Published: 01 December 2015
Fig. 22 Cavitation damage to an ACI CN-7M stainless steel cast pump impeller used to pump ammonium nitrate solution at 140 °C (280 °F). Courtesy of A.R. Wilfley and Sons, Inc., Pump Division More
Image
Published: 01 December 1995
Fig. 2-158 Non-magnetic (austenitic stainless steel) cylinder castings for a diesel engine which powers a mine sweeper. Weights 35 to 150 lb (16 to 68 kg) More
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310233
EISBN: 978-1-62708-326-3
... Abstract This chapter discusses the composition and classification of stainless steels and focuses on the processes involved in heat treatment and applications of these steels. The wrought and the cast stainless steels covered are ferritic, austenitic, duplex (ferritic-austenitic), martensitic...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310147
EISBN: 978-1-62708-286-0
... Abstract With typical alloy systems, casting is often the most convenient method by which to produce components. This is true for stainless steels, both for corrosion-resisting and for heat-resisting applications. This chapter discusses stainless steel casting alloys and their metallurgy...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240433
EISBN: 978-1-62708-251-8
... to refine stainless steel. The chapter also provides information on the classification and composition of stainless steel castings. It concludes with a brief description of the Schaeffler constitution diagram which is useful in predicting the type of stainless steel as a function of its alloy content...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080445
EISBN: 978-1-62708-304-1
... Abstract This appendix is a collection of tables listing the chemical compositions of wrought ferritic steels; wrought stainless steels; cast corrosion- and heat-resistant alloys; wrought iron-, nickel-, and cobalt-base alloys; cast nickel- and cobalt-base alloys; oxide-dispersion-strengthened...
Image
Published: 01 June 1983
Figure 11.25 The effect of δ -ferrite and nitrogen content on the tensile properties at 4 K of CF8M austenitic stainless steel castings. The castings in the δ -ferrite study contained 0.05% N and the castings in the nitrogen study contained 9 ± 1% δ -ferrite ( Whipple and McHenry, 1982 ). More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2010
DOI: 10.31399/asm.tb.hss.t52790241
EISBN: 978-1-62708-356-0
... 300-series numbers, and “51” preceded the AISI three-digit 400-series numbers. Thus, AISI 304 became SAE 30303, and AISI 410 became SAE 51410. For the stainless steel casting alloys, the prefix “60” was to precede AISI designations with comparable corrosion-resisting compositions to the Alloy Casting...
Image
Published: 01 August 2018
Fig. 16.18 Constitution diagram by Siewert, McCowan, and Olson for the estimation of the solidification mode of stainless steel castings, adapted from Ref 13 . The numbers on the lines in the regions where ferrite is present are the volumetric fraction of ferrite (FN) in the steel More
Image
Published: 01 June 1983
Figure 11.26 The effect of δ -ferrite on the fracture toughness at 4 K of CF8M austenitic stainless steel castings containing 0.05% N ( Whipple and McHenry, 1982 ). More
Image
Published: 01 December 1995
Fig. 20-6 Constitution diagram for estimation of ferrite content in stainless steel castings within the composition range of 16-26Cr, 6-14Ni, 4 max Mo, 1 max Cb, 0.2 max C, 0.19 max N, 2 max Mn, 2 max Si More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030167
EISBN: 978-1-62708-282-2
... (approximately 10.5 wt%) of chromium and, depending on the alloy, other elements such as nickel, molybdenum, and nitrogen. Figure 1 shows the effects of selected alloying elements on a 19Cr-9Ni stainless steel casting alloy. The corrosion resistance of stainless steels is based on the protective nature...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2010
DOI: 10.31399/asm.tb.hss.t52790235
EISBN: 978-1-62708-356-0
... steels S xxxxx Stainless steels, valve steels, and superalloys H xxxxx AISI H-steels T xxxxx Tool steels J xxxxx Cast steels W xxxxx Welding filler metals and electrodes K xxxxx Miscellaneous steels and ferrous alloys Z xxxxx Zinc and zinc alloys The procedure...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.tt2.t51060273
EISBN: 978-1-62708-355-3
... Nickel-base superalloys 1186 172 276 40 Alloy steels, cast; quenched and tempered 1172 170 772 112 Stainless steels; cast 1138 165 214 31 Tantalum and its alloys 1089 168 331 48 Steel P/M parts; heat treated 1062 154 517 75 Ductile (nodular) irons, cast 1034 150 276...
Image
Published: 01 December 1995
Fig. 2-151 Beater casting for dough mixing equipment. Stainless cast steel CF-8M More
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060291
EISBN: 978-1-62708-261-7
... the classification, composition, properties, treatments, and applications of austenitic, ferritic, martensitic, duplex, precipitation-hardening, powder metallurgy, and cast stainless steels. It also reviews the history of stainless steels and provides information on alloy designation systems. austenitic...
Image
Published: 01 March 2002
Fig. 7.33 Micrographs of AISI 316L stainless steel powder particles mounted in a castable epoxy mount. (a) 50× and (b) 400× More
Image
Published: 01 January 2000
Fig. 29 Erosion-corrosion of a cast stainless steel pump impeller after exposure to hot concentrated sulfuric acid with some solids present. Note the grooves, gullies, waves, and valleys common to erosion-corrosion damage. More
Image
Published: 01 August 2018
Fig. 16.31 As-cast ASTM A890/A890M Grade 6A duplex stainless steel. The composition has been adjusted for FA solidification. Austenite (light, dendritic) and interdendritic ferrite. Etchant: Beraha II. Courtesy of M. Martins. (See also Ref 25 ). More
Image
Published: 01 August 2018
Fig. 16.33 ASTM A890/A890M Grade 6A cast duplex stainless steel annealed at 1100 °C (2010 °F) and quenched. Austenite (light) and ferrite. The annealing temperature defines the volume fraction of the phases present, for each specific chemical composition. Etchant: Beraha II. Courtesy of M More