Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290165
EISBN: 978-1-62708-306-5
... or brazed together. Intricate assemblies can be produced with low distortion, high fatigue resistance, and good resistance to thermal shock. Joints tend to be strong if well filled, unless embrittling phases are produced by reaction between the filler metal and the components. Soldered and brazed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480265
EISBN: 978-1-62708-318-8
.... It describes several welding processes, including arc welding, resistance welding, and friction stir welding, and addresses related issues such as welding defects, quality control, and stress relieving. The chapter also covers mechanical fastening techniques along with adhesive bonding and brazing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290001
EISBN: 978-1-62708-306-5
... is also simplified by the fact that heat can be applied to the joint by many means, including torches, furnaces, induction coils, electrical resistance, and dipping. Several joints in one assembly often can be produced in one multiple-braze operation during one heating cycle, further enhancing production...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170550
EISBN: 978-1-62708-297-6
... properties as well as corrosion resistance. gold alloys silver alloys platinum alloys Composition Introduction and Overview The noble metals include silver, gold, and the six platinum group metals—platinum, palladium, ruthenium, rhodium, osmium, and iridium—so named because they commonly...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.t51230047
EISBN: 978-1-62708-351-5
... to the service environment, in terms of corrosion and oxidation resistance and compatibility with vacuum, in accordance with functional requirements. Zinc-containing brazes are particularly restrictive in this regard. The filler must be compliant with statutory needs. These include hallmarking regulations...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870161
EISBN: 978-1-62708-299-0
... Abstract This chapter describes the factors that affect the corrosion performance of aluminum assemblies joined by methods such as welding, brazing, soldering, and adhesive bonding. The factors covered include galvanic effects, crevices, and assembly stresses in products susceptible to stress...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230401
EISBN: 978-1-62708-298-3
... to the heating sources. Of industrial importance are furnace, induction, torch, resistance, dip, diffusion, and infrared brazing. (Furnace brazing is performed using a heated furnace. Induction brazing uses the heat from the resistance of the workpieces subjected to a voltage induced through one or more coils...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120065
EISBN: 978-1-62708-269-3
..., and the need for contaminant-free surfaces and atmospheres. It describes common forms of fusion, arc, and solid-state welding along with the use of filler metals, shielding gases, and stress-relief treatments. It also discusses the practice of titanium brazing and the role of filler metals. arc welding...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000167
EISBN: 978-1-62708-312-6
... Abstract This chapter describes secondary processes employed in the production of powder-metal stainless steel parts, including various machining operations, welding, brazing, sinter bonding, resin impregnation, re-pressing and sizing, and surface finishing. It also discusses the factors...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280149
EISBN: 978-1-62708-267-9
... Abstract Superalloys, except those with high aluminum and titanium contents, are welded with little difficulty. They can also be successfully brazed. This chapter describes the welding and brazing processes most often used and the factors that must be considered when making application...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280203
EISBN: 978-1-62708-267-9
... and grit should not be used to descale superalloys unless their use is followed by pickling to remove metal contamination. For parts that must be resistance or solid-state welded or brazed or that have highly tenacious scales produced by furnace atmospheres, pickling after dry abrasive cleaning...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.t51230189
EISBN: 978-1-62708-351-5
... Abstract Brazes for carat gold jewelry must meet or exceed the fineness/caratage of the component piece parts of the assembly in order for it to meet the national fineness/caratage standards and marking or hallmarking regulations for jewelry. This chapter concentrates on brazes for gold jewelry...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.t51230143
EISBN: 978-1-62708-351-5
... Abstract This chapter considers the role of materials in brazing operations and the manner in which they impact on the choice of processing conditions and their optimization. The concepts covered are metallurgical and mechanical constraints, and constraints imposed by the components...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.t51230221
EISBN: 978-1-62708-351-5
... of magnitude slower than for braze/metal combinations. Fig. 7.2 The normalized tensile strength, σ t / E , plotted against coefficient of linear thermal expansion, α. The contours show a measure of the thermal shock resistance, Δ T . Corrections must be applied for constraint and to allow...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720411
EISBN: 978-1-62708-305-8
... of nondestructive inspection of weldments including visual inspection, liquid penetrant inspection, magnetic particle inspection, radiographic inspection, ultrasonic inspection, leak testing, and eddy current and electric current perturbation inspection. The chapter also describes the properties of brazing filler...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290079
EISBN: 978-1-62708-306-5
... Abstract This chapter discusses the fusion welding processes, namely oxyfuel gas welding, oxyacetylene braze welding, stud welding (stud arc welding and capacitor discharge stud welding), high-frequency welding, electron beam welding, laser beam welding, hybrid laser arc welding, and thermit...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.t51230001
EISBN: 978-1-62708-351-5
... with low distortion, high fatigue resistance, and good resistance to thermal shock. Joints tend to be strong if well filled, unless embrittling phases are produced by reaction between the filler metal and the components. Brazed and soldered joints can be endowed with physical and chemical properties...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.t51230207
EISBN: 978-1-62708-351-5
... metal with copper. Provided the copper is sufficiently thin and well diffused after brazing, the mechanical and corrosion resistance of the aluminum parts are not compromised. The joining process temperature can be as low as 540 °C (1000 °F). Using the same idea, the filler metal foil or coating can...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.9781627083515
EISBN: 978-1-62708-351-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200369
EISBN: 978-1-62708-354-6
... are submerged arc, gas metal arc, gas tungsten arc, plasma arc, plasma powder spray, thermal spray, oxy-fuel metallizing, electron beam, resistance brazing, induction brazing, and laser welding. When using an arc welding process or any process which results in a homogeneous structure, a multipass weld procedure...