Skip Nav Destination
Close Modal
Search Results for
publish
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 578 Search Results for
publish
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780267
EISBN: 978-1-62708-281-5
...Abstract Abstract This article provides details on several of the classifications of polymer wear mechanisms, using wear data and micrographs from published works. The primary goals are to present the mechanisms of polymer wear and to quantify wear in terms of wear rate. The discussion begins...
Abstract
This article provides details on several of the classifications of polymer wear mechanisms, using wear data and micrographs from published works. The primary goals are to present the mechanisms of polymer wear and to quantify wear in terms of wear rate. The discussion begins by providing information on the processes involved in interfacial and cohesive wear. This is followed by sections describing the wear process and applications of elastomers, thermosets, glassy thermoplastics, and semicrystalline thermoplastics. The effects of environmental and lubricant on the wear failures of polymers are then discussed. The article further includes a case study describing the tribological performance of nylon. It ends by presenting some examples of wear failures of plastics.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090257
EISBN: 978-1-62708-266-2
...Abstract Abstract Stress-corrosion cracking (SCC) in magnesium alloys was first reported in the 1930s and, within ten years, became the focus of intense study. This chapter provides a summary of all known work published since then on the nature of SCC in magnesium alloys and how it is related...
Abstract
Stress-corrosion cracking (SCC) in magnesium alloys was first reported in the 1930s and, within ten years, became the focus of intense study. This chapter provides a summary of all known work published since then on the nature of SCC in magnesium alloys and how it is related to composition, microstructure, and heat treatment. It describes the types of environments where magnesium alloys are most susceptible to SCC and the effect of contributing factors such as temperature, strain rate, and applied and residual stresses. The chapter also discusses crack morphology and what it reveals, provides information on proposed cracking mechanisms, and presents a practical approach for preventing SCC.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130529
EISBN: 978-1-62708-284-6
...Abstract Abstract This appendix is a collection of tables listing examples of published hardness conversion equations, approximate Rockwell B and C hardness conversion numbers for nonaustenitic steels, and equivalent hardness numbers for Brinell hardness numbers and Vickers (diamond pyramid...
Abstract
This appendix is a collection of tables listing examples of published hardness conversion equations, approximate Rockwell B and C hardness conversion numbers for nonaustenitic steels, and equivalent hardness numbers for Brinell hardness numbers and Vickers (diamond pyramid) hardness numbers for steel.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120307
EISBN: 978-1-62708-269-3
...Abstract Abstract This appendix provides corrosion rate values for various grades of commercially pure and alloyed titanium. The values were derived from published sources and in-house laboratory tests. These data serve only as a starting point or initial guideline for corrosion performance...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200233
EISBN: 978-1-62708-354-6
...Abstract Abstract The design stresses for most pressure-containing structural application, which are based upon minimum mechanical properties designated in the specifications published by the American Society for Testing and Materials (ASTM). This chapter reviews metallurgical characteristics...
Abstract
The design stresses for most pressure-containing structural application, which are based upon minimum mechanical properties designated in the specifications published by the American Society for Testing and Materials (ASTM). This chapter reviews metallurgical characteristics and their influence on the properties and performance of structural carbon and low alloy steels and contains a summary of the relevant features of the ASTM product specifications.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140193
EISBN: 978-1-62708-335-5
... is representative of the behavior of several cast alloys under tensile or compressive loads. The curves are arranged by alloy designation. The curves are from the Atlas of Stress-Strain Curves , published by ASM International ( Ref 1 ). The original source of and, when available, some background on the data...
Abstract
The stress-strain curves in this data set are representative examples of the behavior of several cast alloys under tensile or compressive loads. The curves are arranged by alloy designation. Each figure cites the original source of the curve and provides pertinent background information as available. Compressive tangent modulus curves are presented for certain alloys. The effects of cyclic loading are given on several curves.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2010
DOI: 10.31399/asm.tb.hss.t52790257
EISBN: 978-1-62708-356-0
... Guillet Léon B. Guillet, professor of metallurgy and metal processing at the Conservatoire des Arts et Métiers, publishes a series of research on iron-chromium alloys having carbon contents acceptably low for modern stainless steel analyses. He made his steels with carbon-free Goldschmidt chromium...
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420143
EISBN: 978-1-62708-310-2
..., and Structure on Properties of Irons and Steels , Materials Selection and Design , Vol 20 , ASM Handbook , ASM International , 1997 10.31399/asm.hb.v20.a0002461 8.5 Guy A.G. and Hren J.R. , Elements of Physical Metallurgy , 3rd ed. , Addison-Wesley Publishing Company , 1974 8.6...
Abstract
This chapter discusses the characteristics of eutectoid transformations, a type of solid-state transformation associated with invariant reactions, focusing on the iron-carbon system of steel. It describes the compositions, characteristics, and properties of ferrite, eutectoid, hypoeutectoid, and hypereutectoid structures and how they are affected by the addition of various alloying elements. The chapter also discusses the formation of peritectoid structures in the uranium-silicon alloy system.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420135
EISBN: 978-1-62708-310-2
... eventually undergoes a eutectic reaction, producing α and β, where the β is almost pure lead. The microstructure of this alloy contains spherical β particles randomly distributed in a matrix of copper-rich α. Fig. 7.2 Monotectic reaction in copper-lead system. Source: Ref 7.2 as published in Ref...
Abstract
This chapter provides a brief overview of monotectic alloy systems and reactions. It begins by presenting a monotectic phase diagram and identifying important points, lines, and regions. It then describes the monotectic reactions that occur in copper-lead systems and the associated solidification structures. It also discusses the morphology of the microstructure produced during directional solidification and the classification criteria of low- and high-dome alloys.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2010
DOI: 10.31399/asm.tb.hss.9781627083560
EISBN: 978-1-62708-356-0
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420303
EISBN: 978-1-62708-310-2
... Transformation of retained austenite to ferrite and cementite 200–300 390–570 III Replacement of the transition carbide and low-carbon martensite by cementite and ferrite 250–350 480–660 Source: Ref 15.8 as published in Ref 15.9 Tempering reactions in steel Table 15.2 Tempering...
Abstract
This chapter examines two important strengthening mechanisms, martensitic and bainitic transformations, both of which occur under nonequilibrium cooling conditions. It explains how time-temperature-transformation diagrams are constructed and how they are used to understand and control the formation of martensite and bainite in steel and other alloys. It describes the morphology of both types of structures, the factors that influence their formation, how they respond to tempering processes, and their effect on mechanical properties and behaviors. It also discusses the role of transformation hysteresis in shape memory alloys.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420429
EISBN: 978-1-62708-310-2
... –0.95 Si Diamond cubic –12 (a) fcc, face-centered cubic; hcp, hexagonal close-packed; bcc, body-centered cubic; bct, body-centered tetragonal. Source: Ref B.2 Fig. B.13 Porosity in cast metals. Source: Ref B.7 as published in Ref B.2 Fig. B.3 Dendrite formation...
Abstract
The solidification process has a major influence on the microstructure and mechanical properties of metal casting as well as wrought products. This appendix covers the fundamentals of solidification. It discusses the formation of solidification structures, the characteristics of planar, cellular, and dendritic growth, the basic freezing sequence for an alloy casting, and the variations in cooling rate, heat flow, and grain morphology in different areas of the mold. It also describes the types of segregation that occur during freezing, the effect of solidification rate on secondary dendrite arm spacing, and the factors that contribute to porosity and shrinkage.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 May 2018
DOI: 10.31399/asm.tb.hma.t59250059
EISBN: 978-1-62708-287-7
... , 1935 Howe H.M. , The Metallurgy of Steel , Vol 1 , The Scientific Publishing Company , 1892 Johnson W.A. and Mehl R.F. , Reaction Kinetics in Processes of Nucleation and Growth , Trans. Am. Instit. Min. Metall. Eng. , Vol 135 , 1939 , p 416 – 42 Jominy W.E...
Abstract
This chapter discusses the evolution of engineering alloy steels, namely chromium, nickel, and nickel-chromium alloy steels. The discussion includes the automotive demand and development of specifications for the alloy steels. It also covers various research on heat treatment of alloy steels, providing information on hardening, transformation of austenite, hardenability testing, and tempering of as-quenched martensite.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420117
EISBN: 978-1-62708-310-2
... systems. (a) Type A system where the β/α + β solvus and the β solidus have slopes of the same sign. (b) Type B system where the slopes have opposite signs. (c) Type C system where the β phase has a limited composition. Source: Ref 6.1 as published in Ref 6.4 Peritectic reactions can proceed...
Abstract
This chapter discusses the phase transformations of peritectic alloy systems. It describes the processes involved with equilibrium and nonequilibrium freezing, the mechanisms of peritectic formation, and the resulting microstructures. It also discusses the formation of peritectic structures in iron-base alloys and multicomponent systems.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2010
DOI: 10.31399/asm.tb.hss.t52790059
EISBN: 978-1-62708-356-0
... for his invention of Hadfield’s manganese steel. Dr. William Hatfield was the Director of the Firth Brown Laboratories in 1916, succeeding Harry Brearley and continuing Brearley’s work on stainless steel. Hatfield published a report entitled “Heat Treatment of Aircraft Steels” in the British...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.htpa.t53310235
EISBN: 978-1-62708-346-1
... of the interested parties and for the benefit of the community as a whole, it prepares, publishes, and promotes the implementation of German Standards or other results of standards work which serve to advance rationalization, quality assurance, environmental protection, safety, and communication in industry...
Abstract
This chapter reviews the general principles involved in codifying standards and describes the historical development of materials testing standards. It provides information on the standards related to the Brinell, Vickers, Rockwell, and Knoop methods as well as those for the instrumented indentation test and hardness conversions.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420171
EISBN: 978-1-62708-310-2
... Source: Ref 9.2 as published in Ref 9.3 Antiphase Boundaries Long-Range and Short-Range Order L1<sub>0</sub> Superlattice (CuAu I Structure) L1<sub>2</sub> Superlattice (Cu<sub>3</sub>Au Structure) B2 Superlattice (FeAl Structure) D0<sub>3</sub> Superlattice (Fe<sub>3</sub>Al...
Abstract
This chapter explains how the presence of intermediate phases affects the melting behavior of binary alloys and the transformations that occur under different rates of cooling. It begins by examining the phase diagrams of magnesium-lead and copper-zinc, noting some of the complexities associated with intermediate phases. It then discusses the difference between ordered and disordered phases and how they are accounted for on phase diagrams. It describes how the atoms in a disordered solution may arrange themselves into an ordered array, forming a superlattice in the process of cooling, and goes on to identify the most common superlattice structures and their corresponding alloy phases. It also discusses the factors that limit the formation of superlattices along with the kinetics of spinodal decomposition and its effect on microstructure development.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 May 2018
DOI: 10.31399/asm.tb.hma.t59250153
EISBN: 978-1-62708-287-7
... Henry Marion Howe Albert Sauveur Isaiah (Zay) Jeffries Paul Dyer Merica Edgar C. Bain Samuel Leslie Hoyt Francis L. VerSnyder References References 1. Howe H.M. , The Metallurgy of Steel , Vol 1 , The Scientific Publishing Company , 1890 2. Hoyt S.L...
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420339
EISBN: 978-1-62708-310-2
... as published in Ref 16.3 Surface energies for different types of interfaces Table 16.2 Surface energies for different types of interfaces Type of interface Surface energy Coherent γ coherent = γ chemical ≤ 200 mJ/m 2 Semicoherent γ semicoherent = γ chemical + γ structural ≈ 200...
Abstract
This chapter discusses the basic principles of precipitation hardening, an important strengthening mechanism in nonferrous alloys as well as stainless steel. It begins with a detailed review of the theory of precipitation hardening, then describes its application to aluminum alloys and nickel-base superalloys.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420087
EISBN: 978-1-62708-310-2
... Publishing Company , 1959 5.4 Rooy E.L. and Kearney A. , Aluminum Foundry Products , Properties and Selection: Nonferrous Alloys and Special-Purpose Materials , Vol 2 , ASM Handbook , ASM International , 1990 5.5 Smith W.F. , Principles of Materials Science...
Abstract
This chapter begins by presenting a generic eutectic phase diagram and identifying critical points, lines, and features. It then describes the composition and properties of aluminum-silicon and lead-tin eutectic systems, the characteristics of eutectic morphologies, the solidification and scale of eutectic structures, and the competitive growth of dendrites and eutectic colonies or cells. It also examines the different types of precipitation structures that form during slow cooling cycles.