1-19 of 19 Search Results for

pneumatic pressure vessel

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780131
EISBN: 978-1-62708-268-6
... or creation of excess pressure in areas where the liquid or gas migrates. Leaks can induce failure to function or inadvertent function in hydraulic or pneumatic logic mechanisms. Leaks can result in a loss of pressure in backup systems. Leaks can result in gas or liquid mixing where none is allowed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860343
EISBN: 978-1-62708-348-5
.... ( 1965 ). On pyrophoricity of metals, and of fine metal powders in particular . Pyrodynamics 3 , 29 – 41 . Bates C. E. , Wren J. E. , Monroe R. , and Pears C. D. ( 1979 ). Ignition and combustion of ferrous metals in high pressure, high velocity, gaseous oxygen . J. Mater...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460107
EISBN: 978-1-62708-285-3
... the delivery pressure from the tubes at the desired process feed pressure into the houseline. This normally includes a pneumatic regulator that must be specified to handle the desired flow rate. Adequate houseline pressure-relief valves should be included to provide protection for the downstream components...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030292
EISBN: 978-1-62708-282-2
... to be the associated reduction in residual tensile stresses in the area of the weldment, and the reduction in hardness and changes in the carbide morphology of weld heat-affected zones (HAZ). For refinery reactor vessels, which operate at high temperatures and pressures, 2.25Cr-1Mo steel is widely used. For improved...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290207
EISBN: 978-1-62708-306-5
... by foot force, air pressure, or electricity. For high-production situations, the operations can be made fully automatic. Hand-held pneumatic rivet guns are driven by compressed air and are classified as light, medium, and heavy hitting. Light-hitting guns are used to install 2.3 to 3.2 mm (0.09...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140021
EISBN: 978-1-62708-335-5
... Shell molds assembled before pouring. Source: Ref 1 Fig. 3.6 Alloy 224.0 impellers produced by low-pressure plaster casting Fig. 3.8 Permanent mold machined from steel. Source: Ref 1 Fig. 3.14 Semisolid formed alloy A357.0 landing gear component Fig. 3.15 One...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000039
EISBN: 978-1-62708-312-6
... used for compaction of iron and low-alloy steel powders. Because information on these types of compacting equipment is covered in detail in a number of books on PM (including Ref 1 ), those details are not covered here. Bodycote Powdermet AB, Sweden, manufactures pressure vessel components, valve...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480113
EISBN: 978-1-62708-318-8
... reasonable toughness, a necessary property for pressure vessels. As the strength level of metal increases, the ability for plastic flow diminishes in the presence of a crack. At this point, a crack propagates suddenly from a flaw and completely through the specimen without much plastic flow...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.9781627083195
EISBN: 978-1-62708-319-5
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290111
EISBN: 978-1-62708-319-5
... to avoid leaks and then pressurized in a vessel filled with oil or water that transfers the load to the flexible tooling, which, in turn, transmits the load to the powders inside the tooling. A favorite binder is paraffin wax, due to its low cost, easy removal, and adequate green strength. Compaction...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870031
EISBN: 978-1-62708-314-0
... cases, pressure vessels, sporting goods, cables, and tension members. Aramid paper used in honeycomb sandwich constructions is made of Nomex aramid fiber. Nomex is chemically related to Kevlar, but its strength and modulus are considerably lower, more like those of conventional textile fibers...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980009
EISBN: 978-1-62708-342-3
...). Source: Alusuisse Fig. 2.48 Bus bar sections in aluminum alloys with pressure clad layer of stainless steel. The bus bars from S and U trains collect the electrical energy through the stainless steel layer. Source: Alusuisse Fig. 2.49 Installation-friendly large section in the alloy...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610263
EISBN: 978-1-62708-303-4
... is never fully effective. Residual stresses up to yield point have been measured in stress-relieved pressure vessels and up to 75% of yield in stress-relieved nodes in offshore structures. Due consideration must be given to the complexity of the overall structure when stress relieving and to the time...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720293
EISBN: 978-1-62708-305-8
... pressures can be leak tested at the foundry. Various methods are used, according to the type of metal being tested. One method consists of pumping air at a specific pressure into the inside of the casting in water at a given temperature. Any leaks through the casting become apparent by the release...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.9781627083355
EISBN: 978-1-62708-335-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.9781627083485
EISBN: 978-1-62708-348-5
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850334
EISBN: 978-1-62708-260-0
... number can easily be calculated from the applied load and the projected area of the impression in terms of a pressure in units such as kilograms per square millimeter. 5-2.1 Relationship to Stress-Strain Curve Examination of the indentation hardness test reveals some close parallels...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.9781627083423
EISBN: 978-1-62708-342-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.9781627082600
EISBN: 978-1-62708-260-0