EISBN: 978-1-62708-270-9
... basic mechanisms of residual stress formation: thermal, transformational, mechanical, and chemical. residual stress thermal residual stresses transformational residual stresses mechanical residual stresses IT IS LITERALLY a shattering experience to witness a metal part suddenly split into...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410487
EISBN: 978-1-62708-265-5
... austenite transformations operate. Source: Ref 20.2 Figure 20.2 shows schematically the residual-stress evolution of parts that cool at different surface and interior rates from temperatures in the austenite phase field ( Ref 20.2 ). Ebert made this sketch for a carburized steel in which the...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290099
EISBN: 978-1-62708-306-5
... concentration due to weld shape and joint geometry; stress concentration due to weld imperfections; and residual welding stresses. Inspection and characterization of welds are described in the final section of this chapter. cast iron fusion welding residual stress solid-state transformation steel...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310055
EISBN: 978-1-62708-326-3
... information on the causes and characteristics of residual stresses, distortion, and quench cracking of steel. austenite transformation continuous cooling transformation diagram cooling rate distortion isothermal transformation diagram quench cracking quenchants quenching steel THE...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480075
EISBN: 978-1-62708-318-8
... Abstract Titanium alloys respond well to heat treatment be it to increase strength (age hardening), reduce residual stresses, or minimize tradeoffs in ductility, machinability, and dimensional and structural stability (annealing). This chapter describes the phase transformations associated with...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130255
EISBN: 978-1-62708-284-6
... Abstract This chapter provides an overview of the fundamental material- and process-related parameters of quenching on residual stress, distortion control, and cracking. It begins with a description of phase transformations during heating and quenching of steel. This is followed by a section on...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050093
EISBN: 978-1-62708-311-9
..., the role of carbon in the hardening of steels, the process of austenitization, and the influence of cooling rate on subsequent transformations. The chapter also explains how induction heating affects residual stress, distortion, and grain size. austenite transformation cooling rate distortion...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050155
EISBN: 978-1-62708-311-9
... Abstract Induction hardened steels are often tempered to increase their ductility and relieve quenching stresses. During tempering, martensitic microstructures supersaturated with carbon decompose into a more stable, ductile form. This chapter discusses the transformations associated with the...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240153
EISBN: 978-1-62708-251-8
... rapidly. It is not an instantaneous transformation, but it is quicker and distinct from the slower, diffusion-controlled process in isothermal transformations. The M s temperature can be raised by the application of stress during transformation. This occurs because a crystal that forms during a...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540047
EISBN: 978-1-62708-309-6
... stress should be balanced by the same amount of tension stress in order to maintain equilibrium. For high-hardenability steels, the residual stress distribution may be different if there is a phase transformation during cooling and if the new phase is brittle. It may have tensile residual stresses in the...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140055
EISBN: 978-1-62708-264-8
... Abstract Steels contain a wide range of elements, including alloys as well as residual processing impurities. This chapter describes the chemical composition of low-alloy AISI steels, which are classified based on the amounts of chromium, molybdenum, and nickel they contain. It explains why...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090367
EISBN: 978-1-62708-266-2
... strain, plastic strain, and residual stress responses. It also describes the difference between smooth and precracked specimens and how they are used, provides information on slow-strain-rate testing and how to assess the results, and discusses various test environments and procedures, including tests...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420303
EISBN: 978-1-62708-310-2
... appreciable volume increase, because it replaces the close-packed fcc structure with the more loosely packed bct structure. This transformation creates residual stresses that are related to the specific volume change, in addition to the strains due to the misfit of the interstitial solute atoms. At high...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610327
EISBN: 978-1-62708-303-4
..., and grain size distribution. As shown in Fig. 2 , the tetragonal zirconia can transform to monoclinic under the influence of a crack tip stress. The transformation may cause the crack tip to deflect due to the shear stress (approximately 1 to 7%) or to be impeded by the local compressive stress (&gt...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1999
DOI: 10.31399/asm.tb.cmp.t66770199
EISBN: 978-1-62708-337-9
... challenges, particularly in regard to grinding. bending fatigue carburizing contact fatigue fatigue strength grinding microstructure residual stress roller burnishing shot peening surface hardness The mechanical treatments most commonly applied to case-hardened parts are shot peening and...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170417
EISBN: 978-1-62708-297-6
...-alloys cannot be significantly strengthened by heat treatment. Generally, α alloys are annealed or recrystallized to remove residual stresses induced by cold working. Alpha alloys have good weldability because they are insensitive to heat treatment. They generally have poorer forgeability and narrower...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500107
EISBN: 978-1-62708-317-1
... Abstract This chapter discusses the forming characteristics of dual-phase (DP) and transformation-induced plasticity (TRIP) steels. It begins with a review of the mechanical behavior of advanced high-strength steels (AHSS) and how they respond to stress-strain conditions associated with...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220273
EISBN: 978-1-62708-259-4
... for the average are plotted. Source: Ref 14 Martensitic microstructures obtained directly from quenching usually have high residual stresses and insufficient ductility and toughness for use in most applications. Further heat treatment is required to properly condition the...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060197
EISBN: 978-1-62708-261-7
...-relief heat treating is used to relieve stresses from cold working. Care must be taken to ensure uniform cooling, particularly when a component is composed of variable section sizes. If the rate of cooling is not constant and uniform, new residual stresses can result that are equal to or greater than...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410335
EISBN: 978-1-62708-265-5
... Abstract The properties of martensite and the mechanisms that govern its formation are the key to understanding hardness and the hardenability of carbon steel. Martensite is a transformation product of austenite that requires rapid cooling to suppress diffusion-dependent transformation pathways...