1-20 of 436 Search Results for

titanium alloy castings

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120039
EISBN: 978-1-62708-269-3
... to Ti-6Al-4V, beta transus temperature approximately 995 °C (1825 °F). (b) GFC, gas fan cooled. (c) RT, room temperature Typical room-temperature tensile properties of titanium alloy castings (bars machined from castings) Table 6.2 Typical room-temperature tensile properties...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550223
EISBN: 978-1-62708-307-2
..., compositions, and grades of commercially pure titanium and alpha and near-alpha, alpha-beta, and beta titanium alloys. It describes primary and secondary fabrication processes, including melting, forging, forming, heat treating, casting, machining, and joining as well as powder metallurgy and direct metal...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480161
EISBN: 978-1-62708-318-8
... as a temporary alloying element Research base Porous materials Less than 100% dense materials Research base Titanium alloys used for producing cast parts Table 8.2 Titanium alloys used for producing cast parts Alloy designation Alloy class Remarks Commercially pure titanium Oxygen...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240527
EISBN: 978-1-62708-251-8
... on melting, forging, casting, heat treating, and secondary fabrication. It also discusses the advantages and disadvantages of titanium and its alloys in various applications. melting primary fabrication forging casting heat treatment secondary fabrication titanium titanium alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120095
EISBN: 978-1-62708-269-3
... sample. (e) Annealed for 2 h at 650 °C (1200 °F) Cast titanium alloys with estimates of relative casting usage Table 12.15 Cast titanium alloys with estimates of relative casting usage Alloy Estimated relative use of castings Nominal composition, wt% Special properties (a) (b...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120005
EISBN: 978-1-62708-269-3
... beam for Boeing 757 aircraft Fig. 2.5 Some areas of titanium use in the F-22 Raptor advanced fighter aircraft Fig. 2.6 Typical titanium alloy casting for aircraft gas turbine use. Courtesy of Precision Castparts Corp. Fig. 2.1 Some titanium and titanium alloys product...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120047
EISBN: 978-1-62708-269-3
... of wrought, cast, and P/M titanium alloy products Table 7.2 Comparison of typical room-temperature properties of wrought, cast, and P/M titanium alloy products Product and condition Tensile strength Yield strength Elongation, % Reduction in area, % Charpy impact strength Fracture toughness...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740001
EISBN: 978-1-62708-308-9
...: Ref 1 Ironmaking Steelmaking Alloy Steel Refining Stainless Steel Refining Ingot Casting Continuous Casting Rolling Aluminum Production Titanium Production Acknowledgment References References 1. McGannon H.E. , The Making, Shaping, and Treating...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540411
EISBN: 978-1-62708-309-6
...Abstract Abstract This appendix provides tensile property data for titanium alloys and castings and plane-strain fracture toughness data for Ti-6Al-4V castings. alpha-beta titanium alloys beta titanium alloys titanium castings plane-strain fracture toughness tensile properties...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550001
EISBN: 978-1-62708-307-2
... Castings , Casting , Vol 15 , ASM Handbook , ASM International , 2008 10.31399/asm.hb.v15.a0005337 1.7 Forming of Titanium and Titanium Alloys , Forming and Forging , Vol 14 , ASM Handbook , ASM International , 1988 1.8 Niu M.C.Y. , Composite Airframe Structures , 2nd ed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120295
EISBN: 978-1-62708-269-3
... Grover Beach, CA 93483 Tel: 805-489-5144 Fax: 805-489-5352 Titanium and titanium alloys, 0.0008 in. and larger, spooled or cut to length, ribbon, square, sheets, and special shapes, for aerospace, military/defense, medical, and other electronic instrumentation and applications Cast Alloys Inc. 703...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.9781627082693
EISBN: 978-1-62708-269-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120001
EISBN: 978-1-62708-269-3
... and tested for applications requiring higher-temperature capability, but economic application for industrial and commercial use is going to be limited for many years. Wrought titanium alloy products are the more readily available, but castings are close behind. Wrought alloys also have the greatest...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120131
EISBN: 978-1-62708-269-3
... replacements to facio-maxillary bone plates. Biomedical applications should see continued growth and the potential introduction of additional alloys. As previously noted, the current temperature limit of conventionally processed wrought and cast titanium alloys is about 595 °C (1100 °F). This limit is due...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240607
EISBN: 978-1-62708-251-8
... reinforced with 10 vol% of alumina particles; 6061/SiC/47f is the alloy 6061 reinforced with 47 vol% of continuous SiC fibers; and A356/C/05c is the casting alloy A356 reinforced with 5 vol% of chopped graphite fibers. 33.1.1 Discontinuously Reinforced Aluminum Composites 33.1.2 Processing DRA...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870537
EISBN: 978-1-62708-314-0
... concepts. Source: Ref 10 Fig. 20.12 Squeeze casting. Source: Ref 6 Fig. 20.21 Silicon carbide monofilament/titanium matrix composite Fig. 20.34 Rod-reinforced niobium carbide/niobium eutectic. Source: Ref 7 Fig. 20.31 Diamond-impregnated core drill and coolant...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120345
EISBN: 978-1-62708-269-3
.... , Comparative Evaluation on Ti-10V-2Fe-3Al Cast, PM and Wrought Product Forms , Powder Metall. Int. , Vol 17 ( No. 5 ), 1985 , p 239 – 240 • Breslauer E. and Rosen A. , Relationship between Microstructure and Mechanical Properties in Metastable Beta Titanium 15-3 Alloy , Mater. Sci...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550299
EISBN: 978-1-62708-307-2
... such as niobium, chromium, manganese, vanadium, tantalum, and tungsten. Gamma titanium aluminide alloys can be processed by ingot metallurgy, powder metallurgy, or by casting to final shape ( Fig. 6.12 ). Fig. 6.12 Processing methods and routes for gamma titanium aluminides. HIP, hot isostatic pressing; HP...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120143
EISBN: 978-1-62708-269-3
...Key to the abbreviations used in the titanium alloy datasheets Table B.1 Key to the abbreviations used in the titanium alloy datasheets Abbreviation Definition Aged Aged AH Age hardened Ann Annealed Apps Applications As Weld As welded Auto Automotive Ave...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060333
EISBN: 978-1-62708-261-7
... S.R. , Principles of Beta Transformation and Heat Treatment of Titanium Alloys Lesson 4 , ASM Course: Titanium and Its Alloys, revised by Bania P.J. , ASM International , 1994 , p 1 – 23 Annealing Wrought and cast aluminum alloys are commonly designated by a series originally...