Skip Nav Destination
Close Modal
Search Results for
sand hoppers
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 29 Search Results for
sand hoppers
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Image
Published: 30 November 2023
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.t59370021
EISBN: 978-1-62708-447-5
... units; magnetic separators; lump breakers and core crushers; screens; sand coolers; sand reclamation systems; and sand hoppers. core sand mixers sand aerators sand coolers sand mullers sand reclaimers shakeout units MOLD QUALITY is an extremely important factor with regards to casting...
Abstract
This chapter focuses on the elements and functions of sand conditioning equipment which are critical to achieving good quality castings. The sand conditioning equipment include sand muller; core sand mixers; sand conveyors and bucket elevators; sand aerators; mold conveyors; shakeout units; magnetic separators; lump breakers and core crushers; screens; sand coolers; sand reclamation systems; and sand hoppers.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.t59370013
EISBN: 978-1-62708-447-5
... raw materials sand dryers sand hoppers SAND AND METALLIC charge materials are two essential and heavy raw materials that are needed for molding and casting. Planning for efficient receipt, storage, and handling of these materials is a key element of manufacturing engineering. For every ton...
Abstract
Sand and metallic charge materials are two essential and heavy raw materials that are needed for molding and casting. This chapter focuses on planning and provision for storage and handling of the raw materials needed for casting manufacturing. The major raw materials used for molding and casting are metallic charge materials and nonmetallic materials. The chapter also presents the advantages, limitations, and applications of drum or rotary dryers (also known as rotary kiln dryers) and fluidized bed dryers (also known as vibration fluidized bed dryers).
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.t59370059
EISBN: 978-1-62708-447-5
... of an arm or a combination of arms that produce a crank action movement to move the compacted mold to the pattern draw and stripping station. The flask is clamped onto the machine platen using pneumatic clamps. The jolt table compacts the sand which descends from the overhead hopper. The top of the mold...
Abstract
Molding flasks and other supplementary equipment are essential for molding complex shapes at competitive production rates and costs. This chapter addresses the design aspects of molding flasks and accessories, the features and handling accessories of molding machines, core making machines and innovations for productivity and quality, and automated core-setting aids.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320011
EISBN: 978-1-62708-332-4
..., vertically filled flaskless molding. The left-hand side of the pattern plate is attached to a hydraulic cylinder. The right-hand side of the pattern plate is hinged so that it can be swung out, making room for the mold to move forward. Prepared green sand that flows from the overhead hopper is pressurized...
Abstract
Most iron and steel castings are produced by casting into sand molds. Sand cores are needed primarily to form hollow cavities in castings for collapsibility and ease of cleaning. This chapter begins with an overview of the classification of molding and core-making systems. This is followed by a section discussing the process involved in shell molding, along with its applications. A brief description of the special casting processes is then presented. Next, the chapter discusses the processes involved in core making. Further, it provides an overview of casting manufacturing. Finally, the chapter provides information on the factors that influence a casting facility layout.
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.t59370001
EISBN: 978-1-62708-447-5
... of the molds passes through a cooler and returns to the sand hopper and the muller for blending with clay and water. The mulled sand is then ready for reuse in molding. The molding flasks used to contain the mold sand move from the knockout station back to the molding station. Gates, feeders, and any flash...
Abstract
Planning and laying out casting facilities involve a number of vital factors, such as available infrastructure, selection of suitable sites, orientation of operations and process flow, markets and products, operating parameters, and targeted hourly output and annual capacity. This chapter presents guiding principles and layout concepts with these factors in mind. It also presents steps for the creation of a plant layout. Plant layout involves the arrangement of processing areas, machinery, and equipment for the efficient conversion of raw materials into finished products. The chapter discusses general guidelines for developing a layout.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410029
EISBN: 978-1-62708-280-8
... . The bottom mold, or the drag half, is similarly prepared. The core is set in the drag. Frame 8 . The mold is closed and poured. The mold moves to the shakeout, with the vacuum still held for both the flasks. Frame 9 . When the vacuum is released, the sand falls into the hopper below...
Abstract
This chapter discusses the advantages, limitations, and applications of various aluminum casting processes, namely green sand casting process, air set or no-bake molding process, vacuum molding process, evaporative foam casting process, and die casting process. The processes covered also include gravity permanent molding, low-pressure permanent molding, counter pressure, squeeze casting, investment casting, rapid prototype casting, cast forge hybrid, and semisolid metal processes.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.9781627082808
EISBN: 978-1-62708-280-8
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320003
EISBN: 978-1-62708-332-4
... economical alternative compared with pelletizing, which is a pellet-forming process. The sintered charge is fed into the top of the blast furnace either by a double bell system or a valve-controlled hopper system. The systems are designed for proper charge distribution while preventing the escape of flue...
Abstract
This chapter provides a brief overview of iron and steel manufacturing and the major equipment involved in the process as well as identifying where casting fits into the overall process. In addition, it provides an overview of cast iron manufacturing, including the processes involved in converting pig iron into cast iron and steel.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200144
EISBN: 978-1-62708-354-6
... no change in shape was required to convert the part to cast steel. Reduced breakage, less down time, and longer service life resulted from the conversion. The function of this cutter head is to remove sand from a pipe flask, cutting sand from between the flask and the cast iron pipe. The cutter head...
Abstract
Parts of machines and equipment that have previously been designed as wrought or fabricated parts, or as cast parts of metals other than steel, are often reconsidered as steel castings. This chapter presents bending test data for several junction designs of L and box sections and discusses redesign from fabrication, forgings, and cast iron. The chapter also includes the benefits of redesign.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300121
EISBN: 978-1-62708-323-2
... Fretting – 1 million cycles Galling – one 360° pass Sand abrasion – 3,000 9-inch diameter rubber wheel revolutions Solid particle erosion – (ASTM G76) 10 minutes (20 g) Scratch tests – one pass In general, tests should be long enough to establish a steady-state condition of wear...
Abstract
This chapter discusses the processes and procedures involved in tribotesting, the significance of test parameters and conditions, and practical considerations including test metrics and measurements and the interpretation of wear damage. It also describes the different types of erosion tests in use and common approaches for adhesive wear and abrasion testing.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.sch6.9781627083546
EISBN: 978-1-62708-354-6
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.t59370115
EISBN: 978-1-62708-447-5
... about 100 scfm, flows through the plasma torch. Oxidation loss of silicon, chrome, and manganese are minimized due to the reducing conditions in the lower sections of the cupola. Silicon loss is reduced by 30%. Silica sand which has been added is reduced to silicon at these temperatures...
Abstract
The melting furnace is a critically important piece of equipment in a foundry; it influences the balance between the metal required by molding machines and the melting capacity. This chapter presents the features, types, advantages, and applications of furnaces suitable for iron and steels such as cupolas, induction furnaces, and arc furnaces.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.t59370167
EISBN: 978-1-62708-447-5
... applications, avoiding the need for machining Thin walls (as little as 2 mm or 0.08 in.), which allow for lightweight applications High surface integrity Higher mechanical properties compared to sand castings Leakproof casting capability to handle fluids (engine blocks, crankcases, front engine...
Abstract
This chapter provides an overview of aluminum die casting and the equipment used. It discusses the advantages and limitations of the die casting process and the design and operation of hot- and cold-chamber die casting machines. It also discusses clamping systems and forces and the factors affecting die life, including die materials, metal injection cycles, and lubrication. A typical die casting cell layout is also provided.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350043
EISBN: 978-1-62708-315-7
... High-stress gouging or grinding: Wet, as in ball and rod mills Dry, as in jaw-type or roll-type ore crushers Low-stress scratching or sliding: Wet, such as conveyor screws for wet sand Dry, as against plows or earthmoving devices operating in dry soil Impact of loose abrasive (erosion): Wet...
Abstract
This chapter discusses the basic principles of friction and the factors that must be considered when determining its effect on moving bodies in contact. It provides an extensive amount of friction data, including static and kinetic friction coefficients for numerous combinations of engineering materials and coatings. It also describes the causes and effects of the most common forms of wear, the conditions under which they occur, the role of lubrication, and wear testing methods.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290009
EISBN: 978-1-62708-319-5
... depends on both technical aspects and cost advantages. 2.1 Introduction A powder consists of many particles; each particle is similar to grains of sand in terms of packing and flow. The scanning electron microscope (SEM) is an excellent tool for observing the characteristics of a powder. Figure...
Abstract
This chapter introduces the key powder fabrication attributes to assist in the identification of the right powders for an application. First, it describes the characteristics of engineering powders such as particle size distribution, powder shape and packing density, surface area, powder flow and rheology, and chemical analysis. The chapter then describes the general categories of powder fabrication methods, namely mechanical comminution, electrochemical precipitation, thermochemical reaction, and phase change and atomization. It provides information on the two largest contributors to powder price, namely raw material cost and conversion cost. The applicability of various processes to specific material systems is mentioned throughout this chapter.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870001
EISBN: 978-1-62708-299-0
... such as polishing, sand blasting, or wire brushing meet the majority of needs. In many instances, the surface finish supplied is entirely adequate without further finishing. Where the plain aluminum surface does not suffice or where additional protection is required, any of a wide variety of surface finishes may...
Abstract
Aluminum is the second most widely used metal in the world. It is readily available, offers a wide range of properties, and can be shaped, coated, and joined using a variety of methods. This chapter discusses some of the key attributes of wrought and cast aluminum alloys and the classifications, designations, and grades of available product forms. It also explains how aluminum alloys are used in aerospace, automotive, rail, and marine applications as well as in building and construction, electrical products, manufacturing equipment, packaging, and consumer durables such as appliances and furniture.
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.9781627083232
EISBN: 978-1-62708-323-2
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200007
EISBN: 978-1-62708-354-6
... of a large number of structural and operation parts. For example, a steel casting used with many design variations is the hopper frame, Figure 2-8 . From four to eight of these frames are used on each hopper car. Fig. 2-8 Railroad hopper car door frame with integral hinges and cover. Size about 3...
Abstract
Steel castings are produced in thousands of designs for different applications. They fill needs in many industries, including transportation, construction machinery, earthmoving equipment, rolling mills, mining, oil and gas exploration, and power generation. This chapter touches upon the variety of applications for which steel castings can be supplied and the ranges of casting size and complexity. Photographs in this chapter provide an understanding of these applications, their size and complexity, and the types of cast steels produced.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550325
EISBN: 978-1-62708-307-2
.... Sheet stainless steel Stamped Welded fabrication As above, except SMCs offer a vast cost saving. Sheet aluminum Stamped Riveted skin and stronger construction Integrated SMC offers equal performance at equal weight with substantial cost saving. Cast aluminum Sand permanent or die cast...
Abstract
This chapter describes the molecular structures and chemical reactions associated with the production of thermoset and thermoplastic components. It compares and contrasts the mechanical properties of engineering plastics with those of metals, and explains how fillers and reinforcements affect impact and tensile strength, shrinkage, thermal expansion, and thermal conductivity. It examines the relationship between tensile modulus and temperature, provides thermal property data for selected plastics, and discusses the effect of chemical exposure, operating temperature, and residual stress. The chapter also includes a section on the uses of thermoplastic and thermosetting resins and provides information on fabrication processes and fastening and joining methods.