1-20 of 299 Search Results for

sand molds

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 December 2018
Fig. 3.1 Range of aluminum casting processes using sand and metal molds More
Image
Published: 01 December 1995
Fig. 13-2 Sand slinger for filling large floor molds. Operator controls the slinger from his control post on the sand slinger. More
Image
Published: 30 November 2023
Fig. 1.2 Basic elements of a green sand-molding foundry More
Image
Published: 30 November 2023
Fig. 4.6 Classification of green sand molding machines More
Image
Published: 30 June 2023
Examples of (a) aluminum cast components by sand-mold casting. Courtesy of Leitelt Brothers Inc. and (b) a precision high-vacuum die casting of integral motorcycle frame. Courtesy of Suzuki More
Image
Published: 01 December 2018
Fig. 3.7 Schematic of a prototype sand mold of a rear knuckle More
Image
Published: 01 October 2011
Fig. 5.23 Major components of a sand mold. (a) Pattern assembly for cope and drag sections. (b) Cross section of mold with core More
Image
Published: 01 December 2016
Fig. 1.44 (a) Microstructure of AlSi10Mg alloy, sand mold, lamellar eutectic. (b) Microstructure of AlSi11 alloy, metal mold, rod eutectic. LM, etched 1HF(1) More
Image
Published: 01 December 2016
Fig. 3.2 Microstructure of alloy AlSi7Mg, sand mold. (a, b) Wall thickness 3 cm. (c, d) Wall thickness 1 cm. Light microscopy (LM), etch. 1HF(1). Source: Ref 3 More
Image
Published: 01 December 2016
Fig. 3.3 Microstructure of alloy AlSi7Mg, sand mold, wall thickness 3 cm. (a–e) Silicon in the interdendritic eutectic. (f) Enlarged microregion visible in (e), showing silicon lamellae in the interdendritic eutectic. Scanning electron microscopy (SEM), deep etch More
Image
Published: 01 December 2016
Fig. 3.12 Microstructure of alloy AlSi10Mg, sand mold. (a, b) Wall thickness 3 cm. (c, d) Wall thickness 1 cm. LM, etch. 1HF(1). Source: Ref 3 More
Image
Published: 01 December 2016
Fig. 3.18 Microstructure of alloy AlSi11, sand mold, wall thickness 3 cm. (a–e) Silicon in the interdendritic eutectic, eutectic silicon lamellae. (f) Hypereutectic silicon precipitate, eutectic silicon lamellae. SEM, deep etch More
Image
Published: 01 December 2004
Fig. 3.1 Typical sand mold gating. Source: Ref 1 More
Image
Published: 01 January 2022
Fig. 3.6 Layout of a chemically bonded sand molding line. Source: Ref 2 More
Image
Published: 01 December 1995
Fig. 1-2 Typical steps involved in making a casting from a green sand mold More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200173
EISBN: 978-1-62708-354-6
... Abstract This chapter discusses the following conventional molding processes for static casting: green sand molding, dry sand molding, vacuum molding, and expendable pattern casting. It also discusses core and mold processes for steel castings. The chapter provides an overview of sand molds...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410021
EISBN: 978-1-62708-280-8
... Abstract This chapter provides information on comparative attributes of sand molds and metal molds for aluminum casting. The cooling rates and microstructures obtained with each mold type are discussed. In addition, the chapter explains why sand castings work successfully in certain...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320011
EISBN: 978-1-62708-332-4
... Abstract Most iron and steel castings are produced by casting into sand molds. Sand cores are needed primarily to form hollow cavities in castings for collapsibility and ease of cleaning. This chapter begins with an overview of the classification of molding and core-making systems...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2016
DOI: 10.31399/asm.tb.ascaam.t59190089
EISBN: 978-1-62708-296-9
... Abstract This chapter is an atlas of microstructures observed in AlSi7Mg, AlSi11, and Al21CuNiMg modified with either eutectic (strontium, sodium) or hypereutectic (phosphorus) silicon crystals. The microstructure images reveal the as-cast state of gravity castings made in sand and metal molds...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740047
EISBN: 978-1-62708-308-9
..., crucible, and vacuum melting, and common casting techniques such as sand casting, plaster and shell casting, evaporative pattern casting, investment casting, permanent mold casting, cold and hot chamber die casting, squeeze casting, semisolid metal processing, and centrifugal casting. casting...