1-20 of 406 Search Results for

precipitation-hardenable stainless steel

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310137
EISBN: 978-1-62708-286-0
... Abstract This chapter discusses the composition, alloying characteristics, mechanical properties, corrosion resistance, advantages, limitations, and applications of martensitic, semiaustenitic, and austenitic precipitation-hardenable stainless steels. mechanical properties corrosion...
Image
Published: 01 March 2002
Fig. 8.42 Lath martensite in a precipitation-hardening stainless steel (Custom 630). Kalling’s reagent #2. 200× More
Image
Published: 01 March 2002
Fig. 8.43 Lath martensite in a precipitation-hardening stainless steel (Custom 630). Fry’s reagent. 250× More
Image
Published: 01 June 2008
Fig. 23.11 Comparison of heat treatments for precipitation-hardenable stainless steels More
Image
Published: 01 June 2008
Fig. 23.13 Tempering response of several precipitation-hardenable stainless steels. Source: Ref 8 More
Image
Published: 01 March 2002
Fig. 1.17 Micrograph of a precipitation-hardening stainless steel (Custom 630) showing a microstructure consisting of martensite. Etched in Fry’s reagent. 320× More
Image
Published: 01 November 2007
Fig. 13.24 Compositions of the three precipitation-hardening stainless steels in Table 13.15 plotted on the metastable phase diagram shown in Fig. 13.20 More
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220551
EISBN: 978-1-62708-259-4
... (duplex), and precipitation hardening stainless steels. It also describes solidification sequences and explains how chromium carbides may segregate to grain boundaries at certain temperatures, making grain boundary regions susceptible to intercrystalline or intergranular corrosion. austenitic...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140133
EISBN: 978-1-62708-264-8
... Abstract Stainless steels derive their name from their corrosion-resisting properties first observed in 1912. Two groups, working independently, concurrently discovered what came to be known as austenitic and ferritic stainless steels. Martensitic and precipitation-hardened stainless steels...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170257
EISBN: 978-1-62708-297-6
... Abstract This article covers the metallurgy and properties of stainless steels. It provides composition information on all types of ferritic, austenitic, martensitic, duplex, and precipitation-hardening stainless steels, including proprietary and nonstandard grades, along with corresponding...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240135
EISBN: 978-1-62708-251-8
... Abstract Precipitation hardening is used extensively to strengthen aluminum alloys, magnesium alloys, nickel-base superalloys, beryllium-copper alloys, and precipitation-hardening stainless steels. This chapter discusses two types of particle strengthening: precipitation hardening, which takes...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090095
EISBN: 978-1-62708-266-2
..., polythionic acid, and high-temperature environments and the correlating effects on austenitic, ferritic, duplex, martensitic, and precipitation hardening stainless steels and nickel-base alloys. It also discusses the contributing effects of sensitization and hydrogen embrittlement and the role of composition...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000005
EISBN: 978-1-62708-312-6
... characteristics of austenitic, ferritic, martensitic, duplex, and precipitation hardening stainless steel powders and metal injection molding grades. alloy composition stainless steel stainless steel powder 2.1 Introduction STAINLESS STEELS, as a class of ferrous alloys, are mainly distinguished...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310201
EISBN: 978-1-62708-286-0
... of the categories of stainless steels, namely austenitic, duplex, ferritic, martensitic, and precipitation-hardening stainless steels. This is followed by a discussion of the selection criteria for materials to be welded. Various welding processes used with stainless steel are then described. The chapter ends...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410579
EISBN: 978-1-62708-265-5
... detrimental to corrosion resistance or toughness. In austenitic stainless steels, strength is also developed by cold work and strain-induced martensite formation. Martensitic stainless steels can be heat treated by quench and tempering to high hardness and strength. Precipitation-hardening grades of stainless...
Image
Published: 01 January 2015
Fig. 23.30 Fine, disc-shaped γ′ precipitates in an aged austenitic precipitation-hardening stainless steel, JBK-75. Transmission electron micrograph. Source: Ref 23.53 More
Image
Published: 01 January 2015
Fig. 23.28 Martensite start (M s ) temperatures as a function of austenitizing temperature for several precipitation-hardening stainless steels. Data from references listed in Ref 23.51 . Source: Ref 23.51 More
Image
Published: 01 January 2015
Fig. 23.27 Solution-treated and aged microstructure of martensitic precipitation-hardening stainless steel PH 13-8 Mo. Etched in Fry’s reagent. Light micrograph. Courtesy of G. Vander Voort, Carpenter Technology Corp., Reading, PA More
Image
Published: 01 August 2005
Fig. A10.5 Plane-strain fracture toughness of PH13-8Mo and Custom 465 precipitation-hardening stainless steels. ○, PH13-8Mo (Source: Ref A10.5 ); ●, PH13-8Mo (Source: Ref A10.1 ); ◊, Custom 465 (Source: Ref A10.1 ) More
Image
Published: 01 August 2018
Fig. 16.42 Longitudinal cross sections of a 100 mm (4 in.) diameter bar of 17-4PH precipitation hardening stainless steel. (a) Martensite with presence of segregated areas containing retained austenite. (b) Presence of delta ferrite. In some oil industry specifications, these conditions More