Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860133
EISBN: 978-1-62708-348-5
.../andp.19003060312 Fevrier A. and Morize D. (1973) . The effect of magnetic field on the thermal conductivity and electrical resistivity of different materials. Cryogenics 13 , 603 – 606 . 10.1016/0011-2275(73)90114-8 Gladun C. and Holzhauser W. (1964...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780115
EISBN: 978-1-62708-281-5
..., thermogravimetric analysis, thermomechanical analysis, and rheological analysis. The basic thermal properties covered include thermal conductivity, temperature resistance, thermal expansion, specific heat, and the determination of glass-transition temperatures. The article further describes various factors...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110196
EISBN: 978-1-62708-247-1
...-Induced Resistance Change/Thermally-Induced Voltage Alteration and Seebeck Effect Imaging. Lastly, the article discusses the application of solid immersion lenses to improve spatial resolution. References References 1. Wills K.S. , Lewis T. , Billus G. , and Hoang H...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860515
EISBN: 978-1-62708-348-5
... C. Y. , and Kreitman M. M. ( 1973 ). Use of linear heat flow for poor conductors and its application to the thermal conductivity of nylon . Cryogenics 13 , 34 – 40 . 10.1016/0011-2275(73)90263-4 Barber C. R. ( 1950 ). Platinum resistance thermometers of small dimensions...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110219
EISBN: 978-1-62708-247-1
... to the thermal attenuation, the applicable electrical power, and the electrical resistance value of the defect. The power spectrum in Figure 4 shows that the power at the individual frequencies (harmonics in this case) decreases as frequency increases, resulting in a decreasing SNR that may prevent...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310279
EISBN: 978-1-62708-286-0
... resistivity. The mechanical properties listed include yield strength, tensile strength, elongation and hardness. stainless steel density modulus of elasticity coefficient of thermal expansion thermal conductivity specific heat electrical resistivity yield strength tensile strength elongation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030025
EISBN: 978-1-62708-282-2
... cations and corrodent anions) so that the scale has a slow growth rate High melting temperature Good adherence to the metal substrate, which usually involves a coefficient of thermal expansion close to that of the metal, and sufficient high-temperature plasticity to resist fracture from differential...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240469
EISBN: 978-1-62708-251-8
... and aluminum. The attributes of copper include availability, excellent formability, good strength when alloyed, high thermal conductivity, good corrosion resistance, and a pleasing color. However, it is the very high electrical conductivity of pure copper that leads to its extensive use as electrical wiring...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240487
EISBN: 978-1-62708-251-8
...Abstract Abstract Aluminum has many outstanding properties, leading it to be used for a wide range of applications. It offers excellent strength-to-weight ratio, good corrosion and oxidation resistance, high electrical and thermal conductivity, exceptional formability, and relatively low cost...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050009
EISBN: 978-1-62708-311-9
.... electrical resistivity induction heating magnetic permeability skin effect specific heat thermal conduction INDUCTION HEATING was first studied when it was found that heat was produced in transformer and motor windings, as mentioned in Chapter 1, “History of Metallurgy and Induction Heating...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430087
EISBN: 978-1-62708-253-2
... operating point comes greater efficiency, as well as greater demand on construction materials. This chapter discusses the primary requirements for boiler tube materials, including oxidation and corrosion resistance, fatigue strength, thermal conductivity, and the ability to resist creep and rupture. It also...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240607
EISBN: 978-1-62708-251-8
...Abstract Abstract Metal-matrix composites (MMCs) work at higher temperatures than their base metal counterparts and can be engineered for improved strength, stiffness, thermal conductivity, abrasion and/or creep resistance, and dimensional stability. This chapter examines the properties...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230131
EISBN: 978-1-62708-298-3
... resistance, and density. It explains how beryllide intermetallics are formed using sputter deposition, diffusion, and powder metal methods. beryllides intermetallic compounds mechanical properties oxidation resistance thermal properties 11.1 Background and Historical Information 11.2...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500317
EISBN: 978-1-62708-317-1
... hardening, case (surface) hardening, and nitriding as well as hard chrome plating, vapor deposition, and thermal diffusion coating. It explains how to measure wear resistance using various tests and provides guidelines for selecting tool materials, treatments, and coatings. chemical vapor deposition...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110499
EISBN: 978-1-62708-247-1
... know-how-based analysis techniques of array failures by bitmap classification. The limits of bitmapping that lead to well-known localization techniques like thermally induced voltage alteration and optical beam induced resistance change are also discussed. The article concludes by providing information...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120055
EISBN: 978-1-62708-269-3
... are used to make titanium stronger, tougher, more ductile, and easier to machine as well as more resistant to the effects of corrosion and thermal and mechanical fatigue. It describes accepted practices for stress relieving, aging, annealing, and post-treatment processing along with associated challenges...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.fdmht.t52060001
EISBN: 978-1-62708-343-0
..., dislocation movement, and grain boundary sliding. It describes these mechanisms in qualitative terms, explaining how they are driven by thermal energy and how they can be analyzed using creep curves and deformation maps. In addition, it examines the types of damage associated with creep, presents a number...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.t53730161
EISBN: 978-1-62708-283-9
...Abstract Abstract This appendix contains a table listing density, thermal conductivity, linear expansion, electrical resistivity, and Young's modulus of various materials. density electrical resistivity linear expansion thermal conductivity Young's modulus ...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240303
EISBN: 978-1-62708-251-8
... temperature Table 17.1 Physical properties of some metals at room temperature Metal Density, g/cm 3 Specific heat capacity ( C p ), kJ/kg · K Coefficient of linear thermal expansion, μm/m · K Thermal conductivity, W/m · K Electrical resistivity, nΩ · m Aluminum 2.6989 0.900 22.8 247...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870063
EISBN: 978-1-62708-314-0
... premature failure due to fiber microbuckling. The matrix also provides the composite with toughness, damage tolerance, and impact and abrasion resistance. The properties of the matrix also determine the maximum usage temperature, resistance to moisture and fluids, and thermal and oxidative stability...