1-20 of 175 Search Results for

ring compression test

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040083
EISBN: 978-1-62708-300-3
... the cylinder upset and ring compression tests, provided experimental measurements are accurate enough, Fig. 8.1(b) . Therefore, an inverse problem is regarded as a parameter identification problem that can be formulated further as an optimization problem where the difference between measurement and FEM...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040067
EISBN: 978-1-62708-300-3
..., ” Ann. CIRP , Vol 49 , 2000 , p 1 – 24 . 10.1016/S0007-8506(07)63456-8 [Male et al., 1970] Male A.T. , DePierre V. , “ The Validity of Mathematical Solutions for Determining Friction from the Ring Compression Test, ” Trans. ASME, J. Lubr. Technol. , Vol 92 , 1970 , p 389...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860095
EISBN: 978-1-62708-338-6
...)00073-0 8.37 Kugler D. and Moon T.J. , A Technique for Compression Testing of Composite Rings , Compos. Part A: Appl. Sci. Manuf. , Vol 33 , 2002 , p 507 – 514 10.1016/S1359-835X(01)00144-0 8.38 “ Plastics Piping Systems—Glass-Reinforced Thermosetting Plastics (GRP) Pipes...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720117
EISBN: 978-1-62708-305-8
... from the tensile test include strength properties (yield strength and ultimate tensile strength) and, a measure of ductility, either percent elongation or reduction in area. Conventional test machines for measuring mechanical properties include tensile testers, compression testers...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780164
EISBN: 978-1-62708-281-5
... Abstract This article discusses electrical testing and recommended procedures for determining the electrical properties of insulating materials, with particular emphasis on plastics. It describes the electrical characteristics of various forms of plastics and also presents definitions...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040025
EISBN: 978-1-62708-300-3
... Abstract This chapter explains how to determine flow stress and forgeability using data from tensile tests, compression tests, ring tests, and torsion tests. It describes sample preparation, tooling and equipment, test procedures, error sources, and data plotting techniques. It also provides...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040059
EISBN: 978-1-62708-300-3
.... The effects of forging pressure, deformation rate, and lubrication on the heat transfer coefficient and the friction shear factor were evaluated simultaneously. A schematic of ring compression tests used for the measurement of interface heat transfer coefficient is shown in Fig. 6.8 . Two pairs...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870219
EISBN: 978-1-62708-299-0
... Abstract This chapter describes the use of standardized tests to determine the susceptibility of aluminum alloys to specific forms of corrosion, including pitting, intergranular corrosion, filiform corrosion, exfoliation corrosion, and stress-corrosion cracking. aluminum alloys corrosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860115
EISBN: 978-1-62708-338-6
... standard for short-beam shear and tensile ring testing. Dick Young was one of the early leaders who filed key patents in this fledgling technology and then started his own company. His development work included filament-wound pipe nozzles and prototype RMCs. He licensed this technology to several other...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720085
EISBN: 978-1-62708-305-8
... that directly or indirectly indicate the contact pressure involved in deforming the test surface. Because the indenter is pressed into the material during testing, hardness is also viewed as the ability of a material to resist compressive loads. The indenter may be spherical as in the Brinell test, pyramidal...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780185
EISBN: 978-1-62708-281-5
... D4703 293 Compression molding thermoplastic materials into test specimens, plaques, or sheets D 524 95 Compression molding test specimens of thermosetting molding compounds D 6289 2577 Measuring shrinkage from mold dimensions of molded thermosetting plastics Mechanical properties D...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060149
EISBN: 978-1-62708-261-7
... Conventional testing machines for measuring mechanical properties include tension testers, compression testers, or the more versatile universal testing machine (UTM). Universal testing machines have the capability to test material in tension, compression, or bending. The word universal refers to the variety...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910427
EISBN: 978-1-62708-250-1
... Abstract Corrosion testing and monitoring are powerful tools in the fight to control corrosion. This chapter provides a general overview of three major categories of corrosion tests, namely laboratory tests, pilot-plant tests, and field tests. It begins with brief sections describing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040237
EISBN: 978-1-62708-300-3
... Determination of Flow Stress and Friction,” of this book. The friction and heat-transfer coefficient are not readily available in literature. The most common way to determine the shear friction factor in forging is to perform ring compression tests. Friction factors measured with the ring compression test...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040007
EISBN: 978-1-62708-300-3
... ) . There are various methods of evaluating friction, i.e., estimating the value of μ or m. In forging, the most commonly used tests are the ring compression test, spike test, and cold extrusion test. In forging, material is deformed plastically to generate the shape of the desired product. Metal flow is influenced...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.9781627083003
EISBN: 978-1-62708-300-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500289
EISBN: 978-1-62708-317-1
... Abstract This chapter describes joining by forming processes including riveting, clinching, crimping, and dieless joining techniques. It also discusses the fatigue behavior of clinched joints and the results of fatigue tests that compare clinched and spot welded joints. clinching...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040193
EISBN: 978-1-62708-300-3
... the coulomb friction coefficient. The most common way to determine the shear friction factor in forging is to perform ring compression tests. From these tests, it is possible to estimate the heat-transfer coefficient, flow stress and friction as a function of temperature, strain rate, strain, and forming...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090367
EISBN: 978-1-62708-266-2
.... , Modified WOL Specimen for K ISCC Environmental Testing , J. Met. , Vol 4 ( No. 3 ), 1969 , p 701 – 728 17.35 Kaufman J.G. , Coursen J.W. , and Sprowls D.O. , An Automated Method for Evaluating Resistance to Stress-Corrosion Cracking with Ring-Loaded Precracked Specimens...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630117
EISBN: 978-1-62708-270-9
... of the problems of laboratory fatigue testing and of the fatigue process itself. Finally, information on types and statistical aspects of fatigue is provided along with examples. fatigue fracture laboratory fatigue testing macroscopic characteristics microscopic characteristics strength stress...