... in diameter and up to 61 cm long were produced in this manner. They found that initial attempts to melt unconsolidated pebble, electrolytic flake, and induction-melted chips were unsuccessful, and that it was necessary to compact the material into a feed ingot. Three separate melting stages were used...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850001
EISBN: 978-1-62708-260-0
... inclusions have segregated to the pattern interface. Decarburization . Occurs at the surfaces of steel ingots and billets during processing and shows up as a light etching rim. Carburized surfaces . Surfaces that etch darker than the interior of the disc due to enrichment of carbon content...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550569
EISBN: 978-1-62708-307-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.9781627082600
EISBN: 978-1-62708-260-0