1-20 of 952 Search Results for

resistance heating

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200298
EISBN: 978-1-62708-354-6
...Abstract Abstract This chapter provides a detailed discussion on the definitions, alloy classification, alloy selection, mechanical properties, hot gas corrosion resistance, and formability of heat-resistant high alloy steels. In addition, the applications of cast heat-resistant alloys are also...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.pnfn.t65900111
EISBN: 978-1-62708-350-8
...-like behavior of gas fluidized beds. Source: Ref 1 Heating Method The methods of heating a fluidized bed are very similar to those used to heat an atmosphere-type furnace or a salt bath. The heating system can be electrical or gas, and internal or external. External Resistance Heating...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480243
EISBN: 978-1-62708-318-8
... heat-resistant tool materials Tools must be adapted for heating Requires use of slow press with some dwell time (5 min or more) Limited to forming operations on equipment that can use heated tools Requires additional equipment (hot sizing presses) Long dwell times in hot sizing press...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290061
EISBN: 978-1-62708-306-5
...Abstract Abstract Resistance welding is a group of processes in which the heat for welding is generated by the resistance to the flow of an electrical current through the parts being joined. This chapter discusses the processes, advantages, and limitations of specific resistance welding...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980417
EISBN: 978-1-62708-342-3
..., poor heat extraction from the shape-forming areas of the extrusion tooling can result in the temperature exceeding the tempering temperature of the tool material used, and plastic deformation occurring after a few extrusions. The control of the material flow with the aid of varying flow resistances...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170003
EISBN: 978-1-62708-297-6
... Room-temperature strength Hardenability Fatigue resistance Creep resistance Processing properties Castability Weldability, brazeability, and solderability Formability Machinability Service properties Heat resistance Toughness and cold resistance Corrosion...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220315
EISBN: 978-1-62708-341-6
... used during these periods. The effects of utilization level on energy costs for several means of heating prior to forging are illustrated in Fig. 12.2 . In this plot, data are given for a typical motor-generator induction system as well as for a direct-resistance heating method. Not shown is the trend...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.tt2.t51060209
EISBN: 978-1-62708-355-3
..., as discussed in more detail in the section “Frame-Furnace Tensile-Testing Equipment” in this chapter. The heating method used for hot tensile testing varies with the application. The most common heating techniques are direct-resistance heating (in the case of Gleeble systems) and indirect-resistance...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500133
EISBN: 978-1-62708-317-1
..., the sheet metal loses heat and also oxidizes. This may be avoided in the conductive heating method by directly heating the sheets, set into the dies by means of electrical resistance. In the conduction heating method, the component is connected to a series of power sources. Due to the electric...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410091
EISBN: 978-1-62708-280-8
... Resistance to wear and low coefficient of expansion Alloy choice Heat treat Choc. Suspension parts, wheels, knuckles, control arms, brackets X X X X … … … … … … A 356 T6 T61 Brake calipers, highly stressed aircraft and missile parts, high velocity blowers, and impellers X X X...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440175
EISBN: 978-1-62708-262-4
..., and corrosion resistance of stainless steels and the effect of specific elements on the characteristics of iron-base alloys. Five groups of stainless steels are discussed: austenitic, ferritic, martensitic, precipitation-hardening, and duplex grades. The chapter also describes the heat treatment conditions...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200369
EISBN: 978-1-62708-354-6
...Abstract Abstract This chapter covers the basics of weldability of cast steels such as carbon and low alloy steels, corrosion-resistant high alloy steels, nickel-base alloys, heat-resistant high alloy steels, and wear-resistant high austenitic manganese steels. It provides an overview of weld...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240547
EISBN: 978-1-62708-251-8
...Abstract Abstract Nickel and nickel alloys have an excellent combination of corrosion, oxidation, and heat resistance, combined with good mechanical properties. Nickel alloys can be divided into alloys that combine corrosion and heat resistance, superalloys for high-temperature applications...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240395
EISBN: 978-1-62708-251-8
... the inner core during heat treatment. The end result is a hard, wear-resistant surface with a tough inner core. This process, called carburizing, is one of several case-hardening processes. Another case-hardening process is nitriding. Since nitriding is done at a lower temperature, the part is quenched...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080005
EISBN: 978-1-62708-304-1
... year 2005 (79) … 310 3000 h … 34 (1.34) (a) Specimens were cycled to room temperature after every 20 h of exposure. Source: Ref 36 Cycles to failure of a thin foil (0.050 mm, or 0.002 in., thick) of ALFA IV repeatedly resistance heated to the indicated temperatures for 2 min...
Book Chapter

By J. W. Ekin
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860465
EISBN: 978-1-62708-348-5
... critical field, H c2 , and critical current density, J c , described in § 13.4 and § 13.5 . 13.2.3 Measurement of Critical Temperature There are three basic methods of determining the critical temperature: measuring the change in the resistance, magnetic permeability, or heat capacity...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630237
EISBN: 978-1-62708-270-9
... • Davis J.R. , Ed., ASM Specialty Handbook: Heat-Resistant Materials , ASM International , 1997 • Donachie M.J. , Ed., Superalloys: Source Book , American Society for Metals , 1983 • Fatigue and Fracture , Vol 19 , ASM Handbook , ASM International , 1996 • Khare...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1999
DOI: 10.31399/asm.tb.cmp.t66770077
EISBN: 978-1-62708-337-9
.... and Fournelle R.A. , High Cycle Fatigue Resistance of AISIE 9310 Carburised Steel with Two Different Levels of Retained Austenite and Surface Residual Stress , J. Heat Treat. , Vol 2 ( No. 1 ), 1981 , p 54 – 61 10.1007/BF02833074 28. Razim C. , Effects of Residual Austenite...