... + 1 where ρ = b 2 / a by definition. The subscript ∞ implies that the load is applied at infinity and the stress-concentration factor is actually the ratio of the local stress to the far-field gross area stress. This value reduces to 3 for a circular hole, identical to those given by Kirsch...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400033
EISBN: 978-1-62708-316-4
... failure occurs in the test for different punch corner radius-to-thickness ( r -to- t ) ratios. In general, height of failure increases with increases in the r -to- t ratio, as a smaller radius induces very high bending stress, resulting in failure at smaller height/punch strokes. Fig. 4.28 shows...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540391
EISBN: 978-1-62708-309-6
... are interchangeable. That means the engineer may substitute K SSF for K t when the situation warrants. These two factors ( K t and K SSF ) both represent the ratio of the peak elastic notch stress at a critical area to the maximum nominal stress S max . Actually, a K SSF includes a baseline K t...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400053
EISBN: 978-1-62708-316-4
... the principal stress and the plastic strain increments. Based on the experimental observations, the hypothesis postulates that the ratio of plastic strain increment is the same as the ratio of the principal deviatoric stress. This is commonly known as the Levy-Mises flow rule. In other words, the axis...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090001
EISBN: 978-1-62708-266-2
..., width, and aspect ratio, and (b) crack opening and crack-tip closure Stress-corrosion cracks can initiate and propagate with little outside evidence of corrosion and with no warning as catastrophic failure approaches. The cracks frequently initiate at surface flaws that either preexist...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030126
EISBN: 978-1-62708-282-2
... segregation, and residual stresses Crack geometry, which includes length, width, and aspect ratio; and crack opening and crack tip closure Stress-corrosion cracks can initiate and propagate with little outside evidence of corrosion and no warning as catastrophic failure approaches. The cracks...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780199
EISBN: 978-1-62708-281-5
... Abstract This article describes the general aspects of and practical problems of failure analysis of creep, stress relaxation, and yielding for homogeneous polymers. The effect of temperature and strain rate on the relationship between yield point and elastic modulus and the aging effect...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090241
EISBN: 978-1-62708-266-2
... Abstract Aluminum is protected by a barrier oxide film that, if damaged, reforms immediately in most environments. Despite this inherent corrosion resistance, there are conditions where aluminum alloys, like many materials, are subject to the effects of stress-corrosion cracking (SCC...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040083
EISBN: 978-1-62708-300-3
... to a uniaxial stress state for a limited reduction in height during the test. However, the frictional force at large compression ratio (a) starts to bulge the sample (i.e., inhomogeneous deformation) regardless of the quality of the lubricant and (b) affects the measured load-stroke curve. In other words...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090359
EISBN: 978-1-62708-266-2
... Abstract This chapter describes how ultrasonic testing came to be a viable method for evaluating intergranular stress-corrosion cracking (SCC) in large-diameter stainless steel pipe welds in boiling water reactor service. Intergranular SCC can be difficult to detect using nondestructive...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090367
EISBN: 978-1-62708-266-2
... Abstract This chapter addresses the challenge of selecting an appropriate stress-corrosion cracking (SCC) test to evaluate the serviceability of a material for a given application. It begins by establishing a generic model in which SCC is depicted in two stages, initiation and propagation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090043
EISBN: 978-1-62708-266-2
... Abstract This chapter addresses the issue of stress-corrosion cracking (SCC) in carbon and low-alloy steels. It discusses crack initiation, propagation, and fracture in aqueous chloride, hydrogen sulfide, sulfuric acid, hydroxide, ammonia, nitrate, ethanol, methanol, and hydrogen gas...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090349
EISBN: 978-1-62708-266-2
... Abstract This chapter examines the stress-corrosion cracking (SCC) failure of stainless steel pipe welds in boiling water reactor (BWR) service. It explains where most of the failures have occurred and provides relevant details about the materials of construction, fabrication techniques...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090067
EISBN: 978-1-62708-266-2
... Abstract High-strength steels are susceptible to stress-corrosion cracking (SCC) even in moist air. This chapter identifies such steels and the applications where they are typically found. It provides information on crack growth kinetics and crack propagation models in which hydrogen...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090419
EISBN: 978-1-62708-266-2
... and complex phase array systems have developed the ability to detect and size stress-corrosion cracks. Determining crack profiles based on historical crack length to crack depth ratios are insufficiently quantitative for fitness for service and engineering critical assessments ( Ref 18.2 ). Laser-induced...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090221
EISBN: 978-1-62708-266-2
... Abstract This chapter describes the conditions under which copper-base alloys are susceptible to stress-corrosion cracking (SCC) and some of the environmental factors, such as temperature, pH, and corrosion potential, that influence crack growth and time to failure. It explains that, although...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090191
EISBN: 978-1-62708-266-2
... Abstract Irradiation-assisted stress-corrosion cracking (IASCC) has been a topic of engineering interest since it was first reported in the 1960s, having been observed in stainless steel cladding on light water reactor fuel elements. This chapter summarizes the results of decades...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040025
EISBN: 978-1-62708-300-3
... Abstract This chapter explains how to determine flow stress and forgeability using data from tensile tests, compression tests, ring tests, and torsion tests. It describes sample preparation, tooling and equipment, test procedures, error sources, and data plotting techniques. It also provides...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090135
EISBN: 978-1-62708-266-2
... Abstract Nickel and nickel-base alloys are specified for many applications, such as oil and gas production, power generation, and chemical processing, because of their resistance to stress-corrosion cracking (SCC). Under certain conditions, however, SCC can be a concern. This chapter describes...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090271
EISBN: 978-1-62708-266-2
... Abstract Titanium alloys are generally resistant to stress-corrosion cracking (SCC), but under certain conditions, the potential for problems exists. This chapter identifies the types of service environments where titanium alloys have exhibited signs of SCC. It begins by describing the nominal...