1-20 of 1781

Search Results for resistance

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000059
EISBN: 978-1-62708-312-6
... Abstract This chapter discusses the sintering process for stainless steel powders and its influence on corrosion resistance. It begins with a review of sintering furnaces and atmospheres and the effect of temperature and density on compact properties such as conductivity, ductility...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290061
EISBN: 978-1-62708-306-5
... Abstract Resistance welding is a group of processes in which the heat for welding is generated by the resistance to the flow of an electrical current through the parts being joined. This chapter discusses the processes, advantages, and limitations of specific resistance welding processes...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350001
EISBN: 978-1-62708-315-7
... them in critical industries such as mining, energy production, transportation, and mineral and chemical processing. The chapter also describes basic approaches to dealing with corrosion and wear in steel. corrosion protection corrosion resistance steel wear resistance SURFACE ENGINEERING...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780211
EISBN: 978-1-62708-281-5
... Abstract This article briefly describes the historical development of fracture resistance testing of polymers and reviews several test methods developed for determining the fracture toughness of polymeric materials. The discussion covers J-integral testing, the methods for determining linear...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030167
EISBN: 978-1-62708-282-2
... Abstract This chapter discusses the factors influencing the corrosion resistance of bulk materials, namely alloying, metallurgical factors, and mechanical treatments. corrosion resistance bulk materials alloying metallurgical factors mechanical treatments THE CORROSION RESISTANCE...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030169
EISBN: 978-1-62708-282-2
... Abstract This chapter addresses the general effects of composition, mechanical treatment, surface treatment, processing, and fabrication operations on the corrosion resistance of aluminum and its alloys. Different types of surface treatments covered include claddings, anodizing, and conversion...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030172
EISBN: 978-1-62708-282-2
... Abstract This chapter discusses the effects of metallurgical factors on the corrosion resistance of magnesium alloys. The factors are chemical composition, heat treating, grain size, and cold-work effects. The chapter describes the causes of corrosion failures in magnesium alloys, namely heavy...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030176
EISBN: 978-1-62708-282-2
... Abstract Stainless steels and nickel-base alloys are recognized for their resistance to general corrosion and other categories of corrosion. This chapter examines the effects of specific alloying elements, metallurgical structure, and mechanical conditioning on the corrosion resistance...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120123
EISBN: 978-1-62708-269-3
... Abstract Titanium and its alloys are used chiefly for their high strength-to-weight ratio, but they also have excellent corrosion resistance, better even than stainless steels. Titanium, as the chapter explains, is protected by a tenacious oxide film that forms rapidly on exposed surfaces...
Image
Published: 01 June 1988
Fig. 2.12 Workpiece resistance factor used for calculating workpiece resistance as reflected in induction-coil circuit for round, hollow loads. From C. A. Tudbury, Basics of Induction Heating , Vol 1, John F. Rider, Inc., New York, 1960 ( Ref 2 ) More
Image
Published: 01 June 1988
Fig. 2.13 Workpiece resistance factor used for calculating workpiece resistance as reflected in induction-coil circuit for rectangular loads. From C. A. Tudbury, Basics of Induction Heating , Vol 1, John F. Rider, Inc., New York, 1960 ( Ref 2 ) More
Image
Published: 01 January 1998
Fig. 13-25 Heat-checking resistance (lower readings indicate higher resistance) as a function of unnotched impact toughness and hardness of H13 steel. Source: Ref 24 More
Image
Published: 01 September 2008
Fig. 31 Heat checking resistance (lower readings indicate higher resistance) as a function of unnotched impact toughness and hardness of H13 steel. Heat checking is evaluated by the photographs on the left; the rating is calculated by adding the column representing the largest cracks (leading More
Image
Published: 01 June 2007
Fig. 6.3 Effect of pitting resistance equivalent on corrosion resistance (5% NaCl by immersion) of standard (▭)and tin- and copper- ( o ) modified austenitic stainless steels (unpublished data) More
Image
Published: 01 June 2007
Fig. 2.7 Relationship between number of corrosion pits formed and pitting resistance equivalence number (PREN) for three powder metallurgy 400-series stainless steels. ABS, antilock brake sensor More
Image
Published: 01 December 2008
Fig. 23 Influence of sulfur level on pitting resistance of unannealed welds for different solidification modes. Source: Ref 23 More
Image
Published: 01 December 2008
Fig. 24 Influence of sulfur level on pitting resistance of welds without homogenizing anneal. FA, ferrite forming first on solidification as opposed to austenite first, AF. Source: Ref 23 More
Image
Published: 01 December 2008
Fig. 25 Variation of critical pitting temperature with pitting resistance equivalent number (PREN) of austenitic steels in water plus 6% FeCl e . Source: Ref 26 More
Image
Published: 01 December 2008
Fig. 31 Influence of molybdenum on resistance to stress corrosion cracking (SCC) in austenitic steels More