Published: 01 June 2016
Fig. 1.6 Schoop patent, “Method of Plating or Coating with Metallic Coatings,” 1915 More
Image
Published: 01 January 2015
Fig. 22.10 (Ti 33 Al 17 )N coating deposited by triode ion plating at low substrate current density. Scanning electron micrograph. Courtesy of A.S. Korhonen, Helsinki University of Technology. Source: Ref 22.40 , 22.41 More
Image
Published: 01 January 2015
Fig. 22.11 (T i ,Al)N coating deposited by triode ion plating at high substrate current density. Courtesy of A.S. Korhonen, Helsinki University of Technology. Source: Ref 22.40 , 22.41 More
Image
Published: 01 January 2015
Fig. 22.12 ZrN coating deposited by triode ion plating. Scanning electron micrograph. Courtesy of A.S. Korhonen, Helsinki University of Technology. Source: Ref 22.40 , 22.41 More
Image
Published: 01 January 1998
Fig. 16-14 (Ti 1 , Al) coating deposited by triode ion plating at high substrate current density. Courtesy of A.S. Korhonen, Helsinki University of Technology More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350231
EISBN: 978-1-62708-315-7
...: a cermet composite coating on a cemented carbide cutting tool. Also known as multilayer coating. composite plate. An electrodeposit consisting of layers of at least two dif- ferent compositions. contact corrosion. A term primarily used in Europe to describe galvanic corrosion between dissimilar metals...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350195
EISBN: 978-1-62708-315-7
... moderate protection Thermally sprayed zinc or aluminum for moderate protection Electrolytic zinc or zinc-nickel alloy (10–14% Ni) coating followed by chromate passivation and an organic topcoat Painting, with appropriate preparation and priming, perhaps zinc or aluminum loaded Cadmium plate...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300335
EISBN: 978-1-62708-323-2
... Abstract This chapter covers coatings and treatments that are used to improve the friction and wear behaviors of materials. It describes modifications that work by hardening contacting surfaces, including heat treating, vacuum coating, thermal spray, and plating, and those that separate...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120085
EISBN: 978-1-62708-269-3
... of scale and how it can be removed via belt grinding, abrasive blasting, and molten salt descaling baths. It also discusses the role of acid pickling, barrel finishing, polishing, and buffing as well as the use of chemical conversion coatings and protective platings. barrel finishing chemical...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350183
EISBN: 978-1-62708-315-7
... Fig. 14 Compares the abrasion resistance of TiN coatings applied by various thin-film processes Fig. 15 Compares the surface hardness of hardened tool steel and a cemented carbide with that of the following surface-hardening processes: TRD, CVD, PVD, boriding, chrome plating, electroless...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
... Abstract This chapter covers a wide range of finishing and coating operations, including cleaning, honing, polishing and buffing, and lapping. It discusses the use of rust-preventative compounds, conversion coatings, and plating metals as well as weld overlay, thermal spray, and ceramic...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850538
EISBN: 978-1-62708-260-0
... edge preparation schemes. A very wide range of materials have been coated in this way. For metals, the procedures [ 19 ] [1] used can be categorized as follows: Direct plating . Iron, cobalt, nickel, ruthenium, palladium, osmium, iridium, and platinum. Galvanic initiation . Copper, silver...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870191
EISBN: 978-1-62708-299-0
...) as a result of soil accumulation. Finishes are applied to aluminum alloys for aesthetic reasons and to provide protection against corrosion. These finishes include nonfinished (bare) aluminum, anodized aluminum, conversion coatings, painted aluminum, porcelain finishes, and plated finishes. In retarding...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
... protective linings barrier protection chemical inhibition galvanic protection surface preparation inspection quality assurance electroplating electroless plating hot dipping thermal spraying cladding pack cementation vapor deposition ion implantation laser processing COATINGS are the most...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.pnfn.t65900163
EISBN: 978-1-62708-350-8
... Abstract Stop-off coatings prevent nitriding of selected areas on components. This chapter discusses the processes, advantages, and disadvantages of stop-off techniques for gas nitriding, salt bath nitriding, and ion nitriding. gas nitriding ion nitriding salt bath nitriding stop-off...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350125
EISBN: 978-1-62708-315-7
... Abstract This chapter discusses the use of coating methods and materials and their impact on corrosion and wear behaviors. It provides detailed engineering information on a wide range of processes, including organic, ceramic, and hot dip coating, metal plating and cladding, and the use of weld...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 January 2023
DOI: 10.31399/asm.tb.itfdtktmse.t56060013
EISBN: 978-1-62708-440-6
...-enhanced CVD process temperature sputtering thin film purity vacuum ion plating Problem 1 Gas leaks into a vacuum chamber at a rate of 5 cm 3 atm sec −1 . The pump has a volumetric flow rate of 2000 liters sec −1 . Calculate the limiting achievable pressure. Solution P = Q / S...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 January 2023
DOI: 10.31399/asm.tb.itfdtktmse.9781627084406
EISBN: 978-1-62708-440-6
Series: ASM Technical Books
Publisher: ASM International
Published: 31 January 2023
DOI: 10.31399/asm.tb.itfdtktmse.t56060001
EISBN: 978-1-62708-440-6
... deposition processes coating microstructure coating properties compound films dielectric coatings e-beam evaporation ion plating metallic coatings physical deposition processes sputtering thin films vapor phase epitaxy Introduction Thin films, like all coatings, are applied to base...