Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740047
EISBN: 978-1-62708-308-9
..., cupola, crucible, and vacuum melting, and common casting techniques such as sand casting, plaster and shell casting, evaporative pattern casting, investment casting, permanent mold casting, cold and hot chamber die casting, squeeze casting, semisolid metal processing, and centrifugal casting...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060085
EISBN: 978-1-62708-261-7
.... It describes the design and operation of melting furnaces as well as melting practices and the role of fluxing. It also discusses casting methods, nonferrous casting alloys, and atomization processes used to make metal powders. atomization foundry casting melting furnaces nonferrous casting alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140021
EISBN: 978-1-62708-335-5
... Fig. 3.1 Typical sand mold gating. Source: Ref 1 Fig. 3.2 Typical permanent mold gating. Source: Ref 2 Fig. 3.3 Typical die casting gating. Source: Ref 3 Fig. 3.4 Typical castings produced by the evaporative pattern casting (EPC) process Fig. 3.5...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410029
EISBN: 978-1-62708-280-8
... are stacked together to obtain the solid, as detailed in section 4.11.3 . Die cast tooling is very expensive to build, and it takes longer than the permanent mold build. Die alterations are expensive, and they decrease the tooling life. Therefore, a faster, less expensive method of die building...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.9781627083355
EISBN: 978-1-62708-335-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240095
EISBN: 978-1-62708-251-8
... pattern casting, investment casting, permanent mold casting, and die casting. solidification castings wrought products grain refinement secondary dendrite arm spacing porosity shrinkage sand casting plaster mold casting evaporative pattern casting investment casting permanent mold casting...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.9781627082808
EISBN: 978-1-62708-280-8
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550033
EISBN: 978-1-62708-307-2
... any color or texture. The ease with which aluminum may be fabricated into any form is one of its most important assets. Often, it can compete successfully with cheaper materials having a lower degree of workability. The metal can be cast by any method known. It can be rolled to any desired...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240201
EISBN: 978-1-62708-251-8
... loads or forces. Since the results of these tests are often used by regulatory agencies, it is important that these test methods are consistent and standardized. In the United States, ASTM International is the most widely recognized source of standardized testing procedures. Fig. 12.1 States...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140001
EISBN: 978-1-62708-335-5
... Development Council , 1996 9. “ The NFFS Guide to Aluminum Casting Design: Sand and Permanent Mold ,” Non-Ferrous Founders Society , 1994 10. “ Designations and Chemical Composition Limits for Aluminum Alloys in the Form of Castings and Ingot ,” The Aluminum Association Alloy and Temper...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.9781627082709
EISBN: 978-1-62708-270-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.horfi.9781627082563
EISBN: 978-1-62708-256-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.9781627083096
EISBN: 978-1-62708-309-6
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610025
EISBN: 978-1-62708-303-4
... to applied loads or forces. Because the results of these tests are often used by regulatory agencies, it is important that these test methods are consistent and standardized. In the United States, ASTM International is the most widely recognized source of standardized testing procedures. Fig. 1 States...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110603
EISBN: 978-1-62708-247-1
... process also requires access to data sheets and support from manufacturers to obtain the actual attributes of parts, e.g., date code validity. An electronic part that has been re-marked with good quality ink and without errors is hard to detect through the visual inspection method. Marking permanency...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290001
EISBN: 978-1-62708-306-5
... permanent joints. Mechanical fastening and adhesive bonding usually do not cause metallurgical reactions. Consequently, these methods are often preferred when joining dissimilar combinations of materials and for joining polymer-matrix composites that are sensitive to extreme heat. Welding processes...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610055
EISBN: 978-1-62708-303-4
... be careful to qualify its brittleness as a function of temperature. Ordinary glass is brittle at ambient temperatures, but when heated in a flame or a furnace, it becomes extremely plastic or ductile. Then, it is readily moldable into an infinite variety of shapes. Indeed, heating glass is the major method...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090349
EISBN: 978-1-62708-266-2
... other important factors must be considered: the permanence of the weld residual stresses, the mechanical properties of the weldment, and the effect of the pipe weld preparation method. Permanence of Weld Residual Stresses Mechanical Properties of Weldments Effect of Weld Preparation Method...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060149
EISBN: 978-1-62708-261-7
...Abstract Abstract This chapter explains how metallography and hardness testing are used to evaluate the quality and condition of metal products. It also discusses the use of tensile testing, fracture toughness and impact testing, fatigue testing, and nondestructive test methods including...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720183
EISBN: 978-1-62708-305-8
... Evaluation , McGraw-Hill , 2000 • Nondestructive Testing and Quality Control , Vol 17 , ASM Handbook , ASM International , 1989 Liquid penetrant inspection is a nondestructive method used to find discontinuities that are open to the surface of solid, essentially nonporous materials...