1-20 of 129 Search Results for

solid-state sintering

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290137
EISBN: 978-1-62708-306-5
... Abstract Solid-state welding processes are those that produce coalescence of the faying surfaces at temperatures below the melting point of the base metals being joined without the addition of brazing or solder filler metal. This chapter discusses solid-state welding processes such as diffusion...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290169
EISBN: 978-1-62708-319-5
... Distribution, and Grain Growth Kinetics in Solid-Pore Systems , Crit. Rev. Solid State Mater. Sci. , Vol 35 , 2010 , p 263 – 305 10.1080/10408436.2010.525197 • German R.M. , “ MIM 17-4 PH Stainless Steel: Processing, Properties and Best Practice , Powder Inj. Mould. Int. , Vol 10 ( No. 2...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000059
EISBN: 978-1-62708-312-6
... boron-containing austenitic (316L) phase during solidification, assuming limited diffusion in the solid state, and found that the last fraction of solidified austenite was significantly decreased in both chromium and molybdenum. Becker et al. ( Ref 76 ) also made use of computer-calculated phase...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280149
EISBN: 978-1-62708-267-9
... welding techniques, defect prevention, fixturing, heat treatments, and general practices, including the use of filler metals. It also discusses several solid-state welding methods, superplastic forming, and transient liquid phase bonding, a type of diffusion welding process. The chapter includes extensive...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290201
EISBN: 978-1-62708-319-5
... – 127 10.1016/j.ijrmhm.2004.11.005 • Favrot N. , Besson J. , Colin C. , and Delannay F. , Cold Compaction and Solid-State Sintering of WC-Co Based Structures: Experiments and Modeling , J. Am. Ceram. Soc. , Vol 82 , 1999 , p 1153 – 1161 10.1111/j.1151-2916.1999.tb01889.x...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290193
EISBN: 978-1-62708-319-5
... strength-limiting defects. This idea is presented in the Weibull distribution. For ductile solids, significant deformation occurs after yielding but prior to failure, measured by the elongation to failure. High-ductility materials reach high permanent stretch prior to failure. Compression tests assume...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000167
EISBN: 978-1-62708-312-6
... 316L stainless steel using a number of different welding techniques. Their study included GTAW, GMAW, three types of resistance welding (namely, resistance spot welding, upset welding, and flash welding), friction welding (solid state), and arc stud welding. Except for friction welding, all other...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290279
EISBN: 978-1-62708-306-5
... mechanical fastening, adhesive bonding, and, for thermoplastic composites, welding; the making of glass-to-metal seals; and joining of oxide and nonoxide ceramics to themselves and to metals by solid-state processes and by brazing. The classification, types, applications, and the mechanism of each of these...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140165
EISBN: 978-1-62708-264-8
... relationship between cooling rate, grain size, grain shape, and phase structures. It explains how the transition from liquid to solid state creates the conditions under which microsegregation occurs, and how it impacts the distribution of alloying elements, carbides, and inclusions. The link between...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560125
EISBN: 978-1-62708-291-4
... route that involves solid-state sintering of compressed powder—the powder metallurgy route. We need to note two points before discussing the structures of steels produced in this manner. First, carbon analyses are unreliable as indicators of the carbon present in the metallic regions of the product...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240017
EISBN: 978-1-62708-251-8
... , 2005 • Sadoway D.R. , “ The Imperfect Solid State ,” Lecture notes, Introduction to Solid-State Chemistry, Department of Materials Science and Engineering, Massachusetts Institute of Technology, Fall 2006 A point defect is an irregularity in the lattice associated with a missing...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740373
EISBN: 978-1-62708-308-9
... powders are mixtures of several components that alloy with each other during sintering by solid-state diffusion. In the presence of large particles, the sintering times of such systems would be unacceptably long. The lower end of the particle size spectrum of typical P/M powders is approximately 1 μm...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720393
EISBN: 978-1-62708-305-8
... densities that resulted in various tensile properties and velocities are given in Table 3 . With similar data for a specific part, ultrasonic velocity can be easily measured, thereby determining the state of sintering and mechanical properties. Fig. 12 Relationship of ultrasonic velocity and...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000109
EISBN: 978-1-62708-312-6
.... Ferritic and austenitic stainless steels do not benefit from strengthening by a second phase or by the austenite- (γ) to-martensite transformation, which is the most popular strengthening mechanism for carbon and low-alloy steels. Solid-solution strengthening is the primary mode of strengthening in these...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550569
EISBN: 978-1-62708-307-2
.../00196-0 • Naslain R. , Design, Preparation and Properties of Non-Oxide CMCs for Application in Engines and Nuclear Reactors: An Overview , Compos. Sci. Technol. , Vol 64 , 2004 , p 155 – 170 10.1016/S0266-3538(03)00230-6 • State of the Art in Ceramic Fiber Performance , Ceramic...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000147
EISBN: 978-1-62708-312-6
... oxidation of sintered stainless steels assumed a more prominent role. Although complications arise from the presence of pores in sintered metals, attempts to improve their oxidation resistance are based on the principles of oxidation established for solid metals. Many high-temperature alloys rely on...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000185
EISBN: 978-1-62708-312-6
... , Princeton, NJ , 2002 , p 207 – 212 29. Banhart J. , Manufacture, Characterization and Application of Cellular Metals and Metal Foams , Prog. Mater. Sci. , Vol 46 , 2000 , p 559 – 632 10.1016/S0079-6425(00)00002-5 30. Stephani G. and Andersen O. , Solid State and...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.9781627083126
EISBN: 978-1-62708-312-6
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550511
EISBN: 978-1-62708-307-2
... Heating elements, insulators, magnets, sensors, integrated circuit packages, substrates, solid electrolytes, piezoelectrics, dielectrics, superconductors Optical Low absorption coefficient Lamps, windows, fiber optics, infrared optics Nuclear Irradiation resistance, high absorption coefficient...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000131
EISBN: 978-1-62708-312-6
.... Typically, a water-atomized austenitic powder would contain a small amount of delta ferrite as a result of rapid cooling from the molten state. Thus, a small fraction of the as-atomized powder would be magnetic. However, during sintering of the compacted powder, delta-ferrite phase will transform into the...