1-20 of 43 Search Results for

sleeve-bearing stock

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320217
EISBN: 978-1-62708-332-4
... the ore in between two jaws. Both the fixed and the movable jaws are lined with wear-resisting jaw plates. The movable jaw is driven back and forth because of the noncentric rotation of the cylindrical bearing. The crushed ore flows down the chute. Figure 12.32 illustrates the moving jaw of an ore...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290207
EISBN: 978-1-62708-306-5
... are: d , fastener diameter t , thickness of the joint elements w , width of the plate e , edge distance P , load dt , bearing area loaded in compression 2et , total shear-out area loaded in shear ( w – d )/ t , net section loaded in tension wt , gross section loaded...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.9781627082808
EISBN: 978-1-62708-280-8
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320063
EISBN: 978-1-62708-332-4
... of chaplets and chills in cast iron castings; guidelines for drafts, machine stock, tolerances, and contraction or shrink rule; and guidelines for pattern layouts and nesting are also covered. cast iron chaplets chills core making drafts machine stock manufacturability molding nesting...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740103
EISBN: 978-1-62708-308-9
... in stock that has been excessively reduced in one operation. Inclusions, segregation, and porosity result from forging stock that contains these types of discontinuities. Titanium alloys: Discontinuities that are most likely to occur in titanium alloy forgings are usually carried over in the bar...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.htgpge.t67320133
EISBN: 978-1-62708-347-8
.... 6.13 View of dislocated tooth Tooth debris was noticed in various gear meshes. No abnormal distress was found on planet sleeve bearings, although the thrust faces of output shaft sleeve bearings were completely wiped out. Also, sealing surfaces of the output shaft and labyrinth seal were found...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980009
EISBN: 978-1-62708-342-3
... for the manufacture of soft solder, which is described in section 5.3 . Lead alloys, similar to tin alloys, are also suitable for the production of custom shaped anodes as shown in Fig. 2.2 for electrochemical plating. An example is the approximately 20 μm thick and soft running surface in plain bearings...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410151
EISBN: 978-1-62708-280-8
... should be taken to avoid poor die steel condition. Sharp or thin die or mold steel that gets overheated should be avoided because it can retard the life of the mold coating and the mold. Figure 7.1(b) and (c) illustrate examples of preventing poor steel condition by modifying the finish stock...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2022
DOI: 10.31399/asm.tb.tstap.t56040010
EISBN: 978-1-62708-428-4
... for the reclamation of worn or out-of-tolerance parts, frequently with nickel-base alloys. Bronze alloys may be sprayed for some bearings and seal areas. Blends of tungsten carbide and nickel-base alloys are applied for wear resistance. Zinc is commonly coated on bridges and other structures for corrosion resistance...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320103
EISBN: 978-1-62708-332-4
... area should be well supported for accurate load bearing. Brinell hardness is designated as a Brinell Hardness Number (BHN) using a compression test. The test consists of measuring the depth of an indentation produced by a hardened 10 mm (0.4 in.) diameter steel ball under a load of 3000 kg...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250227
EISBN: 978-1-62708-345-4
..., and Fig. 9 shows the severed tooth. Fig. 8 Overall view of one damaged planet gear Fig. 9 View of dislocated tooth Tooth debris was noticed in various gear meshes. No abnormal distress was found on planet sleeve bearings, although the thrust faces of output shaft sleeve bearings...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870001
EISBN: 978-1-62708-299-0
... conversion of used beverage cans (UBC) by primary producers engaged in the production of rigid container stock. Fig. 3 Flow diagram for aluminum in the United States, showing the role of recycling in the industry. Scrap recycling (lower left) includes scrap collectors, processors, dealers and brokers...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.9781627083232
EISBN: 978-1-62708-323-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720321
EISBN: 978-1-62708-305-8
... attached to the ingot, and finally becomes embedded in the surface of the rolled bar ( Fig. 2d ). Thus, scabs bear some similarity to laminations. Pits and Blisters During subsequent rolling, gaseous pockets in the ingot often become pits or blisters on the surface or slightly below the surface...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
... paint adhesion. A detergent-bearing iron phosphating solution is often ideal for this sort of combined cleaning and etching approach. Molten Salt Bath Cleaning Molten salt bath cleaning is very effective for removing many soils, especially paints and heavy scale. However, the very high operating...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980417
EISBN: 978-1-62708-342-3
... with the same speed as far as possible over the full cross section. Figure 7.17 shows that with all types of die, the shape-forming aperture has a die bearing surface in the direction of the material flow. Adjusting the bearing length to the cross section of the extruded profile and the location...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200144
EISBN: 978-1-62708-354-6
... joining sections which are characteristic of the manufacturing method. The L section and the box section of Figure 10-1 are found in numerous engineering structures. These sections can be cast or fabrication welded. The design and the quality of the weld or the casting could have considerable bearing...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.tb.atia.t59340265
EISBN: 978-1-62708-427-7
... problem was to line the cylinder bores, in which the pistons move, with cast-iron sleeves. This protected the engine block itself from excessive wear from the pistons. The use of cylinder liners added steps and cost to the engine manufacturing process, however. Improvements in the engine material...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390173
EISBN: 978-1-62708-459-8
..., such changes are relatively slow. The work rolls of a four-high or multiroll mill may be mechanically deflected to control the shape of the roll gap very rapidly. This is commonly done by applying an external force at the work roll mounting bearings. In addition to ground and thermal cambers and roll...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.t59370145
EISBN: 978-1-62708-447-5
... on the furnace design. Metal quality is also dependent on the types of products and the processes used. This has a bearing on the types of holders, metal treatment, and dozers. The yield, which is a ratio of the weight of the casting divided by the amount of metal poured, is determined by the processes...