... to Ti-6Al-4V, beta transus temperature approximately 995 °C (1825 °F). (b) GFC, gas fan cooled. (c) RT, room temperature Typical room-temperature tensile properties of titanium alloy castings (bars machined from castings) Table 6.2 Typical room-temperature tensile properties...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480161
EISBN: 978-1-62708-318-8
... as a temporary alloying element Research base Porous materials Less than 100% dense materials Research base Titanium alloys used for producing cast parts Table 8.2 Titanium alloys used for producing cast parts Alloy designation Alloy class Remarks Commercially pure titanium Oxygen...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550223
EISBN: 978-1-62708-307-2
..., compositions, and grades of commercially pure titanium and alpha and near-alpha, alpha-beta, and beta titanium alloys. It describes primary and secondary fabrication processes, including melting, forging, forming, heat treating, casting, machining, and joining as well as powder metallurgy and direct metal...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540411
EISBN: 978-1-62708-309-6
...Abstract Abstract This appendix provides tensile property data for titanium alloys and castings and plane-strain fracture toughness data for Ti-6Al-4V castings. alpha-beta titanium alloys beta titanium alloys titanium castings plane-strain fracture toughness tensile properties...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240527
EISBN: 978-1-62708-251-8
... on melting, forging, casting, heat treating, and secondary fabrication. It also discusses the advantages and disadvantages of titanium and its alloys in various applications. melting primary fabrication forging casting heat treatment secondary fabrication titanium titanium alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120345
EISBN: 978-1-62708-269-3
.... , Comparative Evaluation on Ti-10V-2Fe-3Al Cast, PM and Wrought Product Forms , Powder Metall. Int. , Vol 17 ( No. 5 ), 1985 , p 239 – 240 • Breslauer E. and Rosen A. , Relationship between Microstructure and Mechanical Properties in Metastable Beta Titanium 15-3 Alloy , Mater. Sci...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120295
EISBN: 978-1-62708-269-3
... and castings. Specialist fabricator including superplastic forming/diffusion bonding Wyman Gordon Ltd Houston Road Livingston West Lothian EH54 5BZ Douglas Armet    Tel: +44 (0) 1506 446200    Fax: +44 (0) 1506 446330 Manufacturer of large titanium forgings including large diameter extruded pipe...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120047
EISBN: 978-1-62708-269-3
... of wrought, cast, and P/M titanium alloy products Table 7.2 Comparison of typical room-temperature properties of wrought, cast, and P/M titanium alloy products Product and condition Tensile strength Yield strength Elongation, % Reduction in area, % Charpy impact strength Fracture toughness...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120095
EISBN: 978-1-62708-269-3
... sample. (e) Annealed for 2 h at 650 °C (1200 °F) Cast titanium alloys with estimates of relative casting usage Table 12.15 Cast titanium alloys with estimates of relative casting usage Alloy Estimated relative use of castings Nominal composition, wt% Special properties (a) (b...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870537
EISBN: 978-1-62708-314-0
... concepts. Source: Ref 10 Fig. 20.12 Squeeze casting. Source: Ref 6 Fig. 20.21 Silicon carbide monofilament/titanium matrix composite Fig. 20.34 Rod-reinforced niobium carbide/niobium eutectic. Source: Ref 7 Fig. 20.31 Diamond-impregnated core drill and coolant...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740001
EISBN: 978-1-62708-308-9
..., vacuum induction melting furnaces, and electroslag and vacuum arc remelting furnaces. It also covers casting, rolling, and annealing procedures and describes the basic steps in aluminum and titanium production. primary metal production rolling steel refining A GENERAL DIAGRAM...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120005
EISBN: 978-1-62708-269-3
... for marine and chemical processing operations. Fig. 2.7 Titanium usage in Boeing aircraft from the first commercial jet to the Boeing 757 Fig. 2.2 Investment cast titanium transmission case for Osprey vertical take-off and landing aircraft Fig. 2.3 Forged titanium landing gear...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060085
EISBN: 978-1-62708-261-7
... of castings are also produced for copper, magnesium, and zinc alloys. Casting is also important in the production of titanium components and in directionally solidified and single-crystal superalloys for use in the production of high-performance turbine blades. Titanium castings have been cast in machined...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480353
EISBN: 978-1-62708-318-8
... Compounds Other Salt Solutions Fresh Water/Steam Seawater Nitric Acid Reducing Acids Organic Chemicals Alkaline Media Corrosion Resistance of Titanium Alloys Erosion Resistance Heat Transfer Fabrication Cutting Machining Welding Casting Titanium is fully...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.9781627082693
EISBN: 978-1-62708-269-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120001
EISBN: 978-1-62708-269-3
... of titanium services in the world. Since titanium operations start with the availability of sponge and then ingot for remelt, casting, or for subsequent working, it is desirable that some players in the titanium market be identified. The primary producers of titanium sponge and ingot in the United States...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120131
EISBN: 978-1-62708-269-3
... replacements to facio-maxillary bone plates. Biomedical applications should see continued growth and the potential introduction of additional alloys. As previously noted, the current temperature limit of conventionally processed wrought and cast titanium alloys is about 595 °C (1100 °F). This limit is due...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120055
EISBN: 978-1-62708-269-3
... identified as annealing are: Hot isostatic pressing (HIP) has become an accepted method for the closure of internal solidification shrinkage or gas porosity in titanium castings. It also is used in P/M processing. Because thermal conditions between 899 and 955 °C (1650 and 1750 °F) are used for two...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240607
EISBN: 978-1-62708-251-8
..., compositions, and performance-cost tradeoffs of common MMCs, including aluminum-matrix composites, titanium-matrix composites, and fiber-metal laminates. It also explains how fiber-reinforced composites and laminates are made, describing both continuous and discontinuous fiber matrix production processes...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550001
EISBN: 978-1-62708-307-2
... Castings , Casting , Vol 15 , ASM Handbook , ASM International , 2008 10.31399/asm.hb.v15.a0005337 1.7 Forming of Titanium and Titanium Alloys , Forming and Forging , Vol 14 , ASM Handbook , ASM International , 1988 1.8 Niu M.C.Y. , Composite Airframe Structures , 2nd ed...