Skip Nav Destination
Close Modal
Search Results for
thermoforming techniques
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-17 of 17 Search Results for
thermoforming techniques
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870183
EISBN: 978-1-62708-314-0
... Abstract This chapter discusses thermoplastic composite fabrication processes and related equipment and procedures. The discussion covers consolidation and thermoforming operations as well as joining methods. composite fabrication consolidation joining thermoforming thermoplastic...
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550385
EISBN: 978-1-62708-307-2
..., and high-temperature and corrosion behaviors are determined by the orientation, shape, and spacing of fibers, the number of plies, resin properties, and consolidation and forming methods. The chapter also covers secondary fabrication processes, such as thermoforming, machining, and joining, as well...
Abstract
Polymer-matrix composites are among the lightest structural materials in use today. They are also highly resistant to corrosion and fatigue and their load-carrying capabilities, such as strength and stiffness, can be tailored for specific applications. This chapter discusses the primary advantages and disadvantages of polymer-matrix composites, how they are produced, and how they perform in different applications. It describes the construction of laminates, the fibers and resins used, and the methods by which they are combined. It explains how strength, modulus, toughness, and high-temperature and corrosion behaviors are determined by the orientation, shape, and spacing of fibers, the number of plies, resin properties, and consolidation and forming methods. The chapter also covers secondary fabrication processes, such as thermoforming, machining, and joining, as well as production equipment and product forms, and include guidelines for optimizing tradeoffs when selecting fibers, resins, and production techniques.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.t53730139
EISBN: 978-1-62708-283-9
... may be grown by directional solidification. With the Bridgman technique, a mold is slowly removed from a furnace ( Fig. 13.1 ). Freezing starts at one end and slowly progresses to the other. Because freezing starts at a point, only one crystal is nucleated. The Czochralski method involves lowering...
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780064
EISBN: 978-1-62708-281-5
... Methods<xref rid="t69780064-fn1" ref-type="fn">[1]</xref> The primary plastics processing methods are: Injection molding Extrusion Thermoforming Blow molding Rotational molding Compression molding/transfer molding Composites processing Casting Other plastics...
Abstract
This article describes key processing methods and related design, manufacturing, and application considerations for plastic parts and includes a discussion on materials and process selection methodology for plastics. The discussion covers the primary plastic processing methods and how each process influences part design and the properties of the plastic part. It also includes a brief description of functional requirements in process selection; an overview of various process effects and how they affect the functions and properties of the part; and the selection of processes for size, shape, and design detail factors.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780051
EISBN: 978-1-62708-281-5
...% of forming uses blow molding (10% of all plastics), thermoforming, compression molding, coating, laminating, rotational molding, and all others. However, injection molding is the most important, and, except for compression or transfer molding of thermosets, is usually the most accurate in maintaining...
Abstract
To ensure the proper application of plastics, one must keep in mind three factors that determine the appropriate end-use: material selection, processing, and design. This article begins by providing information on various factors pertinent to the anticipated use conditions of the article to be designed. This is followed by a discussion on several stages necessary to define the geometry of plastic parts. Details on the strength of and cost estimation for plastic parts are then provided. The article ends with a section providing information on the structure, properties, processing, and end-use applications of plastics.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870255
EISBN: 978-1-62708-314-0
... of liquid water in the cells that does the majority of the damage. Many field reports blame water ingression on “poor” sealing techniques. Good sealing practices are important, but in most cases it is just a matter of time until water finds its way into the core of most honeycomb designs and initiates...
Abstract
This chapter discusses the advantages and disadvantages of sandwich and integral cocured structures, and the methods by which they are made. It begins by explaining where and how sandwich construction is used and why it is so efficient. It then describes the design and fabrication of honeycomb panels and foam cores along with their respective applications and unique attributes. The chapter also discusses the cocuring process and its use in fabricating unitized structures.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780028
EISBN: 978-1-62708-281-5
... introduces the basic concepts of polymer structure and properties. This article describes in more detail the importance of chemical composition and morphology to mechanical properties and reviews basic plastic processing techniques. Table 1 and Fig. 1 show the structures and transition temperature...
Abstract
This article describes in more detail the fundamental building-block level, atomic, then expands to a discussion of molecular considerations, intermolecular structures, and finally supermolecular issues. An explanation of important thermal, mechanical, and physical properties of engineering plastics and commodity plastics follows, and the final section briefly outlines the most common plastics manufacturing processes.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780164
EISBN: 978-1-62708-281-5
... be representative of some severe industrial environments. In this case, the time-to-track technique is used because time is needed to decompose the contaminant solution and to build up conducting residues on the sample surface. Very track resistant materials, such as PMMA, may erode rather than track under more...
Abstract
This article discusses electrical testing and recommended procedures for determining the electrical properties of insulating materials, with particular emphasis on plastics. It describes the electrical characteristics of various forms of plastics and also presents definitions of the terms used in connection with testing and specifying plastics for electrical applications.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550325
EISBN: 978-1-62708-307-2
... be thermoformed into structural shapes by simply reheating to the processing temperature. Thermosets, due to their highly cross-linked structures, cannot be reprocessed and will thermally degrade and eventually char if heated to high-enough temperatures. Many thermoplastics are polymerized by what is called...
Abstract
This chapter describes the molecular structures and chemical reactions associated with the production of thermoset and thermoplastic components. It compares and contrasts the mechanical properties of engineering plastics with those of metals, and explains how fillers and reinforcements affect impact and tensile strength, shrinkage, thermal expansion, and thermal conductivity. It examines the relationship between tensile modulus and temperature, provides thermal property data for selected plastics, and discusses the effect of chemical exposure, operating temperature, and residual stress. The chapter also includes a section on the uses of thermoplastic and thermosetting resins and provides information on fabrication processes and fastening and joining methods.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220281
EISBN: 978-1-62708-341-6
... technique rather than as a metal heating process per se. In this chapter, some of the special applications of induction heating which make use of the above features are summarized. These include applications in the plastics, packaging, electronics, glass, and metal-finishing industries. Induction...
Abstract
Induction heating has found widespread use as a method to raise the temperature of a metal prior to forming or joining, or to change its metallurgical structure. However, induction heating has specialized capabilities that make it suitable for applications outside of metal treatment and fabrication. This chapter summarizes some of the special applications of induction heating, including those in the plastics, packaging, electronics, glass, chemical, and metal-finishing industries. The chapter concludes with a discussion of the application of induction heating for vacuum processes.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780359
EISBN: 978-1-62708-281-5
... Abstract This article reviews various analytical techniques most commonly used in plastic component failure analysis. The description of the techniques is intended to make the reader familiar with the general principles and benefits of the methodologies. The descriptions of the analytical...
Abstract
This article reviews various analytical techniques most commonly used in plastic component failure analysis. The description of the techniques is intended to make the reader familiar with the general principles and benefits of the methodologies. The descriptions of the analytical techniques are supplemented by a series of case studies that include pertinent visual examination results and the corresponding images that aided in the characterization of the failures. The techniques covered include Fourier transform infrared spectroscopy, differential scanning calorimetry, thermogravimetric analysis, thermomechanical analysis, and dynamic mechanical analysis. The article also discusses various analytical methods used to characterize the molecular weight distribution of a polymeric material. It provides information on a wide range of mechanical tests that are available to evaluate plastics and polymers, covering the various considerations in the selection and use of test methods.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870063
EISBN: 978-1-62708-314-0
Abstract
This chapter discusses the use of thermoset and thermoplastic resins in polymer matrix composites. It begins by explaining how the two classes of polymer differ and how it impacts their use as matrix materials. It then goes on to describe the characteristics of polyester, vinyl ester, epoxy, bismaleimide, cyanate ester, polyimide, and phenolic resins and various toughening methods. The chapter also covers thermoplastic matrix materials and product forms and provides an introduction to the physiochemical tests used to characterize resins and cured laminates.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780216
EISBN: 978-1-62708-281-5
... of failure. Where possible, well-defined examples of impact events are given, as well as techniques for analyzing and predicting those events. Because puncture resistance is an important characteristic associated with impact behavior, the large-strain material properties of plastics and their relationship...
Abstract
This article discusses the material and engineering issues associated with plastic components subjected to impact. The first part covers the effects of loading rate, temperature, and state of stress on both deformation and mode of failure. It discusses standard impact tests, along with their associated results. A brief discussion on the linear elastic fracture mechanics method is presented, along with an example of its effectiveness as a predictive tool for impact performance. Various issues with a bearing on impact performance, such as processing, chemical attack, and aging, are also described. The second part describes the engineering calculations used to predict the performance of thin plastic beams, plates, and shells. The issue of assuming small displacements for the calculation of plastic structure performance is discussed and its limitations described. An example of the consequence of the very low modulus of elasticity associated with plastics and some plastic design solutions are offered.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780003
EISBN: 978-1-62708-281-5
... of the polymer. For example, special processing techniques are used to produce polymer fibers. Such fibers have substantially greater stiffness and strength along their length than do the unoriented polymers from which they are manufactured. This is because special processing has been used to orient the covalent...
Abstract
This introductory article describes the various aspects of chemical structure and composition that are important to an understanding of polymer properties and their eventual effect on the end-use performance of engineering plastics, namely thermoplastics and thermosets. The most important properties of polymers and the most significant influences of structure on those properties are covered. The article also includes some general information on the classification and naming of polymers and plastics.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.9781627082839
EISBN: 978-1-62708-283-9
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550621
EISBN: 978-1-62708-307-2
... • • • • • • • • — — — — — Electrochemical machining • • • • — — — — • • — X X Electrical discharge machining (EDM) X • • • • • — — — • — X X Wire EDM X • • • • • — — — • — • X Forming Sheet metal forming X • • • • • — — — — X X X Thermoforming X X X X X X X X X...
Abstract
This chapter consists of three parts. The first part provides data and guidelines for selecting materials and processing routes. It compares the basic properties of metals, ceramics, and polymers, identifies important measures of performance, and discusses manufacturing processes and their compatibility with specific materials. The chapter then presents general guidelines for selecting lightweight materials, and concludes with a review of lightweight metals, plastics, and composites used in automotive applications.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610327
EISBN: 978-1-62708-303-4
... -curves of three Si 3 N 4 ceramic materials measured by the short rod chevron notch technique. Adapted from Ref 8 Fig. 9 Rising R -curve of a SiC whisker-reinforced alumina-ceramic-matrix composite, measured by the double-cantilever beam technique. Adapted from Ref 8 Fatigue...
Abstract
This chapter covers the fatigue and fracture behaviors of ceramics and polymers. It discusses the benefits of transformation toughening, the use of ceramic-matrix composites, fracture mechanisms, and the relationship between fatigue and subcritical crack growth. In regard to polymers, it covers general characteristics, viscoelastic properties, and static strength. It also discusses fatigue life, impact strength, fracture toughness, and stress-rupture behaviors as well as environmental effects such as plasticization, solvation, swelling, stress cracking, degradation, and surface embrittlement.