Skip Nav Destination
Close Modal
By
Kenneth G. Budinski, Steven T. Budinski
Search Results for
tribological test
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 118
Search Results for tribological test
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400089
EISBN: 978-1-62708-316-4
... they are applied and removed and how their pressure and temperature ranges can be extended by performance enhancing additives. The chapter also explains how sheet metal forming lubricants are evaluated in the laboratory as well as on the production floor and how tribological tests are conducted to simulate...
Abstract
This chapter discusses the factors that must be considered when selecting a lubricant for sheet metal forming operations. It begins with a review of lubrication regimes and friction models. It then describes the selection and use of sheet metal forming lubricants, explaining how they are applied and removed and how their pressure and temperature ranges can be extended by performance enhancing additives. The chapter also explains how sheet metal forming lubricants are evaluated in the laboratory as well as on the production floor and how tribological tests are conducted to simulate stamping, deep drawing, ironing, and blanking operations.
Book Chapter
Biotribology
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300363
EISBN: 978-1-62708-323-2
... to be hip and knee implants, which are given the most attention in this book as well. 13.2 Dental Tribology For decades, researchers have assessed the relative abrasivity of commercially available toothpastes, and they are still testing new options. The problem is wear through the enamel of the tooth...
Abstract
The chapter covers various aspects of biotribology in the context of dental care, orthopedic implants, haptics, eyewear, and stents and fixation devices. It also addresses the issue of biocompatibility and the effects of friction and contact pressure on skin.
Book Chapter
Tribology, Tribosystems, and Related Terminology
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300001
EISBN: 978-1-62708-323-2
... of laboratory testing of various candidates from each materials group. Modeling and artificial intelligence in tribology are not currently at the point where designers can ask a computer search engine to pick a material for a wear application, as will be pointed out in the book. Testing is often the best way...
Abstract
This chapter provides information on the biennial International Wear of Materials Conference, which is the inspiration for this book. It reviews the fundamentals of tribology, tribosystems, and related terminology. The glossary at the end of this chapter is intended to familiarize readers with some of the fundamental tribology terms that will be repeated throughout this book.
Book Chapter
Measurement Techniques
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390145
EISBN: 978-1-62708-459-8
... Abstract This chapter provides a practical overview of the tools and techniques used to assess the tribological aspects of metal forming processes. It describes test methods that have been developed to evaluate bulk deformation and sheet metal forming processes along with lubricant rheology...
Abstract
This chapter provides a practical overview of the tools and techniques used to assess the tribological aspects of metal forming processes. It describes test methods that have been developed to evaluate bulk deformation and sheet metal forming processes along with lubricant rheology, friction forces, and stress and strain distributions. It explains how to measure temperature between tooling and workpiece surfaces as well as surface topography and composition, film thickness, and wear. It also discusses the benefits of reduced-scale and simulation testing and the transfer of results from one process to another.
Book
Tribomaterials: Properties and Selection for Friction, Wear, and Erosion Applications
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.9781627083232
EISBN: 978-1-62708-323-2
Book Chapter
Sheet Metalworking
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390389
EISBN: 978-1-62708-459-8
..., and strains and the effects of strain hardening on workpiece materials. It presents test methods for evaluating process tribology, describes lubrication and wear control approaches, and discusses the factors, such as surface roughness, lubricant breakdown, and adhesion, that can lead to galling and other...
Abstract
This chapter covers the mechanics and tribology of sheet metalworking processes, including shearing, bending, spinning, stretching, deep drawing, ironing, and hydroforming. It explains how to determine friction, wear, and lubrication needs based on process forces, temperatures, and strains and the effects of strain hardening on workpiece materials. It presents test methods for evaluating process tribology, describes lubrication and wear control approaches, and discusses the factors, such as surface roughness, lubricant breakdown, and adhesion, that can lead to galling and other forms of wear. It also provides best practices for selecting, evaluating, and applying lubricants for specific materials, including steels, stainless steels, and aluminum and magnesium alloys.
Book Chapter
Selection of Materials for Tribosystems
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300421
EISBN: 978-1-62708-323-2
... contact pressures may be locally much higher than anticipated in design calculations. That is why load (force) is usually accelerated in bench tests. Winners in bench tests are screened further, then maybe in prototype assemblies; this is the common methodology. Tribological property information...
Abstract
This chapter provides guidelines and insights on the selection of materials, coatings, and treatments for friction and wear applications. It begins with a review of the system nature of tribological effects, the subtleties of friction, and the selection idiosyncrasies of the material systems and lubricants covered in prior chapters. It then presents a systematic approach for selecting tribomaterials, using an automotive fan motor as an example.
Book Chapter
Tribology of Plastics and Elastomers
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300301
EISBN: 978-1-62708-323-2
.... This is not a significant problem, but users must be aware of it. Type 304 stainless steel is the same from any manufacturer from any place in the world. Polystyrene is different (somewhat) from every compounder. Testing (tribological) is usually necessary when trying to use a plastic or elastomer from multiple suppliers...
Abstract
This chapter covers the friction and wear behaviors of plastics and elastomers. It begins by describing the molecular differences between the two types of polymers and their typical uses. It then discusses the important attributes of engineering plastics and their suitability for applications involving friction, erosion, and adhesive and abrasive wear. It also discusses the tribology of elastomers and rubber along with their basic differences and the conditions under which they produce Schallamach waves. It includes information on polymer composites as well.
Book Chapter
Tribological Properties of Steels
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300199
EISBN: 978-1-62708-323-2
... Pressure Velocity Limit The pressure velocity (PV) limit is a term that originated in plastic bushing tribology, but the concept applies to all tribosystems. A common plastic wear test is to hold the load constant and vary the velocity until an exponential increase in wear rate or friction occurs...
Abstract
This chapter covers the friction and wear behaviors of carbon, alloy, and tool steels. It begins a review of commercially available shapes and forms. It then describes the metallurgy and microstructure of various designations and grades of each type of steel and explains how it affects their performance in adhesive and abrasive wear applications and in environments where they are subjected to solid particle, droplet, slurry, and cavitation erosion and fretting damage.
Book Chapter
Tribological Properties of Copper Alloys
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300163
EISBN: 978-1-62708-323-2
...-body abrasion rate of the copper alloys tested in Fig. 6.6 Wear rate, cm3/min Chapter 6: Tribological Properties of Copper Alloys / 173 Fig. 6.8 Liquid erosion in a copper pipe which carries potable water from rain. A typical copper roof will last 100 years. The only thing keeping copper from being...
Abstract
This chapter covers the friction and wear behaviors of copper alloys. It describes the compositions and forms of copper available and their suitability for applications involving friction, different types of erosion, and adhesive and abrasive wear.
Book Chapter
Material Modifications (Coatings, Treatments, etc.) for Tribological Applications
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300335
EISBN: 978-1-62708-323-2
... surface hardening 12.1 When to Use Material Modifications When a material does not meet service expectations in a tribosystem, there are two choices: try a different material, or alter the wear surface to improve its tribological performance. Changing the underperforming material or materials can...
Abstract
This chapter covers coatings and treatments that are used to improve the friction and wear behaviors of materials. It describes modifications that work by hardening contacting surfaces, including heat treating, vacuum coating, thermal spray, and plating, and those that separate or lubricate surfaces, including solid film, chemical conversion, and vacuum coatings, surface oiling and texturing, and lubricating platings. It compares and contrasts methods based on thickness and depth and their relative effect on friction, erosion, and wear.
Book Chapter
Tribotesting
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300121
EISBN: 978-1-62708-323-2
.... Calculate solutions with tribological models. Simulate the tribosystem and test candidate couples. The low-cost solution to existing or potential tribology problems is option number one, which is to use existing tribological knowledge to solve the problem. For example, fretting damage is caused...
Abstract
This chapter discusses the processes and procedures involved in tribotesting, the significance of test parameters and conditions, and practical considerations including test metrics and measurements and the interpretation of wear damage. It also describes the different types of erosion tests in use and common approaches for adhesive wear and abrasion testing.
Book Chapter
Tribological Properties of Stainless Steel and Other Corrosion-Resisting Metals
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300227
EISBN: 978-1-62708-323-2
... carbon content) of the common Stellite alloys, and it is often used as a test standard for cavitation and liquid erosion applications. Overall, cobalt-base, Stellite-types of alloys have significant utility in tribological applications. Their use, however, is limited by their high cost. They cannot...
Abstract
This chapter covers the tribological properties of stainless steel and other corrosion-resistant alloys. It describes the metallurgy and microstructure of the basic types of stainless steel and their suitability for friction and wear applications and in environments where they are subjected to liquid, droplet, and solid particle erosion. It also discusses the tribology of nickel- and cobalt-base alloys as well as titanium, zinc, tin, aluminum, magnesium, beryllium, graphite, and different types of wood.
Book Chapter
Tribological Properties of Ceramics, Cermets, and Cemented Carbides
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300271
EISBN: 978-1-62708-323-2
...-friction member in these tests. Fig. 10.5 Coefficient of friction of various ceramics in block-on-ring testing, where * indicates thermal spray coatings Adhesive Wear Alumina and all the ceramics that have tribological utility are sintered into shapes. If an application involves rubbing...
Abstract
This chapter concerns itself with the tribology of ceramics, cermets, and cemented carbides. It begins by describing the composition and friction and wear behaviors of aluminum oxide, silicon carbide, silicon nitride, and zirconia. It then compares and contrasts the microstructure, properties, and relative merits of cermets with those of cemented carbides.
Book Chapter
The Mechanisms and Manifestations of Friction
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300013
EISBN: 978-1-62708-323-2
.... A related phenomenon is different test rigs may produce different friction coefficients for the same tribocouple . Many tribology researchers have shown that using different test rigs on the same tribocouple will likely produce different results. Figure 2.20 shows individual test results from three...
Abstract
This chapter reviews the types of friction that are of concern in tribological systems along with their associated causes and effects. It discusses some of the early discoveries that led to the development of friction laws and the understanding that friction is a system effect that can be analyzed based on energy dissipation. It describes the stick-slip behavior observed in wiper blades, the concept of asperities, and the significance of the shape, lay, roughness, and waviness of surfaces in sliding contact. It explains how friction forces are measured and how they are influenced by speed, load, and operating environment. It also covers rolling contact and fluid friction and the effect of lubrication.
Book Chapter
Tribology of Lubricants
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300391
EISBN: 978-1-62708-323-2
... Abstract This chapter covers the tribological properties of different types of oil, greases, solid lubricants, and metalworking and traction fluids. It explains how lubricants are made, how they work, and how they are applied and tested. It also discusses the fundamentals of lubrication...
Abstract
This chapter covers the tribological properties of different types of oil, greases, solid lubricants, and metalworking and traction fluids. It explains how lubricants are made, how they work, and how they are applied and tested. It also discusses the fundamentals of lubrication and friction control, the relationship between viscosity and breakaway friction, and the factors that affect load-carrying capacity and service life.
Book Chapter
Tribological Properties of Cast Irons
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300179
EISBN: 978-1-62708-323-2
... of the oil) for decades. 7.6 Important Grades for Tribological Applications Gray Irons The ferritic gray irons (class 20) (Fig. 7.3) are not generally used for tribological applications, other than perhaps for weights for test machines. The class 35 50 grades of gray cast iron have a pearlite matrix...
Abstract
This chapter covers the friction and wear behaviors of cast irons. It describes the microstructure and metallurgy of gray, white, malleable, and ductile cast irons, their respective tensile properties, and their suitability for applications involving friction, various types of erosion, and adhesive and abrasive wear.
Book Chapter
Extrusion Die and Tooling
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 April 2025
DOI: 10.31399/asm.tb.aet2.t59420107
EISBN: 978-1-62708-487-1
... Abstract This chapter discusses many aspects of extrusion die and tooling, including the terminology and function of extrusion die and tooling, the types of dies, the fundamentals of die design, manufacturing, correction, material, and the surface treatments of die bearings and tribology...
Abstract
This chapter discusses many aspects of extrusion die and tooling, including the terminology and function of extrusion die and tooling, the types of dies, the fundamentals of die design, manufacturing, correction, material, and the surface treatments of die bearings and tribology in extrusion dies. It then presents the fundamentals and function of finite-element modeling simulation. The chapter describes the role of tribology and thermodynamics in the die bearing to control the flow and dimensional stability of extrusion exiting the die.
Book Chapter
Dealing with Friction in Design Engineering
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300047
EISBN: 978-1-62708-323-2
..., and the tribology of metal, ceramic, and polymer surfaces in contact. It also discusses the nature of rolling friction and provides helpful design guidelines. engineering design mechanical friction EVERY PUBLIC AREA in every public building in every country in the world probably has lawyers concerned...
Abstract
This chapter discusses the effect of friction in the context of design. It explains how friction coefficients are determined and how they are used to make sizing and selection decisions. It covers practical issues associated with rolling friction, the use of lubricants, and the tribology of metal, ceramic, and polymer surfaces in contact. It also discusses the nature of rolling friction and provides helpful design guidelines.
Book Chapter
Fundamentals of Metalworking
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390007
EISBN: 978-1-62708-459-8
... Abstract This chapter presents a qualitative and quantitative overview of the stresses, strains, forces, and energy associated with metalworking processes and the tribological behavior of metals. It covers key concepts necessary for understanding metalworking tribology, including plastic...
Abstract
This chapter presents a qualitative and quantitative overview of the stresses, strains, forces, and energy associated with metalworking processes and the tribological behavior of metals. It covers key concepts necessary for understanding metalworking tribology, including plastic deformation, yield criteria, flow strength, and the application of flow rules. It explains how to calculate the work involved in deformation processes, how to assess the propensity for fracture, how to determine temperature rise and strain distribution in the workpiece, and how to classify metalworking processes based on related tribology.
1