1-20 of 218 Search Results for

powder-in-tube processing

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460107
EISBN: 978-1-62708-285-3
.... This device offers the option to adjust the powder injection point and thereby the distance between nozzle throat and powder tube. Fig. 4.6 Inside diameter spray head. Courtesy of Impact Innovations GmbH Fig. 4.7 Inside diameter spray adapter. Courtesy of Impact Innovations GmbH Fig...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980195
EISBN: 978-1-62708-342-3
..., nickel, and powder metals. It discusses their properties and applications as well as suitable equipment for extrusion. It further discusses the processes involved in the extrusion of semifinished products in exotic alloys and extrusion of semifinished products from metallic composite materials...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460227
EISBN: 978-1-62708-285-3
... is shown in Fig. 9.27(a) . The tubing in Fig. 9.27(b) shows the deposition after the surface has been finished. This application demonstrated the ability of cold spray to produce high-quality CP-Ti depositions. Fig. 9.27 Hydraulic tubing with commercially pure titanium powder deposited to prevent...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060117
EISBN: 978-1-62708-261-7
... to produce the desired degree of bend or bend angle after springback. Bending of bar and Tube Sheet Forming Powder metallurgy (PM) is a growing branch of metallurgy based on the production of materials in the form of metal powders and the manufacturing of parts from these materials. The primary...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290001
EISBN: 978-1-62708-319-5
...-cutting inserts Warm extrusion Long, thin, constant wall thickness Honeycomb, tube, rod, spiral Twist drills, filters Green machining Solid interior, surface removal Three-dimensional rough surface Forming tools Powder injection molding Small, complex, thin wall, steps, below 1 kg Three...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220281
EISBN: 978-1-62708-341-6
.... Fig. 11.16 Bonding of aluminum/polyethylene joints (such as for toothpaste tubes) with a high-frequency induction coil and ferrite flux modifier Fig. 11.6 Photograph of a processing line for induction curing of a polyimide film on wire Source: Lepel Corp. Fig. 11.7 Schematic...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280117
EISBN: 978-1-62708-267-9
... and worked under conditions that develop coarse grains during a secondary recrystallization heat treatment. Consequently, MA powder is consolidated and then heat treated to optimize grain structure and properties. After MA, the powder generally is put into low-carbon steel tubes and extruded to full density...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290111
EISBN: 978-1-62708-319-5
... is slid into a metallic cylinder slightly larger in diameter than that of the outer diameter of the flexible mold. The metal tube has perforations that allow for the flow of the liquid between the metal tube and the flexible mold containing the powder. This helps to prevent long, thin samples from...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.t53730139
EISBN: 978-1-62708-283-9
...Abstract Abstract This chapter describes the processes, applications, and limitations of forming and shaping various materials. It discusses bulk forming, hot working, cold working, sheet forming, and polymer and powder processing. bulk forming cold working hot working polymer...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720183
EISBN: 978-1-62708-305-8
...., in width) by capillary action. Therefore, the process is well suited to detect all types of surface cracks, laps, porosity, shrinkage areas, laminations, and similar discontinuities. It is used extensively to inspect ferrous and nonferrous metal wrought and cast products, powder metallurgy parts, ceramics...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000039
EISBN: 978-1-62708-312-6
... material is removed by decladding. With extrusion ratios of 20 to 30, seamless tubes 10 to 15 m (33 to 50 ft) long are produced. Advantages of the PM process over the conventional wrought billet route include: POWDER METALLURGY (PM) employs many methods for compacting and shaping of powders. The vast...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430107
EISBN: 978-1-62708-253-2
...–100 (70–93) Chemically clean within three months > 100 (93) Chemically clean before further operation Inclusion rating in a boiler tube sample Table 5.1 Inclusion rating in a boiler tube sample Type A Type B Type C Type D Thin Thick/heavy Thin Thick/heavy Thin Thick...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120295
EISBN: 978-1-62708-269-3
.... Hardyston, NJ 07460 Tel: 973-328-3228 High-purity and commercial grade alloys, 99.99%; iodide crystal bar, billet, powder, sheet, rod Metalsource, Inc. 2726 Kanasita Dr. Chattanooga, TN 37343 Tel: 800-487-6382 Fax: 423-870-7800 Titanium tubing, grinding, milling, turning burnouts, blanchard-surface...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.9781627083195
EISBN: 978-1-62708-319-5
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240583
EISBN: 978-1-62708-251-8
..., electron tube electrodes, and various types of heating elements. Silicide coatings and noble metal claddings, such as platinum-gold alloys, are effective oxidation-resistant coatings. Powder metallurgy is used to produce most tungsten parts. Whether formed into ingots or bars for further processing...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550193
EISBN: 978-1-62708-307-2
... of beryllium makes it practically transparent to x-rays and other high-energy electromagnetic radiation. It is therefore used as a window material in x-ray tubes and detectors such as those used in energy-dispersive analysis of x-ray equipment. Powder metallurgy is required for a number of reasons...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230295
EISBN: 978-1-62708-298-3
... material and of loose powder. The can for a cylindrical billet consists of outer seamless carbon steel tube and two end plugs. The carbon steel end plugs are 3 to 6 mm (0.125 to 0.250 in.) thick. A groove to facilitate welding to the outer can may be provided. Some producers feel that the front end...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310155
EISBN: 978-1-62708-286-0
... powder in an evacuated canister in which it can be sintered and hot worked to 100% density and virtually complete homogeneity. Chapter 9 on martensitic alloys discusses these materials. Hot rolling remains an essential process for the vast majority of stainless steel used. Hot rolling...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460209
EISBN: 978-1-62708-285-3
... Grujicic M. , Zhao C.L. , Tong C. , DeRosset W.S. , and Helfritch D. , Analysis of the Impact Velocity of Powder Particles in the Cold-Gas Dynamic-Spray Process , Mater. Sci. Eng. A , Vol 368 , 2004 , p 222 – 230 10.1016/j.msea.2003.10.312 8.6 Jodoin B. , Cold...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550511
EISBN: 978-1-62708-307-2
... processing Heat recovery, hot-gas cleanup, general thermal processing Thermal stress resistance, corrosion resistance, and dimensional stability at extreme temperatures Compact heat exchanges, heat exchanger tubes, radiant tubes, furnace components, insulators, thermocouple protection tubes, kiln...