1-20 of 604 Search Results for

transformation

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410197
EISBN: 978-1-62708-265-5
... Isothermal and continuous cooling transformation (CT) diagrams help users map out diffusion-controlled phase transformations of austenite to various mixtures of ferrite and cementite. This chapter discusses the application as well as limitations of these engineering tools in the context of heat...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480075
EISBN: 978-1-62708-318-8
...Abstract Abstract Titanium alloys respond well to heat treatment be it to increase strength (age hardening), reduce residual stresses, or minimize tradeoffs in ductility, machinability, and dimensional and structural stability (annealing). This chapter describes the phase transformations...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700115
EISBN: 978-1-62708-279-2
...Chemical composition of cold rolled transformation-induced plasticity (TRIP) steels Table 7.1 Chemical composition of cold rolled transformation-induced plasticity (TRIP) steels Steel grade Composition, % (max) C Mn Al+Si TRIP 590 0.175 2.0 2.0 TRIP 690 0.200 2.0 2.0...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560221
EISBN: 978-1-62708-291-4
... Fig. 9.1 (Part 1) Pearlite formation (at 705 and 650 °C) in isothermal transformation of 0.8% C eutectoid steels. 0.81C-0.07Si-0.65Mn (wt%). Figure 9.2 completes this series. (a) Austenitized at 860 °C, transformed at 705 °C for 150 s. Picral. 250×. (b) Austenitized at 860 °C...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310055
EISBN: 978-1-62708-326-3
...) 0.40 Induction hardening Simple shapes 0.50 Complex shapes 0.33 Approximate transformation temperatures of low-alloy steels Table 1 Approximate transformation temperatures of low-alloy steels Grade Transformation point, °C (°F) Heating (a) Cooling (b) AISI UNS...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560029
EISBN: 978-1-62708-291-4
... to read isothermal transformation and continuous-cooling diagrams and how to recognize the effect of various alloying elements. alloying elements constitutional diagram continuous-cooling diagram isothermal transformation diagram phase transformations It has been established...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240053
EISBN: 978-1-62708-251-8
...Abstract Abstract This chapter provides a short introduction to phase transformations, namely, the liquid-to-solid phase transformations that occur during solidification and the solid-to-solid transformations that are important in processing, such as heat treatment. It also introduces...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860295
EISBN: 978-1-62708-348-5
...Abstract Abstract This chapter concentrates on very low-temperature martensitic transformations, which are of great concern for cryogenic applications and research. The principal transformation characteristics are reviewed and then elaborated. The material classes or alloy systems that exhibit...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420143
EISBN: 978-1-62708-310-2
...Abstract Abstract This chapter discusses the characteristics of eutectoid transformations, a type of solid-state transformation associated with invariant reactions, focusing on the iron-carbon system of steel. It describes the compositions, characteristics, and properties of ferrite, eutectoid...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420015
EISBN: 978-1-62708-310-2
... and nickel atoms. It discusses the difference between interstitial and substitutional solid solutions and the factors that determine the type of solution that two metals are likely to form. It also addresses the development of intermediate phases, the role of free energy, transformation kinetics, liquid...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410039
EISBN: 978-1-62708-265-5
... The microstructure of carbon steel is largely determined by the transformation of austenite to ferrite, cementite, and pearlite. This chapter focuses on the microstructures produced by diffusion-controlled transformations that occur at relatively low cooling rates. It describes the conditions...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240153
EISBN: 978-1-62708-251-8
...Abstract Abstract This chapter examines the isothermal phase transformations of the iron-carbide system. The discussion includes the formation of ferritic, eutectoid, hypoeutectoid, hypereutectoid, bainitic, and martensitic microstructures as well as their properties, composition...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290099
EISBN: 978-1-62708-306-5
...Abstract Abstract During fusion welding, the thermal cycles produced by the moving heat source causes physical state changes, metallurgical phase transformations, and transient thermal stresses and metal movement. This chapter begins by discussing weld metal solidification behavior...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440009
EISBN: 978-1-62708-262-4
... with excess cementite bounding the grains. 1000×. Source: Ref 4 Fig. 6 Time-temperature-transformation (TTT) diagram for a eutectoid (0.77%) carbon steel. Source: Ref 3 Abstract Abstract Steel is an important material because of its tremendous flexibility in metal working and heat...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420303
EISBN: 978-1-62708-310-2
... Transformation of retained austenite to ferrite and cementite 200–300 390–570 III Replacement of the transition carbide and low-carbon martensite by cementite and ferrite 250–350 480–660 Source: Ref 15.8 as published in Ref 15.9 Tempering reactions in steel Table 15.2 Tempering...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.mgppis.t60400023
EISBN: 978-1-62708-258-7
... transformation diagram for AISI/SAE 1080 steel. A, austenite; F, ferrite; C, cementite; M s , martensite start temperature Fig. 2.9 An isothermal transformation diagram for AISI/SAE 1080 steel showing cooling path to obtain a fully martensitic microstructure Fig. 2.10 An isothermal...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220193
EISBN: 978-1-62708-259-4
... defines the final microstructure, and how the associated phase transformations are driven by nucleation and growth processes. It describes diffusionless and diffusive growth mechanisms and provides detailed information on the properties, structure, and behaviors of the transformation products produced...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220273
EISBN: 978-1-62708-259-4
... of the Jominy specimen, measured from the quenched end) is presented for the steel for which the transformation curves apply. Source: Ref 3 and 23 Fig. 10.27 Cast medium carbon steel annealed in the intercritical region (temperature was too low for complete austenitization). Pearlite areas...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060197
EISBN: 978-1-62708-261-7
...; lower bainite formed at lower temperatures has an acicular appearance. The hardness of bainite increases with decreasing temperature of formation. (a) bcc, body-centered cubic; fcc, face-centered cubic; bct, body-centered tetragonal Definitions of critical (transformation) temperatures...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140083
EISBN: 978-1-62708-264-8
... are often confused. Most of the information in the chapter is of a practical nature, covering application-oriented topics such as isothermal transformation (IT) and continuous transformation (CT) diagrams which are used to predict and control the rate of formation of ferrite, pearlite, and bainite...