... Abstract This chapter discusses the types of failures that can occur in sheet metal forming tools and explains how to mitigate their effects. It describes the factors that influence galling and wear and the benefits of special treatments and coatings. It provides information on through...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310181
EISBN: 978-1-62708-286-0
... on high-speed tool steel and carbide tooling, along with tool coatings and coolants applicable to stainless steel. machinability stainless steel machining high-speed steel carbide tooling coolants tool coatings References 1 Machining Data Recommendations...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240411
EISBN: 978-1-62708-251-8
... carbides. It also describes the methods of applying coatings to cutting tools to improve tool life. tool materials water-hardening tool steels shock-resisting tool steels cold work tool steels hot work tool steels low-alloy special-purpose tool steels mold tool steels high-speed tool steels...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060273
EISBN: 978-1-62708-261-7
... steels, and their counterparts made by powder metallurgy. It includes information on the chemical composition and application range of many commercial tool steels and explains how to apply coatings that reduce friction, thermal conductivity, and wear. alloying elements chemical composition...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500107
EISBN: 978-1-62708-317-1
... with deformation processes such as stretching, bending, flanging, deep drawing, and blanking. It then describes the complex tribology of AHSS forming operations, the role of lubrication, the effect of tool steels and coatings, and the force and energy requirements of various forming presses. It also discusses...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460121
EISBN: 978-1-62708-285-3
... in high-pressure cold spray coating characterization, including residual-stress characterization. The chapter includes some preliminary screening of tool hardness and bond adhesion strength, as well as a distinction between surface and bulk characterization techniques and their importance for cold spray...
Book Chapter

By Soumya Subramonian
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500001
EISBN: 978-1-62708-317-1
... coatings are also instrumental in increasing tool life. Cast irons hardenable to ~60 HRC are used to blank softer materials and at slower speeds. Among tools steels, A2, M2, and D2 are used. A2 is used for producing parts on the order of thousands, while M2 is used for larger quantities on the order...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700177
EISBN: 978-1-62708-279-2
.... Modifications to the current forming system such as higher-tonnage presses, appropriate die materials, effective tool coatings, efficient lubricants, and higher binder forces should be considered. The implications of using thinner gages on the elastic stiffness and corrosion resistance need to be deliberated...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400089
EISBN: 978-1-62708-316-4
... ). This test is very useful to test stamping lubricants and tool materials/coatings by quantifying the amount of galling on the roller or the strip. Fig. 7.5 Various Tribotests used for evaluating stamping lubricants; Region 1, flange deformation; Region 2, bending and undbending; Region 3, bending...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300335
EISBN: 978-1-62708-323-2
... material to a critical surface; however, the most popular application is for cutting tools. The TiN and related coatings work well in reducing adhesive transfer and tool material removal by abrasion. If only 50 holes can be achieved with a conventional high-speed steel drill before sharpening is necessary...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350095
EISBN: 978-1-62708-315-7
...-speed steel cutting tools. Increases in tool life of up to 100% are achieved, mostly due to a decrease in friction, because of the hard oxide coating and the ability of the porous oxide to entrap lubricant and draw it to the tool/workpiece interface. Steam oxidation of a finished tool is accomplished...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110402
EISBN: 978-1-62708-247-1
... delineation between certain layers. For samples which will be imaged directly following cleaving, coatings should be applied after downsizing the wafer and prior to cross-sectioning in a cleaving tool (automated or manual), as the coating will cover and obscure features along the cross-section edge...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410551
EISBN: 978-1-62708-265-5
... ) 22.38 Matthews A. , Titanium Nitride PVD Coating Technology , Surf. Eng. , Vol 1 , 1987 , p 93 – 103 10.1179/sur.1985.1.2.93 22.39 Korhonen A.S. , Molarius J.M. , Osenius S. , and Sulonen M.S. , Ion Plasting of Tools and Dies , Tool Materials for Molds...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030338
EISBN: 978-1-62708-282-2
... common mechanism causing this corrosion is referred to as differential corrosion cells. Microbes and stray direct current (dc) in the soil also can affect underground corrosion. Fig. 1 Example of external corrosion of an underground pipeline. Lower quadrant of pipeline shown after coating removal...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040211
EISBN: 978-1-62708-300-3
... [Wick, 1984] Wick C.H. , “ Tools and Manufacturing Engineers Handbook: Volume I, Forming ,” Society of Manufacturing Engineers , 1984 . [Witte, 1967] “ Investigation on the Variations of Loads and Energies in Cold Extrusion under Production Conditions, Influence of Phosphate Coating...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410215
EISBN: 978-1-62708-280-8
... on to the four side cores after they close in. Directional solidification is targeted in three ways through machine stock adjustment, cooling design of the tooling, and mold coating control. Wheel casters who cast larger wheels for trucks or racing cars use two sprues on the rim and one sprue...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.9781627083232
EISBN: 978-1-62708-323-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040277
EISBN: 978-1-62708-300-3
... 255 . 10.1016/S0257-8972(00)01115-4 [Roberts et al., 1980] Roberts G.A. , and Robert A.C. , Tool Steels , American Society for Metals , 1980 . [Semiatin et al., 1981] Semiatin S.L. , and Lahoti G.D. , “ Forging Die Materials, Coatings, and Surface Treatments...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500133
EISBN: 978-1-62708-317-1
... in.), 180 s for 1.75 mm (0.069 in.), and 240 s for 2.5 mm (0.1 in.) ( Ref 7.28 ). The complete tooling solution contains the tool steel, die design and construction, die coating, process parameters, and die maintenance ( Ref 7.30 ). Coating the blanks before heating...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350183
EISBN: 978-1-62708-315-7
... coatings applied by various thin-film processes Fig. 15 Compares the surface hardness of hardened tool steel and a cemented carbide with that of the following surface-hardening processes: TRD, CVD, PVD, boriding, chrome plating, electroless nickel-phosphorus plating, ferritic nitrocarburizing...