Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780383
EISBN: 978-1-62708-281-5
... only after the oxide is removed. Solder pastes do not have flux that is active enough to remove Ni 3 O 4 . This problem was solved by substituting solder plating (tin/lead) for nickel plating. X-ray photoelectron spectroscopy analysis of a vapor phase reflowed coupon that was not fluxed showed 3.8...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.t53730129
EISBN: 978-1-62708-283-9
... if the plating is scratched. (b) Tin plating offers no cathodic protection so the steel will corrode if the plating is scratched. Stress corrosion can occur in some metals when loaded in tension in a specific environment. Cracks run through grains and along grain boundaries. Brass is susceptible to stress...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220445
EISBN: 978-1-62708-259-4
... surface views of tin plates. In recent years, the quenching and partitioning (Q&P) technique has been developed as an alternative route to obtaining microstructures containing controlled amounts of retained austenite ( Ref 13 , 14 ). In this technique, a steel with an adequate chemical...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
... Moderate to good Ion plating: Al, other metals (few alloys) ARE : TiN and other compounds Electronic, optical, decorative. Corrosion and wear resistance. Dry lubricants. Thicker engineering coatings Sputtering RT–0.7 T m of metal coatings. Best >200 for nonmetals Line of sight Metals, alloys...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.t51230207
EISBN: 978-1-62708-351-5
...-29Cu 510 950 660 1220 Bushby and Scott [1995] (a) Estimated, but not measured Fig. 6.2 Plot of shear strength as a function of brazing temperature for diffusion-brazed assemblies, each comprising a foil of copper plated on both sides with a 2 μm (80 μin.) thick layer of tin...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240323
EISBN: 978-1-62708-251-8
...) Nickel-base alloys (passive) Cu-35%Zn brass Nickel-base alloys (active) Manganese bronze Cu-40%Zn Tin Lead 316 stainless steel (active) 50%Pb-50%Sn solder 410 stainless steel (active) Cast iron Low-carbon steel 2024 aluminum 2017 aluminum Cadmium Alclad...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610501
EISBN: 978-1-62708-303-4
... Comparison of zinc and tin plating on steel. Source: Ref 2 Fig. 13 Exfoliation corrosion. (a) Around a fastener hole in 7049-T73 aluminum alloy longeron. (Radial lines indicate measurements taken to assess damage.) Source: Ref 7 . (b) In aluminum plate, 7178-T651, exposed to maritime environment...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350001
EISBN: 978-1-62708-315-7
... via sacrificial protection of steel substrate Hot-dip aluminizing Improved corrosion and oxidation resistance of steel substrate Hot-dip lead-tin alloy-coatings (terne coatings) Improved corrosion resistance of steel substrate Tin plate (continuous electrodeposition) Improved corrosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300335
EISBN: 978-1-62708-323-2
..., then the use of a TiN-coated drill may make it possible to achieve 500. For decades, many of the surface enhancements competed with chromium plating; it is the hardest metal at 70+ HRC, it is very abrasion resistant, and it does not rust. Thermal spray suppliers for decades have been working on a thermal...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290165
EISBN: 978-1-62708-306-5
... metal. Lead, for example, does not alloy with iron and will not wet it. Tin, on the other hand, does form an alloy with iron, so a tin-lead solder will wet steel. Fig. 7.2 Principle of capillary attraction for selected liquids sandwiched between two clean glass plates: (a) when immersed in water...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410551
EISBN: 978-1-62708-265-5
... and Dies , Krauss G. and Nordberg H. , Ed., Colorado School of Mines Press , Golden, CO , p 217 – 230 22.40 Molarius J.M. , Korhonen A.S. , Harju E. , and Lappalainen R. , Comparison of Cutting Performance of Ion-Plated NbN, ZrN, TiN, and (Ti,Al)N Coatings...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870191
EISBN: 978-1-62708-299-0
...) on aluminum beacon housing. (f) X-ray map showing the thickness of copper/tin plate (arrows) on aluminum antenna blade. Fig. 1 (Part 1) Examples of how design and assembly can affect localized corrosion by creating crevices and traps where corrosive liquids can accumulate. (a) Storage containers...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060175
EISBN: 978-1-62708-261-7
..., with up to 0.4% Mn. Typical uses are in automobile body panels, tin plate, and wire products. These steels have relatively low tensile values (205 to 240 MPa, or 30 to 35 ksi) and are selected when enhanced cold formability or drawability is required. For rolled steel structural plates and sections...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350125
EISBN: 978-1-62708-315-7
...Abstract Abstract This chapter discusses the use of coating methods and materials and their impact on corrosion and wear behaviors. It provides detailed engineering information on a wide range of processes, including organic, ceramic, and hot dip coating, metal plating and cladding, and the use...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2004
DOI: 10.31399/asm.tb.ps.t62440189
EISBN: 978-1-62708-352-2
... ( Minneapolis , MN ), p 296 – 301 • Ho C.T. , 1996 . Nickel and Copper Coated Carbon Fibre Reinforced Tin-Lead Alloy Composite , J. Mater. Sci. , Vol 31 , p 5781 – 5786 10.1007/BF01160828 • Ho C.T. and Chung D.D.L. , 1990 . Carbon Fibre Reinforced Tin-Lead Alloy as a Low...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910331
EISBN: 978-1-62708-250-1
... 0.50 9 Chromium plated; tin plated; 12% Cr type corrosion-resistant steels −0.45 0.60 10 Tin-plate; ternplate; tin-lead solder −0.50 0.65 11 Lead, solid or plated; high-lead alloys −0.55 0.70 12 Aluminum, wrought alloys of the 2000 series −0.60 0.75 13 Iron, wrought, gray...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170528
EISBN: 978-1-62708-297-6
...Abstract Abstract This article examines the role of alloying in the production and use of lead and tin. It describes the various categories and grades of lead and lead-base alloys along with their nominal compositions and corresponding UNS numbers. It also discusses the composition...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2004
DOI: 10.31399/asm.tb.ps.t62440145
EISBN: 978-1-62708-352-2
... rate of platinum in tin-base solder at selected temperatures Temperature Dissolution rate °C °F 80 180 (solid-state aging) 1.0 nm/day 200 390 0.3 nm/s 270 520 1.2 nm/s 320 610 2.2 nm/s Solderable metallizations are usually applied by either wet plating or vapor...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350183
EISBN: 978-1-62708-315-7
... Fig. 14 Compares the abrasion resistance of TiN coatings applied by various thin-film processes Fig. 15 Compares the surface hardness of hardened tool steel and a cemented carbide with that of the following surface-hardening processes: TRD, CVD, PVD, boriding, chrome plating, electroless...