1-20 of 446 Search Results for

precipitation hardenability

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240135
EISBN: 978-1-62708-251-8
...Abstract Abstract Precipitation hardening is used extensively to strengthen aluminum alloys, magnesium alloys, nickel-base superalloys, beryllium-copper alloys, and precipitation-hardening stainless steels. This chapter discusses two types of particle strengthening: precipitation hardening...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310137
EISBN: 978-1-62708-286-0
...Mechanical properties of martensitic precipitation-hardenable alloys Table 1 Mechanical properties of martensitic precipitation-hardenable alloys Alloy UNS Condition Yield, MPa Tensile, MPa Elongation, % HRC Toughness, CVN ft-lb Stainless W S17600 H-950 (510) 1240 1340 14...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420339
EISBN: 978-1-62708-310-2
...Abstract Abstract This chapter discusses the basic principles of precipitation hardening, an important strengthening mechanism in nonferrous alloys as well as stainless steel. It begins with a detailed review of the theory of precipitation hardening, then describes its application to aluminum...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280135
EISBN: 978-1-62708-267-9
...Abstract Abstract All superalloys, whether precipitation hardened or not, are heated at some point in their production for a subsequent processing step or, as needed, to alter their microstructure. This chapter discusses the changes that occur in superalloys during heat treatment and the many...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280149
EISBN: 978-1-62708-267-9
... decisions. It discusses the basic concepts of fusion welding and the differences between solid-solution-hardened and precipitation-hardened wrought superalloys. It addresses joint integrity, design, weld-related cracking, and the effect of grain size, precipitates, and contaminants. It covers common fusion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290099
EISBN: 978-1-62708-306-5
... and the solid-state transformations of the main classes of metals and alloys during fusion welding. The main classes include work- or strain-hardened metals and alloys, precipitation-hardened alloys, transformation-hardened steels and cast irons, stainless steels, and solid-solution and dispersion-hardened...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310163
EISBN: 978-1-62708-326-3
... hardening of 0.06% C steel after quenching from 720 °C (1325 °F) Fig. 33 Partial iron-copper phase diagram showing the solubility of copper in αFe (bcc) at temperatures below 910 °C (1670 °F) Fig. 34 Precipitation hardening of a 1.6Cu-0.06C steel after quenching from 815 °C (1500 °F...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740271
EISBN: 978-1-62708-308-9
... embrittlement and discusses the effect of precipitation hardening on aluminum and other alloys. continuous cooling transformation diagrams hardenability heat treatment temper embrittlement ONE OF THE PRIMARY advantages of steels is their ability to attain high strengths through heat treatment...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310233
EISBN: 978-1-62708-326-3
...), martensitic, and precipitation-hardening. In addition, information on special considerations for stainless steel castings is also provided. The heat treatment processes explained in the chapter are preheating, annealing, stress relieving, hardening, tempering, austenite conditioning, heat aging, and nitride...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140133
EISBN: 978-1-62708-264-8
...Abstract Abstract Stainless steels derive their name from their corrosion-resisting properties first observed in 1912. Two groups, working independently, concurrently discovered what came to be known as austenitic and ferritic stainless steels. Martensitic and precipitation-hardened stainless...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280091
EISBN: 978-1-62708-267-9
... practical concerns such as forming speed, rolling direction, rerolling, and heat treating precipitation-hardened alloys. It presents several application examples involving carbide-hardened cobalt-base and other superalloys, and it concludes with a discussion on superplasticity and its adaptation...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550033
EISBN: 978-1-62708-307-2
..., designations, and achievable strengths. It explains how some alloys are hardened through solution strengthening and cold working, while others are strengthened by precipitation hardening. It also describes production and fabrication processes such as melting, casting, rolling, forging, forming, extruding, heat...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000017
EISBN: 978-1-62708-313-3
...Abstract Abstract This chapter discusses the metallurgical changes that occur and the improvements that can be achieved in superalloys through solid-solution hardening, precipitation hardening, and dispersion strengthening. It also explains how further improvements can be achieved through...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170257
EISBN: 978-1-62708-297-6
...Abstract Abstract This article covers the metallurgy and properties of stainless steels. It provides composition information on all types of ferritic, austenitic, martensitic, duplex, and precipitation-hardening stainless steels, including proprietary and nonstandard grades, along...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440159
EISBN: 978-1-62708-262-4
..., precipitation-hardening, and duplex grades. The chapter also describes the heat treatment conditions that should be followed for processing of stainless steels. References References 1. Boyer H.E. , Chapter 11, Practical Heat Treating , 1st ed. , American Society for Metals , 1984 , p 196...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440175
EISBN: 978-1-62708-262-4
... S44004 440C 0.95–1.20 1.00 1.00 16.0–18.0 … 0.04 0.03 0.75 Mo (a) Single values are maximum values unless otherwise indicated. (b) Optional. Source: Ref 1 Chemical compositions of precipitation-hardening stainless steels Table 5 Chemical compositions of precipitation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090095
EISBN: 978-1-62708-266-2
..., caustic, polythionic acid, and high-temperature environments and the correlating effects on austenitic, ferritic, duplex, martensitic, and precipitation hardening stainless steels and nickel-base alloys. It also discusses the contributing effects of sensitization and hydrogen embrittlement and the role...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240433
EISBN: 978-1-62708-251-8
...Abstract Abstract This chapter discusses the classification, composition, properties, and applications of five types of stainless steels: austenitic, ferritic, duplex, martensitic, and precipitation-hardening steels. It discusses the process involved in argon oxygen decarburization that is used...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310001
EISBN: 978-1-62708-286-0
... of the principal intermetallic phases is also covered. In addition, the chapter provides information on carbides, nitrides, precipitation hardening, and inclusions. stainless steel thermodynamics ferrite austenite martensite intermetallic phase carbides nitrides precipitation hardening inclusions...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310161
EISBN: 978-1-62708-286-0
... quench 730 °C 16 h, 650 °C 8 h ST1800 980 °C 120 min, oil/water quench ST1800A 980 °C 120 min, oil/water quench 730 °C 16 h PH, precipitation-hardenable; RT, room temperature. Recommended annealing and stress-relieving temperatures for duplex alloys Table 5 Recommended...