EISBN: 978-1-62708-281-5
.... The photolytic instability and degradation of plastics have a direct analog in the corrosion of metals, in that function is slowly degraded in the external environment by chemical reactions and must be treated as limiting the true usefulness of the materials. In the future, the full and successful outdoor use...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780336
EISBN: 978-1-62708-281-5
... Abstract This article provides a review of the biodegradation mechanisms of plastics, presents the definitions, and describes the means of measurement of biodegradation and biodeterioration. Various experimental examples of microbial degradation, namely fungal attack in cellophane and amylose films...