1-20 of 805 Search Results for

process considerations

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.pnfn.t65900013
EISBN: 978-1-62708-350-8
... strength. This chapter focuses on key process considerations and factors that helped nitriding gain acceptance. These factors include a low-temperature process, no quench requirement, minimal distortion, high hardness values, and resistance to oxidation. distortion hardness nitriding oxidation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290001
EISBN: 978-1-62708-306-5
...Abstract Abstract Joining comprises a large number of processes used to assemble individual parts into a larger, more complex component or assembly. The selection of an appropriate design to join parts is based on several considerations related to both the product and the joining process. Many...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780064
EISBN: 978-1-62708-281-5
...Abstract Abstract This article describes key processing methods and related design, manufacturing, and application considerations for plastic parts and includes a discussion on materials and process selection methodology for plastics. The discussion covers the primary plastic processing methods...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1999
DOI: 10.31399/asm.tb.cmp.t66770037
EISBN: 978-1-62708-337-9
.... Decarburization might signify an equipment failure. Long reheating times in air are not recommended. In-process considerations: Atmosphere monitoring system might indicate a problem. Reheating in air is not recommended. Postprocess considerations: Post-process corrections depend on the degree...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1999
DOI: 10.31399/asm.tb.cmp.t66770135
EISBN: 978-1-62708-337-9
.... Composition: 0.67 Mn, 0.90 Cr, 0.12 Mo, 1.32 Ni, 0.00 Si, 0.000 P, 0.000 S. Source: Ref 1 Fig. 6.21 Case hardenabilities of a number of carburizing steels with oil quenching. Source: Ref 1 Abstract Abstract The design of case-hardened components is an iterative process, requiring...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.pnfn.t65900089
EISBN: 978-1-62708-350-8
... and processing. Other important considerations discussed include the hollow cathode effect, sputter cleaning, furnace loading, pressure/voltage relationships, workpiece masking, and furnace configuration options. The chapter describes five methods of cooling parts from the process temperature to an acceptable...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910301
EISBN: 978-1-62708-250-1
...% of the time, designers 55%, material suppliers 37%, and contractors only 11% of the time ( Ref 1 ). Design as a Process General Considerations in Corrosion-Control Design Design Details that Accelerate Corrosion Design Solutions for Specific Forms of Corrosion Corrosion Allowance Design...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310213
EISBN: 978-1-62708-286-0
...Abstract Abstract This chapter deals with the technology of stainless steel as it pertains to its proper use in architecture, art, and construction. It begins with an overview of the corrosion resistance of stainless steel, providing guidelines for balancing corrosion resistance, processing...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310233
EISBN: 978-1-62708-326-3
...), martensitic, and precipitation-hardening. In addition, information on special considerations for stainless steel castings is also provided. The heat treatment processes explained in the chapter are preheating, annealing, stress relieving, hardening, tempering, austenite conditioning, heat aging, and nitride...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350195
EISBN: 978-1-62708-315-7
... operations may be required before or after processing and how to estimate or predict coating thickness, case depth, hardness, and the likelihood of distortion. It also addresses related issues and considerations such as part handling and fixturing, surface preparation and cleaning requirements...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220085
EISBN: 978-1-62708-341-6
... Typical channel induction melting furnace Source: Inductotherm Abstract Abstract The detailed heating requirements for specific applications must be considered before construction and implementation of any induction heating process. These requirements may include considerations such as type...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220315
EISBN: 978-1-62708-341-6
... to illustrate the economic considerations in design and application of induction heating processes. References References 1. Burwell C. C. , “ Industrial Electrification: Current Trends ,” Research Memorandum 0RAU/IEA-83-4 (M), Institute for Energy Analysis , Oak Ridge Associated Universities...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440283
EISBN: 978-1-62708-262-4
..., and ferritic nitrocarburizing to provide an accurate heat treating process evaluation. This appendix briefly describes the advantages and selection and design considerations of test coupons. A typical example of the use of test pins for monitoring carburizing and hardening of gears is provided. Reference...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110001
EISBN: 978-1-62708-247-1
... This article introduces the wafer-level fault localization failure analysis (FA) process flow for an accelerated yield ramp-up of integrated circuits. It discusses the primary design considerations of a fault localization system with an emphasis on complex tester-based applications. The article presents...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.htgpge.t67320033
EISBN: 978-1-62708-347-8
..., manganese, molybdenum), normally are used. The processes involved in hardening, tempering, recarburizing, and cold treatment of carburized and quenched gears are discussed. Next, the chapter reviews the selection of materials for carburized gears and considerations related to carbon content, core hardness...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410151
EISBN: 978-1-62708-280-8
... of the processes involved in post-casting operations, namely de-coring and de-gating. The key design aspects for consideration in water quenching during the T6 heat treatment are reviewed. The chapter also provides information on two critical cycle events important in engineering at the manufacturing facility...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290243
EISBN: 978-1-62708-306-5
...Abstract Abstract Adhesive bonding is a widely used industrial joining process in which a polymeric material is used to join two separate pieces (the adherends or substrates). This chapter begins with a discussion on the advantages and disadvantages of adhesive bonding, followed by a section...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110402
EISBN: 978-1-62708-247-1
... mm or more, and as thin as 0.1 mm (after thinning). The thickness of the sample will vary greatly depending on the wafer’s processing level. A failure analyst has many considerations prior to beginning analysis on a wafer. One must consider (i) the number of layers and types of materials present...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910331
EISBN: 978-1-62708-250-1
... of candidate materials, the in-depth evaluation of each candidate material, fabrication requirements, follow-up monitoring, and final materials selection. Material considerations such as cost, materials properties, and processing and fabrication requirements are subsequently covered. Finally, the chapter...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280135
EISBN: 978-1-62708-267-9
...-temperature exposures without changing alloy properties. The time and temperature cycles for stress relief may vary considerably, depending on the metallurgical characteristics of the alloy and on the type and magnitude of residual stresses developed by previous fabricating processes. Stress-relieving...