptible to galvanic corrosion are briefly reviewed. The chapter also discusses various modes of attack that...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030039
EISBN: 978-1-62708-282-2
... Abstract This chapter provides a detailed account of crevice corrosion of metals. It begins by describing various critical factors influencing crevice corrosion. This is followed by a section presenting selected examples of crevice corrosion of stainless steel, nickel alloys, aluminum alloys...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030148
EISBN: 978-1-62708-282-2
... Abstract Hydrogen damage is a form of environmentally assisted failure that results most often from the combined action of hydrogen and residual or applied tensile stress. This chapter classifies the various forms of hydrogen damage, summarizes the various theories that seek to explain hydrogen...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030184
EISBN: 978-1-62708-282-2
... Abstract This chapter provides a detailed account of cathodic protection. It begins by discussing the fundamentals of cathodic protection followed by a description of the various types of cathodic protection. It then describes the origins, types, and alleged failures of cathodic protection...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030215
EISBN: 978-1-62708-282-2
... Abstract This chapter outlines the step-by-step processes by which materials are selected in order to prevent or control corrosion and includes information on materials that are resistant to the various forms of corrosion. The various forms of corrosion covered are general (uniform) corrosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410151
EISBN: 978-1-62708-280-8
... Abstract This chapter discusses the various factors pertinent to gravity permanent mold (GPM) castings, along with their advantages, limitations, and significance. The discussion covers the geometric factors, process and manufacturing elements, gating practices, and feeding principles of and...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050057
EISBN: 978-1-62708-311-9
... Abstract This chapter discusses the design and operating principles of various types of electromagnetic coils. It explains how induction coils are classified based on the direction of the eddy currents they induce in the workpiece and the corresponding orientation, whether longitudinal or...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910193
EISBN: 978-1-62708-250-1
... significantly alter the response of the material in a given environment. This chapter provides a detailed account of all these types of corrosion affecting various industries, pointing out the connection between the characteristics of the corrosive environment that control corrosion behavior, the corrosion...