Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290137
EISBN: 978-1-62708-306-5
... Abstract Solid-state welding processes are those that produce coalescence of the faying surfaces at temperatures below the melting point of the base metals being joined without the addition of brazing or solder filler metal. This chapter discusses solid-state welding processes such as diffusion...
Image
Published: 01 October 2011
Fig. 6.34 Relative regimes of time, temperature, and deformation for solid state welding processes. Source: Ref 6.10 More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280149
EISBN: 978-1-62708-267-9
... welding techniques, defect prevention, fixturing, heat treatments, and general practices, including the use of filler metals. It also discusses several solid-state welding methods, superplastic forming, and transient liquid phase bonding, a type of diffusion welding process. The chapter includes extensive...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560309
EISBN: 978-1-62708-291-4
... Abstract This chapter examines the effects of welding on the structure of metal, particularly the changes induced in the isothermal regions adjacent to the weld. It presents more than 150 images identifying structures and features associated with fusion and solid-state welding processes...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820169
EISBN: 978-1-62708-339-3
... Abstract Many factors must be considered when welding dissimilar metals, and adequate procedures for the various metals and sizes of interest for a specific application must be developed and qualified. Most combinations of dissimilar metals can be joined by solid-state welding (diffusion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120065
EISBN: 978-1-62708-269-3
..., and the need for contaminant-free surfaces and atmospheres. It describes common forms of fusion, arc, and solid-state welding along with the use of filler metals, shielding gases, and stress-relief treatments. It also discusses the practice of titanium brazing and the role of filler metals. arc welding...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290001
EISBN: 978-1-62708-306-5
... examining the various joining processes, namely fusion welding, solid-state welding, brazing, soldering, mechanical fastening, and adhesive bonding. In addition, it provides information on several design considerations related to the joining process and selection of the appropriate process for joining...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060117
EISBN: 978-1-62708-261-7
... process used to produce long, straight, semifinished metal products such as a bar, solid and hollow sections, tubes, wires, and strips. The favorable compressive state of stress during extrusion allows a high capacity for deformation, and so it is possible to extrude metals that can be only slightly...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290099
EISBN: 978-1-62708-306-5
... Abstract During fusion welding, the thermal cycles produced by the moving heat source causes physical state changes, metallurgical phase transformations, and transient thermal stresses and metal movement. This chapter begins by discussing weld metal solidification behavior and the solid-state...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290279
EISBN: 978-1-62708-306-5
... by mechanical fastening, adhesive bonding, and, for thermoplastic composites, welding; the making of glass-to-metal seals; and joining of oxide and nonoxide ceramics to themselves and to metals by solid-state processes and by brazing. The classification, types, applications, and the mechanism of each...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2004
DOI: 10.31399/asm.tb.ps.t62440001
EISBN: 978-1-62708-352-2
... Abstract Soldering and brazing represent one of several types of methods for joining solid materials. These methods may be classified as mechanical fastening, adhesive bonding, soldering and brazing, welding, and solid-state joining. This chapter summarizes the principal characteristics...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820013
EISBN: 978-1-62708-339-3
... and heat-affected zone (HAZ), solid-state phase transformations during welding, control of toughness in the HAZ, the effects of preheating and postweld heat treatment, and weld discontinuities. This chapter provides information on the classification of steels and the welding characteristics of each class...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230401
EISBN: 978-1-62708-298-3
... Abstract Beryllium has been successfully joined by fusion welding, brazing, solid-state bonding, and soldering. This chapter describes these processes in detail along with their advantages and disadvantages. It also addresses application considerations such as surface preparation, joint design...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560427
EISBN: 978-1-62708-291-4
... by improved surface, greater uniformity in thickness, and improved mechanical properties compared with hot-rolled sheet. cold welding. A solid-state welding process in which pressure is used at room temperature to produce coalescence of metals with substantial deformation at the weld. Compare with hot...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.9781627082914
EISBN: 978-1-62708-291-4
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300179
EISBN: 978-1-62708-323-2
...-on-flat test (ASTM G133) Another possible contributing factor to the favorable adhesive wear characteristics of cast iron may be its poor weldability. Adhesive wear involves cold (solid-state) welding of contacting surfaces. Cast irons, because of their high carbon content (and the graphite...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930311
EISBN: 978-1-62708-359-1
..., and the metal becomes highly susceptible to embrittlement by oxygen, nitrogen, and hydrogen, which dissolve interstitially in titanium. Therefore, the melting, solidification, and solid-state cooling associated with fusion welding must be conducted in completely inert or vacuum environments. The fusion...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930003
EISBN: 978-1-62708-359-1
...-in.-thick steel plate in 50 passes with the SMAW process will produce a much finer grain size in both the weld and HAZ than a similar weld deposited in 1 pass with the ESW process, which is an extremely high heat input welding process. Influence of Solidification Structure on Solid-State Transformations...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2022
DOI: 10.31399/asm.tb.dsktmse.t56050001
EISBN: 978-1-62708-432-1
... as (a) liquid state welding (e.g., fusion welding processes such as arc welding, laser welding, and electron beam welding) and (b) solid-state welding (e.g., forge welding, explosive welding, friction-stir welding, and solid-state diffusion bonding). Diffusion bonding is one of the solid-state-diffusion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480265
EISBN: 978-1-62708-318-8
... and toughness in weld-fusion and high-temperature heat-affected zones. Applications of these latter alloys are limited to solid-state welding processes, which produce no adverse microstructures. Special fillers are sometimes used to alter the alloy content of weld-fusion zones, for example, commercially...