1-20 of 180 Search Results for

textured structure

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480095
EISBN: 978-1-62708-318-8
..., and strengthened through deformation processes. This chapter describes the structural changes that occur in titanium during deformation and how they can be controlled. It discusses the role of slip, dislocations, and twinning, the effect of grain size and crystal orientation, the concept of texture strengthening...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220403
EISBN: 978-1-62708-259-4
... 12.7 Warm Working—Working in the Intercritical Region 12.8 Cold Forming of Parts—Fasteners as Examples 12.9 Defects in Cold Forming 12.1.1 Stress-Strain Curve in the Tensile Test 12.1.2 The Effects of Deformation on Structure 12.3.1 Identifying Crystallographic Textures 12.3.2...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980141
EISBN: 978-1-62708-342-3
... Casting and Cast Structure, Homogenizing of Aluminum Alloys 4.3 Development of the Continuous Cast Structure Additional Information 2: Representation of Textures in Pole Figures Additional Information 3: Temperature and Speed Dependence of the Flow Stress in Hot Working...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610209
EISBN: 978-1-62708-303-4
... Microstructure Effect of Texture on Fatigue Life High-Cycle Fatigue Strength Notch Effects Effects of Surface Treatments Fatigue Crack Growth of Titanium Alloys Metallurgical Effects on Titanium FCG The material in this chapter came from “ Fracture Resistance of Structural Alloys ” by K.S...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300335
EISBN: 978-1-62708-323-2
... the very first solid-film lubricant. The classic solid-film lubricants are intercalative materials; they have two-dimensional crystal structures, and they slide on each other in layers. Solid-film lubricants can be dusted on a surface and burnished into the surface texture. They are available...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120331
EISBN: 978-1-62708-269-3
...Symbols Table I.1 Symbols Symbol Description α Hexagonal close-packed (hcp) crystal structure in Ti-base alloys α′ Solute-lean, hcp, martensite α″ Solute-rich, orthorhombic, martensite α-2 Ordered intermetallic compound near Ti 3 Al in Ti-Al alloys β Body-centered...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230295
EISBN: 978-1-62708-298-3
... , Forming and Forging , Vol 14 , ASM Handbook , ASM International , p 805 – 808 Grant L.A. , and Hardesty R.E. , 1990 . Fabrication of Stable Lightweight Beryllium Optical Support Structures , Dimensional Stability , Vol 1335 , Paquin R.A. , Ed., SPIE , p 140 – 155 10.1117...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240117
EISBN: 978-1-62708-251-8
.... Crystallographic texture should not be confused with mechanical fibering or flow lines. Although both will produce directional mechanical properties in deformed metal structures, mechanical fibering is obtained by the alignment of inclusions and second-phase particles in the direction of working and is usually...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700199
EISBN: 978-1-62708-279-2
... Research and Development ,” Auto/Steel Partnership presentation at 2009 U.S. Department of Energy (DOE) Hydrogen Program and Vehicle Technologies Program Annual Merit Review and Peer Evaluation Meeting , May 18–22, 2009 ( Arlington, VA ) 13.4 Liang X. , “ Structure and Mechanical Properties...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230361
EISBN: 978-1-62708-298-3
... W.R. , and Huegel F.J. , 1967 . “ CVD Tungsten and Tungsten-Rhenium Alloys for Structural Applications ,” UCRL Preprints 70340, Parts I and II, Lawrence Livermore National Laboratory , Livermore, CA Hsieh E. , 1988 . Film Deposition and Status, UCID 21384 , Survivability...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090303
EISBN: 978-1-62708-266-2
..., because a more homogeneous structure can be produced. Texture plays an important role in the transgranular SCC of zirconium, and information regarding anisotropy and texture can be used to control SCC. The ideal texture is one in which the basal planes are perpendicular to the potential plane...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230209
EISBN: 978-1-62708-298-3
..., impurities, and strain rate), on the mechanical properties of beryllium is reported in this chapter. In general, ductility and strength improve as the grain size is reduced. An increase in BeO content generally results in a decrease in ductility and an increase in strength. The degree of isotropy (texture...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120095
EISBN: 978-1-62708-269-3
... 0.20 240 35 170–310 25–45 24 ASTM grade 12 (UNS R53400) 0.10 0.25 0.03 0.30 480 70 380 55 12 (a) Unless a range is specified, all listed values are minimums. (b) Only for sheet, plate, and coil Effect of test direction on mechanical properties of textured Ti-6Al-2Sn-4Zr...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630101
EISBN: 978-1-62708-270-9
... of nonfused particles. The circular features on the flat fractures are porosity. Ductile fractures may not always have the classic cup-and-cone or dimpled structures shown in this chapter. High-strength, high-hardness, high-alloy metals may possess a rough texture with very fine dimples, as shown...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410233
EISBN: 978-1-62708-265-5
...-CARBON STEELS, steels that contain less than 0.25% C, make up the highest tonnage of all steels produced in a given year. Structural shapes and beams for buildings and bridges, plate for line pipe, and automotive sheet applications are just a few major applications for low-carbon steels...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300121
EISBN: 978-1-62708-323-2
... Tribotesting Tribosystem Testing Velocity Tribotesting Environment Tribosystem Surface Texture during Testing Defining Tribotest Duration Material Characterization and Selection for Tribotesting Summary—Test Variables Tribotest Metrics Tribotesting Methods This may seem intuitive...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560039
EISBN: 978-1-62708-291-4
...Abstract Abstract This chapter discusses the composition and structure of low-carbon irons and steels, particularly those used in the production of hot-rolled strip. It describes the manufacturing process from the production of ingots to coiling, and it explains how finishing and coiling...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.9781627083232
EISBN: 978-1-62708-323-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310109
EISBN: 978-1-62708-286-0
... with thickness for 29Cr-4Mo-2Ni alloy. Source: Ref 12 Abstract Abstract This chapter discusses the alloy composition, metallurgy, mechanical behavior, stabilization, texture, anisotropy, high-temperature properties, and corrosion and oxidation resistance of ferritic stainless steels. References...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300079
EISBN: 978-1-62708-323-2
... particles), and this is the situation with droplet erosion. However, metal coatings such as thermal spray deposits of metals, cermets, and ceramics can be susceptible to damage by fracture. Often, the coatings can spall since they are held to metal surfaces by mostly mechanical locking to surface texture...