Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170528
EISBN: 978-1-62708-297-6
...Abstract Abstract This article examines the role of alloying in the production and use of lead and tin. It describes the various categories and grades of lead and lead-base alloys along with their nominal compositions and corresponding UNS numbers. It also discusses the composition...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980195
EISBN: 978-1-62708-342-3
... enable a wide spectrum of materials to be extruded. This chapter focuses on the processes involved in the extrusion of semifinished products in various metals and their alloys, namely tin, lead, lead-base soft solders, tin-base soft solders, zinc, magnesium, aluminum, copper, titanium, zirconium, iron...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980567
EISBN: 978-1-62708-342-3
... , lead, tin, and zinc alloys. Approximate composition of aluminum alloys Table 1 Approximate composition of aluminum alloys Material Similar UNS No. Si Fe Cu Mn Mg Cr Zn Other Al 5182 A95182 0.2 max 0.35 max 0.15 max 0.5 max 4.0–5.0 0.1 max 0.25...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910237
EISBN: 978-1-62708-250-1
... in material selection, and discuss, where appropriate, the characteristic forms of corrosion that attack specific materials. The materials addressed in this chapter include carbon steels, weathering steels, and alloy steels; nickel, copper, aluminum, titanium, lead, magnesium, tin, zirconium, tantalum...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980009
EISBN: 978-1-62708-342-3
... extruded through the shape-forming aperture of the extrusion die enables cross-sectional shapes to be produced that cannot be manufactured by any other hot-working process. The favorable deformation conditions with nonferrous metals such as tin and lead alloys as well as magnesium and aluminum alloys...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240075
EISBN: 978-1-62708-251-8
.... The major eutectic systems include the aluminum-silicon eutectic system and the lead-tin eutectic system. The chapter discusses the construction of eutectic phase diagrams from free energy curves. It also provides information on peritectic, monotectic, and solid-state reactions in alloy systems...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240597
EISBN: 978-1-62708-251-8
...Abstract Abstract This chapter discusses the compositions, properties, and applications of nonferrous metals, including zirconium, hafnium, beryllium, lead, tin, gold, silver, and platinum group metals. It also addresses fusible alloys and provides melting temperatures for several compositions...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080423
EISBN: 978-1-62708-304-1
... in such heat-transfer systems are subject to molten metal corrosion as well as other problems. This chapter reviews the corrosion behavior of alloys in molten aluminum, zinc, lead, lithium, sodium, magnesium, mercury, cadmium, tin, antimony, and bismuth. It also discusses the problem of liquid metal...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850509
EISBN: 978-1-62708-260-0
...Abstract Abstract This appendix provides a list of etch compositions and procedures that reveal the macrostructure of aluminum, beryllium, bismuth, antimony, cobalt, copper, lead, magnesium, nickel, tin, titanium, zinc, and their respective alloys as well as iron, steel, noble metals...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850610
EISBN: 978-1-62708-260-0
...Abstract Abstract This appendix contains tables that list the composition and capabilities of etchants that reveal the microstructure of metals and alloys, including aluminum, chromium, cobalt, copper, lead, magnesium, molybdenum, nickel, niobium, palladium, platinum, radioactive metals, rare...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060315
EISBN: 978-1-62708-261-7
... less tin than other alloying elements, such as manganese bronze (copper-zinc plus manganese, tin, and iron) and leaded tin bronze (copper-lead plus tin and sometimes zinc). The generic term bronze also applies to copper-base alloys containing no tin, such as aluminum bronze (copper-aluminum), silicon...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130541
EISBN: 978-1-62708-284-6
... (Yb) 20–33 11–18 Pure Indium (In) 25–28 14–16 Lead tin solder 27–29 15–16 Commercially pure or low-alloyed lead 28 16 Tin silver 23–24 13–19 9xx.x series cast aluminum plus other elements 29 16 Pure Lead (Pb) 28–30 16–17 Pure Thallium (Tl) 26–32 14–18 Magnesium...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170457
EISBN: 978-1-62708-297-6
... 0.09 C51000 94.8 Cu, 5 Sn, 0.2 P 8.86 (0.320) 17.9 (9.9) 69 (40) 15 0.09 C51100 95.6 Cu, 4.2 Sn, 0.2 P 8.86 (0.320) 17.8 (9.9) 84 (48.4) 20 0.09 Copper-tin-lead-phosphorus alloys (leaded phosphor bronzes, C53400–C53500) C54400 88 Cu, 4 Sn, 4 Pb, 4 Zn, 0.5 P max. 8.88 (0.321...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.t53730011
EISBN: 978-1-62708-283-9
... of solubility in the two phases. A phase diagram also may be thought of as a map of permissible phases. Equilibrium between two components consists of single-phase regions and two-phase regions. In a solid alloy of lead and tin, solid lead can dissolve tin, and solid tin can dissolve lead. Figure 2.2...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290165
EISBN: 978-1-62708-306-5
... metal. Lead, for example, does not alloy with iron and will not wet it. Tin, on the other hand, does form an alloy with iron, so a tin-lead solder will wet steel. Fig. 7.2 Principle of capillary attraction for selected liquids sandwiched between two clean glass plates: (a) when immersed in water...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240469
EISBN: 978-1-62708-251-8
... No. Composition Wrought alloys Coppers C10100-C15760 >99% Cu High-copper alloys C16200-C19600 >96% Cu Brasses C20500-C28580 Cu-Zn Leaded brasses C31200-C38590 Cu-Zn-Pb Tin brasses C40400-C49080 Cu-Zn-Sn-Pb Phosphor bronzes C50100-C52400 Cu-Sn-P Leaded phosphor bronzes...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060073
EISBN: 978-1-62708-261-7
... as a weapon. Bronze, developed by alloying copper with tin, had useful strengths, could be hardened by forging, and could be cast to shape. The discovery of bronze significantly altered the development of civilization. Lead was soft, easily worked, and could be made into vessels; later in history it was made...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300163
EISBN: 978-1-62708-323-2
... copper today comes from rocks that contain maybe only 5% copper, but copper did exist in mass form intertwined with rocks. Early mining in the United States involved smashing rock intertwined with metallic copper and picking out the metallic portion. Some other metals such as iron, tin, and lead have...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420087
EISBN: 978-1-62708-310-2
..., the solidification and scale of eutectic structures, and the competitive growth of dendrites and eutectic colonies or cells. It also examines the different types of precipitation structures that form during slow cooling cycles. aluminum-silicon alloys eutectic systems lead-tin-alloys microstructure...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.9781627082976
EISBN: 978-1-62708-297-6