1-20 of 165 Search Results for

tap testing

Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870333
EISBN: 978-1-62708-314-0
..., normal dye penetrants should never be used, because they can contaminate the internal surfaces of the delamination, making subsequent repair more difficult or impossible. Although tap testing is normally classified as a sonic test method, actually a low-frequency vibration method...
Image
Published: 01 August 1999
Tests done in normal room environment Water Tests done with the surface of the test piece wet. Results are similar regardless of whether wetting was with demineralized water, hard (tap) water, or a 3% brine solution More
Image
Published: 01 August 1999
Fig. 20 Correlation of accelerated test media with service environment (industrial atmosphere). Combined data for five lots of rolled plate of aluminum alloy 7039-T64 (4.0Zn-2.8Mg-0.3Mn-0.23Cr). Tests in 3.5% sodium chloride were similar to ASTM G 44, except salt solution was made More
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290009
EISBN: 978-1-62708-319-5
... the density attained through vibration but without compaction. The ratio of tap density to apparent density is a rough particle shape index. The larger this ratio, the less spherical are the particles. These tests are important to powder production, research and development, process control, and property...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220027
EISBN: 978-1-62708-341-6
... and a capacitor in parallel with an inductor and a resistor Tuning Capacitors Capacitor banks often are employed to tune induction heating circuits to obtain a resonant frequency close to the power-supply frequency. [2] Generally, such devices are of two types: oil-filled, multiple-tap units ( Fig. 3.6...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280189
EISBN: 978-1-62708-267-9
..., tool life, and practical issues such as set up time, tool changes, and production scheduling. It describes several machining processes, including turning, boring, planing, trepanning, shaping, broaching, drilling, tapping, thread milling, and grinding. It also provides information on toolholders...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310019
EISBN: 978-1-62708-286-0
...) × ∑ z i 2 C i D i Δ ϕ / L Test solution resistivity Table 2 Test solution resistivity Test solution Ratio by volume Resistivity, ohm-cm Natural Seawater … 25 Fresh (tap) water adjusted with seawater 28:1 500 Fresh (tap) water adjusted with seawater 68:l...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220047
EISBN: 978-1-62708-341-6
... efficiency and not to the “line-to-load” energy transfer. In radio-frequency systems, by contrast, IEEE Standard No. 54 defines the test used to determine power output. This standard describes the use of a calorimeter method for determining power into a load ( Fig. 4.2 ). In practice, a water-cooled...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050025
EISBN: 978-1-62708-311-9
... 100% down to a lower setting. Power supplies are available in which the output frequency can have a range of tuning control from 3 to 10 kHz. Some power supplies can switch frequencies by turning the power off, using a contactor to change capacitor taps for tuning, and then turning the power back...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290207
EISBN: 978-1-62708-306-5
... hand, selection may be dictated by a complex system of specification and qualification controls. The extent and complexity of the system needed are usually dictated by the probable cost of a fastener failure. Adequate testing is the safest method of guarding against failure of a new fastener system...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290085
EISBN: 978-1-62708-319-5
... Abstract This chapter is a detailed account of various attributes related to mixing and testing of powder-binder feedstocks. Mixing parameters and their effects on feedstock properties is discussed. The attributes reviewed include mixture homogeneity, wetting, powder-binder ratio, feedstock...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2023
DOI: 10.31399/asm.tb.edfatr.t56090063
EISBN: 978-1-62708-462-8
... and IEEE 1687 Modeling of Non-TAP Interfaces . in 2021 IEEE European Test Symposium (ETS) 1 – 10 ( 2021 ). 10.1109/ETS50041.2021.9465438 . 5. IEEE P1687.2 Working Group WebPage , https://sagroups.ieee.org/1687-2/sample-page/ ( 2021 ). 6. IEEE P2427 Working Group Webpage , https...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050301
EISBN: 978-1-62708-311-9
... the boiling temperature of the quenchant being used. Brinell. A hardness tester that uses balls to make an impression. A mea- surement of the diameter of the indent is made. A table is used to con- vert the diameter of the indent in millimeters to the Brinell hardness number (BHN). The test is often used...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.9781627083119
EISBN: 978-1-62708-311-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110643
EISBN: 978-1-62708-247-1
... by digital loopback BIST. Control of test mode functions, like loopback or BIST, is widely implemented using the IEEE 1149.1 [3] standard (often called “JTAG”, after the joint test action group that initiated its development). This standard specifies a 4-pin or 5-pin standard test access port (TAP...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2023
DOI: 10.31399/asm.tb.edfatr.t56090021
EISBN: 978-1-62708-462-8
... product arena ever since ( Ref 35 ). The standard test access port (TAP) controller is modified to detect timing-related faulty behaviors, shorts, and opens using the boundary scan architecture, as shown in Fig. 38 ( Ref 36 ). Fig. 38 Boundary scan architecture for interposer and TSV testing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320195
EISBN: 978-1-62708-332-4
... Schematic of alloying segregation. Source: Ref 1 10.1.1 Chemistry Requirements The chemistry limits listed here are for general guidance based on laboratory experiments with test bars quenched in a relatively large quench tank. In practice, casting configurations are complex, with different...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050001
EISBN: 978-1-62708-311-9
.... The first induction heaters sold by General Electric during World War II had rectifier tubes for the conversion of the alternating current (ac) to direct current (dc). Output control and tuning were accomplished through a combination of different taps on the output of the tank coil and a control knob...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550193
EISBN: 978-1-62708-307-2
... of different forms of beryllium alloys Table 4.5 Typical mechanical properties of different forms of beryllium alloys Material Test orientation (a) Ultimate tensile strength Yield strength (b) Elongation (c) , % MPa ksi MPa ksi Block Normal-purity (hot-pressed) structural...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.t59370013
EISBN: 978-1-62708-447-5
... for casting manufacturing. Raw materials are procured according to specifications to ensure suitable process control and outgoing product quality. Suppliers are provided with specifications, and samples are tested for compliance before source approval. They are asked to provide certification of compliance...