Published: 01 December 2003
Fig. 17 High-speed resin transfer molding process More
Image
Published: 01 October 2012
Fig. 8.39 Process flow for resin transfer molding. Source: Ref 8.14 More
Image
Published: 01 October 2012
Fig. 8.40 Typical vacuum-assisted resin transfer molding process setup. Source: Ref 8.1 More
Image
Published: 01 November 2010
Fig. 5.25 Conceptual process flow for resin transfer molding (RTM). Source: Ref 9 More
Image
Published: 01 November 2010
Fig. 5.40 Schematic of a typical resin transfer molding (RTM) process More
Image
Published: 01 November 2010
Fig. 5.45 Examples of resin transfer molding (RTM) carbon composite parts. Source: GKN Aerospace Services More
Image
Published: 01 November 2010
Fig. 5.46 Typical resin transfer molding (RTM) die More
Image
Published: 01 November 2010
Fig. 5.47 Matched-metal resin transfer molding (RTM) die complexity More
Image
Published: 01 November 2010
Fig. 5.51 Vacuum-assisted resin transfer molding (VARTM) of a large boat hull More
Image
Published: 01 November 2010
Fig. 5.52 Typical vacuum-assisted resin transfer molding (VARTM) process setup More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870119
EISBN: 978-1-62708-314-0
... for low-volume, medium-sized and larger parts. It also discusses filament winding and preforming processes (including weaving, knitting, stitching, and braiding) in addition to resin-transfer molding, resin film infusion, and pultrusion. continuous-fiber composites filament winding liquid molding...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780064
EISBN: 978-1-62708-281-5
... … … y y y n n y n y y Resin transfer molding 0.1 0.015 10 1120 … … n y n y n y n n y y High-speed resin transfer molding or fast resinject 2 0.3 30 3370 … … n y n y n y n n y y Foam polyurethane 0.5 0.07 n/a … … … n y y y y y n n y y...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030001
EISBN: 978-1-62708-349-2
... tape lay-up of prepreg materials, resin transfer molding, vacuum-assisted resin transfer molding, resin film infusion, wet lay-up, filament winding, pultrusion, and compression molding of sheet molding or bulk molding compound. While these processes are general in description, the actual process...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.9781627083492
EISBN: 978-1-62708-349-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860001
EISBN: 978-1-62708-338-6
... rather than hand lay-up, spray-up, resin transfer mold, or compression mold their elbows, reducers, and tees. Filament winding these components results in better mechanical properties through the use of continuous fibers, with the accompanying lowering of manufacturing costs ( Ref 1.2 ). Composite...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.9781627082815
EISBN: 978-1-62708-281-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780433
EISBN: 978-1-62708-281-5
... polyvinyl alcohol activation energy gas constant roughness average reaction injection molding reinforced reaction injection molding relative thermal index resin transfer molding uctuating stress Society of Automotive Engineers scanning Auger microscope styrene-acrylonitrile styrene butadiene styrene...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030177
EISBN: 978-1-62708-349-2
... modification are typically thermoplastic or rubber materials with average particle sizes between 20 and 50 μm ( Ref 10 ). This toughening concept is most often applied to prepreg materials and, not until recently, resin transfer-molding applications through the use of particle-modified tackifiers...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870285
EISBN: 978-1-62708-314-0
... reactive resins and short cycle times, SRIM cannot produce as large a part size as resin transfer molding see Chapter 5, “Thermoset Composite Fabrication Processes” . Also, SRIM parts have lower fiber volumes and generally more porosity than RTM parts. Fig. 10.19 Structural reaction injection...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550385
EISBN: 978-1-62708-307-2
... the primary advantages and disadvantages of polymer-matrix composites, how they are produced, and how they perform in different applications. It describes the construction of laminates, the fibers and resins used, and the methods by which they are combined. It explains how strength, modulus, toughness...