1-20 of 123 Search Results for

polymeric composites

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030245
EISBN: 978-1-62708-349-2
...Abstract Abstract Lightning damage in polymer composites, as in metal structures, is manifested by damage at both the macroscopic or visual level and within the material microstructure. In addition to visual damage assessment, non-destructive inspection techniques are employed to detect damage...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030067
EISBN: 978-1-62708-349-2
...Abstract Abstract The most common methods for preparing polymeric composites for microscopic analysis can be used for most fiber-reinforced composite materials. There are, however, a few composite materials that require special preparation techniques. This chapter discusses the processes...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030115
EISBN: 978-1-62708-349-2
...Abstract Abstract Transmitted-light methods reveal more details of the morphology of fiber-reinforced polymeric composites than are observable using any other available microscopy techniques. This chapter describes the various aspects relating to the selection and preparation of ultrathin...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030193
EISBN: 978-1-62708-349-2
...Abstract Abstract As fiber-reinforced polymeric composites continue to be used in more damage-prone environments, it is necessary to understand the response of these materials when subjected to impact from foreign objects. This chapter provides an overview of the analysis methods for impact...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030237
EISBN: 978-1-62708-349-2
...Abstract Abstract Polymer composite materials are subject to degradation if not appropriately protected from the environment. Composite materials having polymeric matrices are susceptible to degradation from heat, sunlight, ozone, atomic oxygen (in space), moisture, solvents (chemicals...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030089
EISBN: 978-1-62708-349-2
... materials. Different composites present different types of resoluble features, depending on the reflectivity of the individual components present. The carbon fibers tend to be very reflective (show a high degree of contrast) and are easily resolved in polymeric resins. By comparison, glass fiber composites...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030211
EISBN: 978-1-62708-349-2
... of a carbon fiber. Transmitted polarized light, 100× objective The use of fiber-reinforced polymeric composite materials continues to increase throughout the world due to their unique performance attributes. These heterogeneous and anisotropic materials are commonly developed from carbon or glass...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.9781627083492
EISBN: 978-1-62708-349-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030001
EISBN: 978-1-62708-349-2
.../Foam Structure Composite Materials Optical Microscopy of Composite Materials References References 1. Halpin J.C. , The Role of the Polymeric Matrix in the Processing and Structural Properties of Composite Materials , Nicolais L. and Seferis J.C. , Ed., Plenum Press...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870235
EISBN: 978-1-62708-314-0
.... Source: Ref 1 Fig. 8.2 Effect of aluminum surface treatments on bond durability. Source: Ref 2 Abstract Abstract This chapter explains how polymeric adhesives are applied to composite as well as metal parts, forming bonded structures. It describes surface preparation practices...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780314
EISBN: 978-1-62708-281-5
...Abstract Abstract This article describes the mechanisms of moisture-induced damage in polymeric materials, covering the characteristics of important structural plastics; the effects of moisture on glass transition temperature, modulus, creep, and stress relaxation of plastic materials...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870489
EISBN: 978-1-62708-314-0
... system and cure method. Source: Ref 1 Common trade-offs when selecting composite materials Table 18.1 Common trade-offs when selecting composite materials Design decision Common trade-offs Typically lowest cost Typically highest performance Fiber type Cost, strength, stiffness...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870001
EISBN: 978-1-62708-314-0
.... Tuttle M.E. , Structural Analysis of Polymeric Composite Materials , Marcel Dekker, Inc. , 2004 10.1201/9780203913314 2. Niu M.C.Y. , Composite Airframe Structures , 2nd ed. , Hong Kong Conmilit Press Limited , 2000 3. Horton R.E. and McCarty J.E. , Damage...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780146
EISBN: 978-1-62708-281-5
.... and Deanin R.D. , Ed., History of Polymeric Composites , VNU Science Press , 1987 4. Semon W.L. , U.S. Patent 1,929,453 , 1933 5. Foss P.H. and Shaw M.T. , J. Vinyl Technol. , No. 12 , 1985 , p 165 6. Moureau C. and Dufraisse C. , Bull. Soc. Chim...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550385
EISBN: 978-1-62708-307-2
... painted before being placed in service. In polymeric composites, a strength loss of aramid composites has not been observed. Being an organic fiber that is susceptible to oxidation, aramid composites are generally not used for long times at temperatures above 149 °C (300 °F). In the transverse direction...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870401
EISBN: 978-1-62708-314-0
... of potential environments that can cause varying degrees of loss of performance will be covered. Since water is pervasive, moisture absorption in polymeric matrix composites is a primary concern. Other potential degradation conditions covered include fluids, ultraviolet radiation, erosion, lightning strikes...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780276
EISBN: 978-1-62708-281-5
.... , Wear Models for Multiphase Materials and Synergistic Effects in Polymeric Hybrid Composites , Advances in Composite Tribology, Composite Materials Series 8 , Friedrich K. , Ed., Elsevier , 1993 , p 209 – 273 10.1016/B978-0-444-89079-5.50010-6 6. Suh N.P. , Tribophysics...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780259
EISBN: 978-1-62708-281-5
...Abstract Abstract This article focuses on friction and wear as they relate to polymeric materials, covering friction and wear applications for polymeric materials. The discussion covers the causes and mechanisms of friction, wear, and lubrication; different test methods developed to simulate...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780359
EISBN: 978-1-62708-281-5
... and gas chromatography-mass spectroscopy, are extremely useful in assessing low-concentration additives within a plastic resin. Nuclear magnetic resonance spectroscopy is useful in polymeric analysis, providing information related to composition beyond FTIR. Nuclear magnetic resonance can provide data...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780267
EISBN: 978-1-62708-281-5
.... , The Role of the Counterface Roughness in the Friction and Wear of Carbon Fibre Reinforced Thermosetting Resins , Wear , Vol 16 , 1970 , p 357 – 374 10.1016/0043-1648(70)90102-X 27. Bhushan B. and Wilcock D.F. , Wear Behaviour of Polymeric Compositions in Dry Reciprocating Sliding...