... to the specimen (assuming that these fixtures are in the hot zone of the furnace). The alternative, which poses its own set of problems, is the use of large specimens and grips outside the test furnace. Typical ferrous materials for grips, pullrods, pushrods, loading anvils, and so on, are limited...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220253
EISBN: 978-1-62708-341-6
... induction heating. (a) Brazing of brass watchband clips without flux in a forming-gas atmosphere. (b) Fixture using an elevator-pushrod arrangement. From Anon., Lepel Review , Vol 1, No. 10, p 1 ( Ref 2 ) Fig. 10.18 Hand-operated fixture for brazing of jewelry settings to gold rings by induction...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870537
EISBN: 978-1-62708-314-0
...-reinforced aluminum MMC is used in pushrods for high-performance racing engines. Hollow pushrods of several diameters are produced; the fibers are axially aligned along the pushrod length. Hardened steel end caps are then bonded to the ends of the MMC tubes. Continuous monofilament titanium matrix...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550457
EISBN: 978-1-62708-307-2
... greater than that of steel, and it has a density approximately one-third that of steel. The Al 2 O 3 /Al MMCs can be fabricated by a number of methods, but liquid or semisolid-state processing techniques are commonly used. A fiber-reinforced aluminum MMC is now used in pushrods for high-performance...