... Transmission electron microscopy images of splat-cooled Ni-37.5Al (at.%) showing accommodating martensite groupings. Source: Ref 15.15 as published in Ref 15.13 Historically, martensitic transformations in metal alloys (specifically steel) have been studied the most, but recent attention has also...