... of corrosion behavior between cast and wrought product forms. austenitic stainless steels ferritic stainless steels high-performance stainless steels duplex stainless steels corrosion corrosion testing corrosion prevention METALLURGICAL VARIABLES can influence the corrosion behavior...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030096
EISBN: 978-1-62708-282-2
... Abstract This chapter discusses various factors that affect corrosion of stainless steel weldments. It begins by providing an overview of the metallurgical factors associated with welding. This is followed by a discussion on preferential attack associated with weld metal precipitates...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030176
EISBN: 978-1-62708-282-2
... Abstract Stainless steels and nickel-base alloys are recognized for their resistance to general corrosion and other categories of corrosion. This chapter examines the effects of specific alloying elements, metallurgical structure, and mechanical conditioning on the corrosion resistance...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170257
EISBN: 978-1-62708-297-6
... Abstract This article covers the metallurgy and properties of stainless steels. It provides composition information on all types of ferritic, austenitic, martensitic, duplex, and precipitation-hardening stainless steels, including proprietary and nonstandard grades, along with corresponding...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000023
EISBN: 978-1-62708-312-6
... Abstract Stainless steel powders are usually made by water or gas atomization. This chapter describes both processes and the properties and characteristics of the powders they produce. It also discusses secondary processes, including drying, screening, annealing, and lubricating...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000101
EISBN: 978-1-62708-312-6
... Abstract This chapter describes the most effective ways to improve the corrosion resistance of sintered stainless steels, including increasing alloy content, optimizing the sintering process, and the use of surface treatments and modifications. alloying element corrosion resistance...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000219
EISBN: 978-1-62708-312-6
... Abstract This appendix provides property data, including strength, tensile properties, elastic constants, and hardness, for 300-series powder metal stainless steels. elastic constants hardness powder metallurgy stainless steel strength tensile properties Table A1.1 gives...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000221
EISBN: 978-1-62708-312-6
... Abstract This appendix provides property data, including strength, tensile properties, elastic constants, and hardness, for 400-series powder metal stainless steels. elastic constants hardness powder metallurgy stainless steel tensile properties Table A2.1 gives minimum...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820043
EISBN: 978-1-62708-339-3
... Abstract Austenitic stainless steels exhibit a single-phase, face-centered cubic structure that is maintained over a wide range of temperatures. This chapter provides a basic understanding of grade designations, properties, and welding considerations of austenitic stainless steels. It also...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820077
EISBN: 978-1-62708-339-3
... Abstract Ferritic stainless steels are essentially iron-chromium alloys with body-centered cubic crystal structures. Chromium content is usually in the range of 11 to 30%. The primary advantage of the ferritic stainless steels, and in particular the high-chromium, high-molybdenum grades...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820099
EISBN: 978-1-62708-339-3
... Abstract Duplex stainless steels are two-phase alloys based on the iron-chromium-nickel system. Duplex stainless steels offer corrosion resistance and cost advantages over the common austenitic stainless steels. Although there are some problems with welding duplex alloys, considerable progress...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820115
EISBN: 978-1-62708-339-3
... Abstract Martensitic stainless steels are essentially iron-chromium-carbon alloys that possess a body-centered tetragonal crystal structure (martensitic) in the hardened condition. Martensitic stainless steels are similar to plain carbon or low-alloy steels that are austenitized, hardened...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090095
EISBN: 978-1-62708-266-2
... Abstract This chapter takes a practical approach to the problem of stress-corrosion cracking (SCC) in stainless steels, explaining how different application environments affect different grades of stainless steel. It describes the causes of stress-corrosion cracking in chloride, caustic...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410579
EISBN: 978-1-62708-265-5
... Stainless steels derive their name from their exceptional corrosion resistance, which is attributed to their finely tuned compositions. This chapter discusses the alloying elements used in stainless steels and the some of the processing challenges they present. One of the biggest challenges...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.9781627082860
EISBN: 978-1-62708-286-0
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 May 2018
DOI: 10.31399/asm.tb.hma.t59250093
EISBN: 978-1-62708-287-7
... Abstract This chapter discusses the development of stainless steel. It begins with some information on the discovery of stainless steel. This is followed by a discussion on the most important patents issued for stainless steel. Applications of stainless steel beyond their original use...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700151
EISBN: 978-1-62708-279-2
... Abstract This chapter is a brief account of the composition, microstructures, heat treatment, deformation mechanisms, mechanical properties, formability, and special attributes of austenitic stainless steels. chemical composition microstructure heat treatment deformation mechanical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310069
EISBN: 978-1-62708-286-0
... Abstract This chapter discusses the compositions, mechanical properties, phase structure, stabilization, corrosion resistance, and advantages of austenitic stainless steels. Austenitic alloys are classified and reviewed in three groups: (1) lean alloys, such as 201 and 301, which are generally...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310091
EISBN: 978-1-62708-286-0
... Abstract This chapter provides information on the structure, design aspects, mechanical properties, forming, machining, and corrosion resistance characteristics of duplex stainless steels. The different types of corrosion covered are general corrosion, pitting corrosion, crevice corrosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310109
EISBN: 978-1-62708-286-0
... Abstract This chapter discusses the alloy composition, metallurgy, mechanical behavior, stabilization, texture, anisotropy, high-temperature properties, and corrosion and oxidation resistance of ferritic stainless steels. ferritic stainless steels alloy composition mechanical behavior...