Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310161
EISBN: 978-1-62708-286-0
... Abstract This chapter discusses different thermal processes applicable to the various alloy groups of stainless steels, namely austenitic, ferritic, martensitic, precipitation hardening, and duplex stainless steels. The processes discussed include soaking, annealing, stress relieving...
Image
Published: 01 August 2013
Fig. 9.4 Thermal processes for TWIP Fe-24Mn steel. Source: Ref 9.3 More
Image
Published: 01 August 2015
Fig. 10.25 Continuous bar heating: thermal profile of a steel bar as processed through an eight-coil induction line. Source: Ref 11 More
Image
Published: 01 November 2013
Fig. 9 Schematic of the basic thermal evaporation process with an electron beam heating source. Source: Ref 6 More
Image
Published: 01 December 2015
Fig. 2 Forms of kinetic curves that represent various thermal degradation processes More
Image
Published: 01 June 2008
Fig. 21.12 Thermal spraying processes used for hardfacing. Adapted from Ref 5 More
Image
Published: 01 June 2022
Figure 3 Types of thermal spray processes. HVOF, high velocity oxy-fuel; HVLF, high velocity liquid-fuel; HVAF, high velocity air-fuel; APS. air plasma spray; LPPS/LVPS, low pressure plasma spray/low vacuum plasma spray; CAPS, controlled atmospheric plasma spray More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310123
EISBN: 978-1-62708-286-0
... Abstract This chapter discusses the metallurgy, phase structure, thermal processing, and applications of martensitic stainless steels. The phenomenon of martensite formation is explained. A table listing the compositions of martensitic stainless steels is also presented. martensitic...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2022
DOI: 10.31399/asm.tb.tstap.t56040010
EISBN: 978-1-62708-428-4
... Abstract This article provides a brief description of commercially important thermal spray processes and gives examples of applications and application requirements. The processes covered are flame, wire arc, plasma, high-velocity oxyfuel processes, detonation gun, and cold spray methods...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310201
EISBN: 978-1-62708-286-0
... Abstract This chapter provides a basis for understanding the influence of stainless steel alloy composition and metallurgy on the welding process, which involves complex dynamics associated with melting, refining, and thermal processing. It begins with an overview of the welding characteristics...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030169
EISBN: 978-1-62708-282-2
... contain magnesium and/or manganese. The alloys in this series are strengthened by thermal processing. These alloys attain high strengths and are used in sheet, plate, and extruded forms, primarily in aerospace applications. Copper in aluminum alloys generally decreases the resistance to general corrosion...
Image
Published: 01 August 2018
Fig. 17.41 Gray cast iron with acicular structure. Graphite flakes in a matrix of bainitic ferrite and retained austenite. ASTM A644 defines as “ausferrite” “a cast iron matrix microstructure, produced by a controlled thermal process, which consists of predominantly acicular ferrite and high More
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.pnfn.t65900119
EISBN: 978-1-62708-350-8
... unpredictable dimensional change in a component due to thermal processing or temperature variations and loading in service. This chapter describes two types of distortion: size distortion and shape distortion. It addresses how distortion can be managed by controlling certain factors. The chapter discusses...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550511
EISBN: 978-1-62708-307-2
... thermal expansion Bearings and bushings, close tolerance fittings, extrusion and forming dies, spindles, metal-forming rolls and tools, coordinate-measuring machine structures Thermal processing Heat recovery, hot-gas cleanup, general thermal processing Thermal stress resistance, corrosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2022
DOI: 10.31399/asm.tb.tstap.t56040020
EISBN: 978-1-62708-428-4
... Abstract This article summarizes the results of work completed by the ASM Thermal Spray Society Advisory Committee to identify key research challenges and opportunities in the thermal spray field. It describes and prioritizes research priorities related to emerging process methods, thermal...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300335
EISBN: 978-1-62708-323-2
... the treatment adds dimension to the treated surface. The treatments that coat (additive) and those that do not intentionally increase dimension include: Not additive: Texturize surfaces, work hardening, thermal processing of the substrate, and so on Additive: Vacuum coat, paint, thermal spray, dip...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2022
DOI: 10.31399/asm.tb.tstap.t56040001
EISBN: 978-1-62708-428-4
... of wear, such as abrasion, erosion, and scuffing Heat insulation or conduction Prevention of oxidation and hot corrosion Electrical conduction or insulation Near-net-shape manufacturing Sealing Engineered emissivity Abradable coatings Decoration Thermal spray processes...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460209
EISBN: 978-1-62708-285-3
... as a fabrication technology for components. Consequently, cold spray can be an alternative coating process to the protective coating method for automotive components. In the case of the thermal spray process, which is conventionally applied to the protective coating of vulnerable automobile parts, oxidation...