1-7 of 7 Search Results for

thixocasting

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740047
EISBN: 978-1-62708-308-9
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550033
EISBN: 978-1-62708-307-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140021
EISBN: 978-1-62708-335-5
.... Important variations include molding and pattern distinctions such as lost-foam (evaporative pattern), shell and V-mold, and process derivatives such as squeeze casting, low-pressure permanent mold, vacuum riserless casting, and semisolid forming based on rheocasting/thixocasting principles. Many...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410029
EISBN: 978-1-62708-280-8
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060085
EISBN: 978-1-62708-261-7
... microstructure of the semisolid mass. Fig. 5.11 Microstructure of a thixocast (semisolid process) AZ91 magnesium alloy. (a) Conventional etching. (b) Electrolytic etching and polarized light illumination. Color helps distinguish grain orientation and the ratio of minimum to maximum grain diameters...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550621
EISBN: 978-1-62708-307-2
... of techniques, ranging from relatively simple sand or die casting to very intricate permanent mold, investment castings, and the newer thixocasting and squeeze casting technologies. When the quantities are small, sand casting is probably the most cost-effective. As the quantities become larger, permanent mold...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.9781627083355
EISBN: 978-1-62708-335-5