1-20 of 28 Search Results for

texture evolution modeling

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700199
EISBN: 978-1-62708-279-2
... of Fe-Mn Alloys, ” master’s thesis, McMaster University, July 2008 13.5 Curtze S. , Kuokkala V.-T. , Hokka M. , and Saarinen T. , Microstructure and Texture Evolution in High Manganese TWIP Steels , Proc. DYMAT 2009 , Vol 2 , Sept 7–11 , 2009 ( Brussels, Belgium...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460121
EISBN: 978-1-62708-285-3
... CHARACTERIZATION is an inherent aspect of the cold spray coating evaluation process. Characterization of the as-sprayed microstructures enables the development of an understanding of the thermomechanical evolution of the coating and elucidates the bonding mechanisms both within the coating and at the coating...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870201
EISBN: 978-1-62708-314-0
.... 7.31 Volatile evolution of K-IIIB prepreg. Source: Ref 5 Abstract Abstract This chapter provides an overview of the tools and techniques, as well as some of the underlying theory, that have proven useful for process modeling and simulation. It begins by presenting the framework...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400089
EISBN: 978-1-62708-316-4
...Abstract Abstract This chapter discusses the factors that must be considered when selecting a lubricant for sheet metal forming operations. It begins with a review of lubrication regimes and friction models. It then describes the selection and use of sheet metal forming lubricants, explaining...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410163
EISBN: 978-1-62708-265-5
... Second Canada-Japan Symposium on Modern Steelmaking and Casting Techniques , Jonas J.J. , Boyd J.D. , and Sano N. , Ed., TMS of the Canadian Institute of Mining, Metallurgy and Petroleum , Montreal, Quebec, Canada , 1994 9.11 Thomas B.G. , Modeling of the Continuous...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220551
EISBN: 978-1-62708-259-4
.... Figures 16.28 to 16.30 present structures of wrought duplex stainless steels. The detailed characterization of the structure evolution during hot working of these steels can be found in Ref 24 . Austenitic stainless steel castings have their structure well described by these models, as shown...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780404
EISBN: 978-1-62708-281-5
... to have started first due to residual stresses developed during injection molding. Failure seems to have occurred due to fatigue crack propagation, as indicated by the presence of discontinuous crack-growth bands and their evolution. Although a tensile-stress component normal to the fracture surface...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230295
EISBN: 978-1-62708-298-3
.... For this reason, all beryllium products should be formed at elevated temperatures, generally 540 to 815 °C (1000 to 1500 °F) and at slow speeds. The primary factors influencing the formability of beryllium are grain size, texture, impurity content, prior metalworking history, ductility as a function...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310127
EISBN: 978-1-62708-326-3
... of intergranular corrosion. 10% oxalic acid, original magnification: 500×. Images courtesy of Jon Dossett Fig. 3 Microstructure evolution during annealing of cold-worked (rolled) Al-Mg alloy (5005, Al-Mg1) and effect on room temperature tensile yield strength (red curve) and elongation (blue curve...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.9781627083232
EISBN: 978-1-62708-323-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220129
EISBN: 978-1-62708-259-4
... Dendrites, Iowa State University , private communication 9. Ruxanda R. , Beltran-Sanchez L. , Massone J. , and Stefanescu D.M. , On the eutectic Solidification of Spheroidal Graphite Iron—An Experimental and Mathematical Modeling Approach , Proceedings of Cast Iron Division, AFS...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410315
EISBN: 978-1-62708-265-5
... of the Deformation of Patented Steel Wire , Metall. Trans. , Vol 1 , 1970 , p 465 – 477 10.1007/BF02811557 15.38 Langford G. , Deformation of Pearlite , Metall. Trans. A , Vol 8A , 1977 , p 861 – 875 10.1007/BF02661567 15.39 Zelin M. , Microstructure Evolution in Pearlitic...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500179
EISBN: 978-1-62708-317-1
.... and Skogsgårdh A. , Theoretical and Experimental Analysis of Stroke-Controlled Tube Hydroforming , Mater. Sci. Eng. A , Vol 279 ( No. 1–2 ), Feb 29 , 2000 , p 95 – 110 10.1016/S0921-5093(99)00646-2 9.25 Yang C. and Ngaile G. , Analytical Model for Planar Hydroforming: Prediction...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610585
EISBN: 978-1-62708-303-4
... Discontinuities Cracking Associated with Welding Porosity Inclusions Oxide Films Second Phases Hot Tears Metal Penetration Surface Defects Design and Service Considerations Fracturing Buckling and Wrinkling Shape Distortion Loose Metal Undesirable Surface Textures...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110351
EISBN: 978-1-62708-247-1
... maximum would be expected. [80] Figure 44 The variation of the electrical resistivity of the FIB deposited SiO 2 with increasing (a) Ga and (b) C content. The black filled circles are experimental data, while the red solid line in (a) represents the modeled fit to the experimental data. [80...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550223
EISBN: 978-1-62708-307-2
.... , Plastic Flow and Microstructure Evolution during Thermomechanical Processing of Laser-Deposited Ti-6Al-4V Preforms , Metall. Mater. Trans. A , Vol 32 , 2002 , p 1801 – 1811 10.1007/s11661-001-0156-0 • Shen G. and Furrer D. , Manufacturing of Aerospace Forgings , J. Mater. Process...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060013
EISBN: 978-1-62708-261-7
... problems with the Bohr model. Its predictions failed badly in atoms with just two electrons in their outermost shells, such as helium. And so a more accurate model of the atom was needed. More refined models were soon developed, and the evolution of atomic theory eventually led to the development...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610327
EISBN: 978-1-62708-303-4
... on the left) and craze tip (arrows on the right) at given cyclic intervals. (b) Model of discontinuous cracking process. Source: Ref 26 Fig. 31 Comparison of macroscopic fatigue crack growth rates and striation spacing measurements in epoxy, polycarbonate (PC), and polystyrene (PS). □, micro...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850060
EISBN: 978-1-62708-260-0
... texture studies of sheet metal, the sheet sample can be glued to a sheet of Plexiglas so that the planar surface can be polished. With rectangular mounts, the length should be kept no more than twice the width for best polishing results. In selecting a mounting material and technique, several factors...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.9781627083355
EISBN: 978-1-62708-335-5