1-8 of 8 Search Results for

photochemical machining

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230339
EISBN: 978-1-62708-298-3
... Abstract Beryllium’s machining characteristics are similar to those of heat-treated cast aluminum and chilled cast iron. Like the other materials, it can be turned, milled, drilled, bored, sawed, cut, threaded, tapped, and trepanned with good results. This chapter explains how these machining...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.t51230207
EISBN: 978-1-62708-351-5
... mm thick, and 185 such sheets were required for each assembly (which included blanking plates at either end for spigots). It was decided to produce the holes by photochemical machining, which is eminently suitable for cutting fine detail in thin sheets. In all, six coolers were required for each...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740213
EISBN: 978-1-62708-308-9
...) Electrical discharge grinding (EDG) Electron beam machining (EBM) Laser beam machining (LBM) Thermal energy method (TEM) Chemical Chemical milling (CM) Photochemical machining (PCM) Types of Machining Equipment There are three types of machining equipment: general-purpose machine tools...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230441
EISBN: 978-1-62708-298-3
... in this figure, such as the half-lap joint, ideally should result in a uniform stress pattern under tensile-shear loading. Several of these joints, however, would involve additional machining. An extensive discussion with corresponding illustrations of adhesive joints is presented in Pizzi and Mittal [2003...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230523
EISBN: 978-1-62708-298-3
.... , Vol 131 , p 130 – 139 10.1002/zaac.19231310111 Friedman G. , 1937 . “ Problems in the Extrusion of Structural Beryllium Shapes ,” Technical Paper MF-67–204, American Society of Tool and Manufacturing Engineers , Dearborn, MI Friedman H. , 1989 . Photochemical Machining...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.9781627082983
EISBN: 978-1-62708-298-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780146
EISBN: 978-1-62708-281-5
... in the environment. Plasticizers Some naturally occurring polymers, such as rubber, are flexible and readily processed by appropriate machines. However, other naturally occurring polymers, such as gutta-percha, lignin, shellac, cellulose, and proteins, are relatively stiff. Both the cellulose present in paper...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2004
DOI: 10.31399/asm.tb.ps.t62440189
EISBN: 978-1-62708-352-2
... environmental concern arose over the use of volatile organic compounds (VOCs). Hitherto, these were a major ingredient of solder fluxes, and emissions of VOCs from an industrial wave-soldering machine can be many kilograms per hour. The VOCs play a major role in the generation of photochemical smog...