... by spinning Table 12.1 Effect of process variables in forming of a round cup by spinning Parameter\target value h D max s min TW SQ Round-off radius (ñ) ↑ ↓ ↑ ↑ ↑ Feed ( f ) ↑ ↔ ↑ ↓ ↓ Spindle speed (s) ↓ ↔ ↓ ↑ ↑ Number of passes ( n ) ↔ ↔...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480293
EISBN: 978-1-62708-318-8
... ... ... ... ... Modern machine tools ... -- X X ... ... ... ... Speed/feed/cutting fluid ... X ... X X X X ... Careful handling ... ... ... ... X ... ... ... Stress relief ... ... ... ... X X ... ... Surface grinding Table 13.23 Surface grinding Material...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860007
EISBN: 978-1-62708-338-6
... increased efficiency. Extractors were developed to remove a part off the mandrel in seconds rather than minutes. High-speed extractors, complete with automated cutting/grinding of the pipe ends, were set up to handle the higher-volume production needs. Fig. 2.7 Two-spindle pipe winder with in-line...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740213
EISBN: 978-1-62708-308-9
... removed, in. 3 /min (cm 3 /min); rpm, revolutions per minute of work or cutter; T s , torque at spindle, in. · lb (N · m); t , cutting time, minutes; V c , cutting speed, ft/min (m/min); w , width of cut, in. (mm). (a) Unit power data are given in Table 8 for turning, milling, and drilling...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230339
EISBN: 978-1-62708-298-3
... these machining operations are conducted and describes the effect of tooling materials, cutting speeds, metal-removal rates, and other variables. It also explains how to assess and remove surface damage caused by machining such as microcracks and twins. beryllium machining surface damage 21.1 Overview...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250089
EISBN: 978-1-62708-345-4
... the type of gear as the major variable and discusses the machining methods best suited to specific conditions. Next, the chapter provides information on gear cutter material and nominal speeds and feeds for gear hobbing. Further, it describes the cutting fluids recommended for gear cutting and presents...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050057
EISBN: 978-1-62708-311-9
.... 4.9 Dual-spindle scanner with coils. Source: Ref 2 Fig. 4.27 Curved channel coil with concentrators. Source: Ref 12 Fig. 4.28 Multiturn channel coil. Source: Ref 12 Fig. 4.33 Two-turn pancake coil. Source: Ref 12 Fig. 4.34 Butterfly coil. Source: Ref...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050215
EISBN: 978-1-62708-311-9
... toward quench cracking because of the part geometry and hardness requirements. A 24% polymer quenchant is considered in this table to produce the same rate as that produced by a fast-speed oil. These recommendations are from commerical practice. Optimum hardness can be produced when the microstructure...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050173
EISBN: 978-1-62708-311-9
... in the quench water. Sometimes enough residual heat can be left in the parts that any remaining water evaporates. Under continuous conditions, air blasts may remove the water. Rotating spindles with workpieces can have a rotation speed high enough to spin off the water. Polymer quenches present a different...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120079
EISBN: 978-1-62708-269-3
... High-temperature nickel and cobalt-base alloys 200–360 2.5 2.0 2.0 Aluminum alloys 30–150 (500 kg) 0.25 0.16 0.32 (a) Power requirements at spindle drive motor, corrected to 80% spindle drive efficiency. Dull tools may require 25% more power. HSS, high-speed steel Some typical...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740103
EISBN: 978-1-62708-308-9
... 10 Capacities of various types of forging hammers Table 2 Capacities of various types of forging hammers Type of hammer Ram weight Maximum blow energy Impact speed Number of blows per minute kg lb kJ ft · lb m/s ft/s Board drop 45–3,400 100–7,500 47.5 35,000 3–4.5...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.9781627083386
EISBN: 978-1-62708-338-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050191
EISBN: 978-1-62708-311-9
... and carries the hot pins to one of three quench spindles. The dual grip enables the previously quenched pin to be removed from centers, with the hot pin then placed into the centers. The pin is rotated and quenched uniformly with a polymer quenchant. During quenching the gantry moves back to pick up the next...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400161
EISBN: 978-1-62708-316-4
... individual motor. Fig. 11.4 Schematic of servo presses with high-speed/low-torque servo-motors (a) with belt and ball screw drive and (b) with ball screw and linkage drive. Source: Ref 11.9 Fig. 11.5 A straight-side four-column press with four spindles directly driven by servo motors...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
... Electroless Nickel Plating Electroless Copper Plating Copper Plating Industrial Hard Chromium Plating Decorative Chromium Plating Nickel Plating Cadmium Plating Zinc Plating Tin Plating Polishing Buffing Barrel Finishing Vibratory Finishing Spindle Finishing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500211
EISBN: 978-1-62708-317-1
... sections. (c) Wide strip. (d) Narrow strip On the other hand, the output of the roll forming process is extremely high. Line speed can go up to 260 m/min (850 ft/min). After the appropriate setup of the line, the labor requirements are usually minimal. Different materials such as steel, stainless...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050025
EISBN: 978-1-62708-311-9
..., or thyristors) and transistors to operate at higher voltages, faster switching speeds, and higher temperatures with better operating characteristics. Newer induction systems are more efficient, more reliable, and more controllable due to magnetic components such as transformers, chokes, and reactors that reduce...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.pnfn.t65900193
EISBN: 978-1-62708-350-8
... component resisted scuffing and exhibited excellent resistance to frictional wear problems. The process was a great success with high-speed spindles and high-speed cutting tools. It did, however, require careful salt bath analysis on a daily basis ( Ref 1 ). Another challenge of the process...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040319
EISBN: 978-1-62708-300-3
..., 1999] Husmann J. , “ High Speed Ring Rolling and Closed-Die Rolling, ” presented at the FIA Conference ( Reno, NV ), May 1999 . [Ishinaga, 1996] Ishinaga N. , “ An Advanced Press Design for Cold Forging, ” Third International Cold and Warm Forging Technology Conference, SME...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050139
EISBN: 978-1-62708-311-9
... cooled that will cool fast enough to permit transformation to martensite without cracking or distortion. Therefore, the general recommendation for selection of a quenchant for induction heat treating is to select the fastest speed quenchant that will produce the desired hardness and case depth without...